| 微合金化元素Sn对Al-Mg-Si合金高温时效强化相析出路径的改变 |
向雪梅, 赖玉香, 刘春辉, 陈江华( ) |
| 湖南大学材料科学与工程学院 长沙 410082 |
|
| Sn-Induced Modification of the Precipitation Pathways upon High-Temperature Ageing in an Al-Mg-Si Alloy |
Xuemei XIANG, Yuxiang LAI, Chunhui LIU, Jianghua CHEN( ) |
| College of Materials Science and Engineering, Hunan University, Changsha 410082, China |
引用本文:
向雪梅, 赖玉香, 刘春辉, 陈江华. 微合金化元素Sn对Al-Mg-Si合金高温时效强化相析出路径的改变[J]. 金属学报, 2018, 54(9): 1273-1280.
Xuemei XIANG,
Yuxiang LAI,
Chunhui LIU,
Jianghua CHEN.
Sn-Induced Modification of the Precipitation Pathways upon High-Temperature Ageing in an Al-Mg-Si Alloy[J]. Acta Metall Sin, 2018, 54(9): 1273-1280.
| [1] | Edwards G A, Stiller K, Dunlop G L, et al.The precipitation sequence in Al-Mg-Si alloys[J]. Acta Mater., 1998, 46: 3893 | | [2] | Marioara C D, Andersen S J, Jansen J, et al.The influence of temperature and storage time at RT on nucleation of the β" phase in a 6082 Al-Mg-Si alloy[J]. Acta Mater., 2003, 51: 789 | | [3] | Zhang H, Li L X, Yuan D, et al.Hot deformation behavior of the new Al-Mg-Si-Cu aluminum alloy during compression at elevated temperatures[J]. Mater. Charact., 2007, 58: 168 | | [4] | Tian N, Zhao G, Zuo L, et al.Study on the strain hardening behavior of Al-Mg-Si-Cu alloy sheet for automotive body[J]. Acta Metall. Sin., 2010, 46: 613(田妮, 赵刚, 左良等. 汽车车身用Al-Mg-Si-Cu合金薄板应变强化行为的研究[J]. 金属学报, 2010, 46: 613) | | [5] | Li L X, Zhou J, Zhang H.Advanced extrusion technology and application of aluminium, magnesium alloy for vehicle body[J]. J. Mech. Eng., 2012, 48(18): 35(李落星, 周佳, 张辉. 车身用铝、镁合金先进挤压成形技术及应用[J]. 机械工程学报, 2012, 48(18): 35) | | [6] | Zandbergen H W, Andersen S J, Jansen J.Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies[J]. Science, 1997, 277: 1221 | | [7] | Chen J H, Costan E, van Huis M A, et al. Atomic pillar-based nanoprecipitates strengthen Al-Mg-Si alloys[J]. Science, 2006, 312: 416 | | [8] | Vissers R, van Huis M A, Jansen J, et al. The crystal structure of the β' phase in Al-Mg-Si alloys[J]. Acta Mater., 2007, 55: 3815 | | [9] | Ravi C, Wolverton C.First-principles study of crystal structure and stability of Al-Mg-Si-(Cu) precipitates[J]. Acta Mater., 2004, 52: 4213 | | [10] | Wang B, Wang X J, Song H, et al.Strengthening effects of microstructure evolution during early ageing process in Al-Mg-Si alloy[J]. Acta Metall. Sin., 2014, 50: 685(汪波, 王晓姣, 宋辉等. Al-Mg-Si合金时效早期显微组织演变及其对强化的影响[J]. 金属学报, 2014, 50: 685) | | [11] | Lai Y X, Jiang B C, Liu C H, et al.Low-alloy-correlated reversal of the precipitation sequence in Al-Mg-Si alloys[J]. J. Alloys Compd., 2017, 701: 94 | | [12] | Pogatscher S, Antrekowitsch H, Leitner H, et al.Mechanisms controlling the artificial aging of Al-Mg-Si Alloys[J]. Acta Mater., 2011, 59: 3352 | | [13] | de Geuser F, Lefebvre W, Blavette D. 3D atom probe study of solute atoms clustering during natural ageing and pre-ageing of an Al-Mg-Si alloy[J]. Philos. Mag. Lett., 2006, 86: 227 | | [14] | Tors?ter M, Hasting H S, Lefebvre W, et al.The influence of composition and natural aging on clustering during preaging in Al-Mg-Si alloys[J]. J. Appl. Phys., 2010, 108: 073527 | | [15] | R?yset J, Stene T, S?ter J A, et al. The effect of intermediate storage temperature and time on the age hardening response of Al-Mg-Si Alloys [J]. Mater. Sci. Forum, 2006, 519-521: 239 | | [16] | Banhart J, Chang C S T, Liang Z Q, et al. Natural aging in Al-Mg-Si alloys—A process of unexpected complexity[J]. Adv. Eng. Mater., 2010, 12: 559 | | [17] | Yamada K, Sato T, Kamio A. Effects of quenching conditions on two-step aging behavior of Al-Mg-Si Alloys [J]. Mater. Sci. Forum, 2000, 331-337: 669 | | [18] | Banhart J, Lay M D H, Chang C S T, et al. Kinetics of natural aging in Al-Mg-Si alloys studied by positron annihilation lifetime spectroscopy[J]. Phys. Rev., 2011, 83B: 014101 | | [19] | Zurob H S, Seyedrezai H.A model for the growth of solute clusters based on vacancy trapping[J]. Scr. Mater., 2009, 61: 141 | | [20] | Liu C H, Lai Y X, Chen J H, et al.Natural-aging-induced reversal of the precipitation pathways in an Al-Mg-Si alloy[J]. Scr. Mater., 2016, 115: 150 | | [21] | Chang C S, Wieler I, Wanderka N, et al.Positive effect of natural pre-ageing on precipitation hardening in Al-0.44at% Mg-0.38at% Si alloy[J]. Ultramicroscopy, 2009, 109: 585 | | [22] | Saga M, Kikuchi M.Effect of Sn Addition on the two-step aging behavior in Al-Mg-Si Alloys for automotive application [A]. Proceedings of the 9th International Conference on Aluminium Alloys[C]. Melbourne: Institute of Material Engineering Australasia Ltd, 2004: 520 | | [23] | Pogatscher S, Antrekowitsch H, Werinos M, et al.Diffusion on demand to control precipitation aging: application to Al-Mg-Si alloys[J]. Phys. Rev. Lett., 2014, 112: 225701 | | [24] | Werinos M, Antrekowitsch H, Fragner W, et al.Influence of temperature on natural aging kinetics of AA6061 modified with Sn[A]. Light Metals 2015 [M]. Cham: Springer International Publishing, 2015: 367 | | [25] | Werinos M, Antrekowitsch H, Kozeschnik E, et al.Ultrafast artificial aging of Al-Mg-Si alloys[J]. Scr. Mater., 2016, 112: 148 | | [26] | Shishido H, Takaki Y, Kozuka M, et al.Effects of Sn addition on clustering and age-hardening behavior in a pre-aged Al-Mg-Si alloy[J]. Mater. Sci. Forum, 2016, 877: 455 | | [27] | Pogatscher S, Antrekowitsch H, Ebner T, et al.The role of co-clusters in the artificial aging of AA6061 and AA6060 [A]. Light Metals 2012[C]. New York: Springer, 2012: 415 | | [28] | Murayama M, Hono K.Pre-precipitate clusters and precipitation processes in Al-Mg-Si-Cu alloys[J]. Acta Mater., 1999, 47: 1537 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|