| 镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为 |
程伟丽1,2( ), 谷雄杰1, 成世明1, 陈宇航1, 余晖3, 王利飞1,2, 王红霞1,2, 李航1 |
1.太原理工大学 材料科学与工程学院 太原 030024 2.太原理工大学 山西省先进镁基材料重点实验室 太原 030024 3.河北工业大学 材料科学与工程学院 天津 300132 |
|
| Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery |
CHENG Weili1,2( ), GU Xiongjie1, CHENG Shiming1, CHEN Yuhang1, YU Hui3, WANG Lifei1,2, WANG Hongxia1,2, LI Hang1 |
1.School of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China 2.Shanxi Key Laboratory of Advanced Magnesium-Based Materials, Taiyuan University of Technology, Taiyuan 030024, China 3.School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China |
引用本文:
程伟丽, 谷雄杰, 成世明, 陈宇航, 余晖, 王利飞, 王红霞, 李航. 镁空气电池阳极用挤压态Mg-2Bi-0.5Ca-0.5In合金的放电性能和电化学行为[J]. 金属学报, 2021, 57(5): 623-631.
Weili CHENG,
Xiongjie GU,
Shiming CHENG,
Yuhang CHEN,
Hui YU,
Lifei WANG,
Hongxia WANG,
Hang LI.
Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery[J]. Acta Metall Sin, 2021, 57(5): 623-631.
| 1 |
Liu X, Xue J L. The role of Al2Gd cuboids in the discharge performance and electrochemical behaviors of AZ31-Gd anode for Mg-air batteries [J]. Energy, 2019, 189: 116314
|
| 2 |
Liu X, Guo Z C, Xue J L, et al. The role of Al2Ca and Al2(Sm, Ca, La) particles in the microstructures and electrochemical discharge performance of as-extruded Mg-3wt.%Al-1wt.%Zn-based alloys for primary Mg-air batteries [J]. Int. J. Energy Res., 2019, 43: 4569
|
| 3 |
Zheng T X, Hu Y B, Zhang Y X, et al. Composition optimization and electrochemical properties of Mg-Al-Sn-Mn alloy anode for Mg-air batteries [J]. Mater. Des., 2018, 137: 245
|
| 4 |
Rahman M, Wang X J, Wen C E. High energy density metal-air batteries: A review [J]. J. Electrochem. Soc., 2013, 160: A1759
|
| 5 |
Xiong H Q, Yu K, Yin X, et al. Effects of microstructure on the electrochemical discharge behavior of Mg-6wt%Al-1wt%Sn alloy as anode for Mg-air primary battery [J]. J. Alloys Compd., 2017, 708: 652
|
| 6 |
Feng Y, Xiong W H, Zhang J C, et al. Electrochemical discharge performance of the Mg-Al-Pb-Ce-Y alloy as the anode for Mg-air batteries [J]. J. Mater. Chem., 2016, 4A: 8658
|
| 7 |
Ma Y B, Li N, Li D Y, et al. Performance of Mg-14Li-1Al-0.1Ce as anode for Mg-air battery [J]. J. Power Sources, 2011, 196: 2346
|
| 8 |
Zeng R C, Cui L Y, Ke W. Biomedical magnesium alloys: Composition, microstructure and corrosion [J]. Acta Metall. Sin., 2018, 54: 1215
|
| 8 |
曾荣昌, 崔蓝月, 柯 伟. 医用镁合金: 成分、组织及腐蚀 [J]. 金属学报, 2018, 54: 1215
|
| 9 |
Zhang Z M, Yu K, Ren W W, et al. Microstructure of directly extruded Mg-1Zn-1Ca alloy and its corrosion behavior in SBF solution [J]. Acta Metall. Sin., 2015, 51: 985
|
| 9 |
张忠明, 余 凯, 任伟伟等. 正挤压态Mg-1Zn-1Ca合金的显微组织及其在SBF溶液中的腐蚀行为 [J]. 金属学报, 2015, 51: 985
|
| 10 |
Zhi Q, Gao J, Dong C F, et al. Corrosion behavior of microarc oxidation film on AZ91D magnesium alloy [J]. Acta Metall. Sin., 2008, 44: 986
|
| 10 |
郅 青, 高 瑾, 董超芳等. AZ91D镁合金微弧氧化膜的腐蚀行为研究 [J]. 金属学报, 2008, 44: 986
|
| 11 |
Wang N G, Wang R C, Peng C Q, et al. Discharge behaviour of Mg-Al-Pb and Mg-Al-Pb-In alloys as anodes for Mg-air battery [J]. Electrochim. Acta, 2014, 149: 193
|
| 12 |
Gu X J, Cheng W L, Cheng S M, et al. Discharge behavior of Mg-Sn-Zn-Ag alloys with different Sn contents as anodes for Mg-air batteries [J]. J. Electrochem. Soc., 2020, 167: 020501
|
| 13 |
Liu X, Xue J L, Zhang P J, et al. Effects of the combinative Ca, Sm and La additions on the electrochemical behaviors and discharge performance of the as-extruded AZ91 anodes for Mg-air batteries [J]. J. Power Sources, 2019, 414: 174
|
| 14 |
Wang N G, Wang R C, Peng C Q, et al. Effect of hot rolling and subsequent annealing on electrochemical discharge behavior of AP65 magnesium alloy as anode for seawater activated battery [J]. Corros. Sci., 2012, 64: 17
|
| 15 |
Feng Y, Lei G, He Y Q, et al. Discharge performance of Mg-Al-Pb-La anode for Mg-air battery [J]. Trans. Nonferrous Met. Soc. China, 2018, 28: 2274
|
| 16 |
Wang N G, Li W P, Huang Y X, et al. Wrought Mg-Al-Pb-RE alloy strips as the anodes for Mg-air batteries [J]. J. Power Sources, 2019, 436: 226855
|
| 17 |
Huang G S, Zhao Y C, Wang Y X, et al. Performance of Mg-air battery based on AZ31 alloy sheet with twins [J]. Mater. Lett., 2013, 113: 46
|
| 18 |
Yuasa M, Huang X S, Suzuki K, et al. Effects of microstructure on discharge behavior of AZ91 Alloy as anode for Mg-air battery [J]. Mater. Trans., 2014, 55: 1202
|
| 19 |
Liu X, Xue J L, Zhang D. Electrochemical behaviors and discharge performance of the as-extruded Mg-1.5 wt%Ca alloys as anode for Mg-air battery [J]. J. Alloys Compd., 2019, 790: 822
|
| 20 |
Deng M, Höche D, Lamaka S V, et al. Revealing the impact of second phase morphology on discharge properties of binary Mg-Ca anodes for primary Mg-air batteries [J]. Corros. Sci., 2019, 153: 225
|
| 21 |
Deng M, Höche D, Lamaka S V, et al. Mg-Ca binary alloys as anodes for primary Mg-air batteries [J]. J. Power Sources, 2018, 396: 109
|
| 22 |
Liu X, Xue J L, Liu S Z. Discharge and corrosion behaviors of the α-Mg and β-Li based Mg alloys for Mg-air batteries at different current densities [J]. Mater. Des., 2018, 160: 138
|
| 23 |
Wang N G, Wang R C, Feng Y, et al. Discharge and corrosion behaviour of Mg-Li-Al-Ce-Y-Zn alloy as the anode for Mg-air battery [J]. Corros. Sci., 2016, 112: 13
|
| 24 |
Cheng S M, Cheng W L, Gu X J, et al. Discharge properties of low-alloyed Mg-Bi-Ca alloys as anode materials for Mg-air batteries: Influence of Ca alloying [J]. J. Alloys Compd., 2020, 823: 153779
|
| 25 |
Flamini D O, Saidman S B. Electrochemical behaviour of Al-Zn-Ga and Al-In-Ga alloys in chloride media [J]. Mater. Chem. Phys., 2012, 136: 103
|
| 26 |
Park I J, Choi S R, Kim J G. Aluminum anode for aluminum-air battery—Part II: Influence of In addition on the electrochemical characteristics of Al-Zn alloy in alkaline solution [J]. J. Power Sources, 2017, 357: 47
|
| 27 |
Yuan S Q, Lu H M, Sun Z G, et al. Electrochemical performance of Mg-3Al modified with Ga, In and Sn as anodes for Mg-air battery [J]. J. Electrochem. Soc., 2016, 163: A1181
|
| 28 |
Gore P, Fajardo S, Birbilis N, et al. Anodic activation of Mg in the presence of In3+ ions in dilute sodium chloride solution [J]. Electrochim. Acta, 2019, 293: 199
|
| 29 |
Chai Y F, Jiang B, Song J F, et al. Improvement of mechanical properties and reduction of yield asymmetry of extruded Mg-Sn-Zn alloy through Ca addition [J]. J. Alloys Compd., 2019, 782: 1076
|
| 30 |
Yuasa M, Huang X S, Suzuki K, et al. Discharge properties of Mg-Al-Mn-Ca and Mg-Al-Mn alloys as anode materials for primary magnesium-air batteries [J]. J. Power Sources, 2015, 297: 449
|
| 31 |
Deng M, Wang L Q, Höche D, et al. Ca/In micro alloying as a novel strategy to simultaneously enhance power and energy density of primary Mg-air batteries from anode aspect [J]. J. Power Sources, 2020, 472: 228528
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|