| 非均匀组织FeMnCoCr高熵合金的微观结构和力学性能 |
王洪伟1, 何竹风1, 贾楠2( ) |
1.东北大学 材料科学与工程学院 材料各向异性与织构教育部重点实验室 沈阳 110819 2.东北大学 轧制技术及连轧自动化国家重点实验室 沈阳 110819 |
|
| Microstructure and Mechanical Properties of a FeMnCoCr High-Entropy Alloy with Heterogeneous Structure |
WANG Hongwei1, HE Zhufeng1, JIA Nan2( ) |
1.Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China 2.State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China |
引用本文:
王洪伟, 何竹风, 贾楠. 非均匀组织FeMnCoCr高熵合金的微观结构和力学性能[J]. 金属学报, 2021, 57(5): 632-640.
Hongwei WANG,
Zhufeng HE,
Nan JIA.
Microstructure and Mechanical Properties of a FeMnCoCr High-Entropy Alloy with Heterogeneous Structure[J]. Acta Metall Sin, 2021, 57(5): 632-640.
| 1 |
Yeh J W. Alloy design strategies and future trends in high-entropy alloys [J]. JOM, 2013, 65: 1759
|
| 2 |
Yao M J, Pradeep K G, Tasan C C, et al. A novel, single phase, non-equiatomic FeMnNiCoCr high-entropy alloy with exceptional phase stability and tensile ductility [J]. Scr. Mater., 2014, 72-73: 5
|
| 3 |
Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153
|
| 4 |
Gali A, George E P. Tensile properties of high- and medium-entropy alloys [J]. Intermetallics, 2013, 39: 74
|
| 5 |
Anand G, Goodall R, Freeman C L. Role of configurational entropy in body-centred cubic or face-centred cubic phase formation in high entropy alloys [J]. Scr. Mater., 2016, 124: 90
|
| 6 |
Senkov O N, Wilks G B, Scott J M, et al. Mechanical properties of Nb25Mo25Ta25W25 and V20Nb20Mo20Ta20W20 refractory high entropy alloys [J]. Intermetallics, 2011, 19: 698
|
| 7 |
Juan C C, Tsai M H, Tsai C W, et al. Enhanced mechanical properties of HfMoTaTiZr and HfMoNbTaTiZr refractory high-entropy alloys [J]. Intermetallics, 2015, 62: 76
|
| 8 |
Zhao Y J, Qiao J W, Ma S G, et al. A hexagonal close-packed high-entropy alloys: The effect of entropy [J]. Mater. Des., 2016, 96: 10
|
| 9 |
Takeuchi A, Amiya K, Wada T, et al. High-entropy alloys with a hexagonal close-packed structure designed by equi-atomic alloy strategy and binary phase diagrams [J]. JOM, 2014, 66: 1984
|
| 10 |
Feuerbacher M, Heidelmann M, Thomas C. Hexagonal high-entropy alloys [J]. Mater. Res. Lett., 2015, 3: 1
|
| 11 |
Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213
|
| 12 |
Otto F, Dlouhý A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy [J]. Acta Mater., 2013, 61: 5743
|
| 13 |
Laplanche G, Kostka A, Horst O M, et al. Microstructure evolution and critical stress for twinning in the CrMnFeCoNi high-entropy alloy [J]. Acta Mater., 2016, 118: 152
|
| 14 |
Oh H S, Ma D C, Leyson G P, et al. Lattice distortions in the FeCoNiCrMn high entropy alloy studied by theory and experiment [J]. Entropy, 2016, 18: 321
|
| 15 |
Xiong F, Fu R D, Li Y J, et al. Effects of nitrogen alloying and friction stir processing on the microstructures and mechanical properties of CoCrFeMnNi high-entropy alloys [J]. J. Alloys Compd., 2020, 822: 153512
|
| 16 |
Li Z M, Pradeep K G, Deng Y, et al. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off [J]. Nature, 2016, 534: 227
|
| 17 |
Li Z M, Tasan C C, Pradeep K G, et al. A TRIP-assisted dual-phase high-entropy alloy: Grain size and phase fraction effects on deformation behavior [J]. Acta Mater., 2017, 131: 323
|
| 18 |
Deng Y, Tasan C C, Pradeep K G, et al. Design of a twinning-induced plasticity high entropy alloy [J]. Acta Mater., 2015, 94: 124
|
| 19 |
Lu W J, Liebscher C H, Dehm G, et al. Bidirectional transformation enables hierarchical nanolaminate dual-phase high-entropy alloys [J]. Adv. Mater., 2018, 30: 1804727
|
| 20 |
Su J, Raabe D, Li Z M. Hierarchical microstructure design to tune the mechanical behavior of an interstitial TRIP-TWIP high-entropy alloy [J]. Acta Mater., 2019, 163: 40
|
| 21 |
Bae J W, Seol J B, Moon J, et al. Exceptional phase-transformation strengthening of ferrous medium-entropy alloys at cryogenic temperatures [J]. Acta Mater., 2018, 161: 388
|
| 22 |
Uzer B, Picak S, Liu J, et al. On the mechanical response and microstructure evolution of NiCoCr single crystalline medium entropy alloys [J]. Mater. Res. Lett., 2018, 6: 442
|
| 23 |
He J Y, Wang H, Huang H L, et al. A precipitation-hardened high-entropy alloy with outstanding tensile properties [J]. Acta Mater., 2016, 102: 187
|
| 24 |
Sun S J, Tian Y Z, An X H, et al. Ultrahigh cryogenic strength and exceptional ductility in ultrafine-grained CoCrFeMnNi high-entropy alloy with fully recrystallized structure [J]. Mater. Today Nano, 2018, 4: 46
|
| 25 |
Li Z M. Interstitial equiatomic CoCrFeMnNi high-entropy alloys: Carbon content, microstructure, and compositional homogeneity effects on deformation behavior [J]. Acta Mater., 2019, 164: 400
|
| 26 |
Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal [J]. Nature, 2002, 419: 912
|
| 27 |
He Z F, Jia N, Wang H W, et al. The effect of strain rate on mechanical properties and microstructure of a metastable FeMnCoCr high entropy alloy [J]. Mater. Sci. Eng., 2020, A776: 138982
|
| 28 |
Takaki S, Nakatsu H, Tokunaga Y. Effects of austenite grain size on ε martensitic transformation in Fe-15mass%Mn alloy [J]. Mater. Trans. JIM, 1993, 34: 489
|
| 29 |
Olsen G B, Cohen M. Dislocation theory of martensitic transformations [A]. Dislocations in Solids [M]. Vol.7.,Amsterdam: North-Holland, 1986: 295
|
| 30 |
Zhang W Y, Yan D S, Lu W J, et al. Carbon and nitrogen co-doping enhances phase stability and mechanical properties of a metastable high-entropy alloy [J]. J. Alloys Compd., 2020, 831: 154799
|
| 31 |
He Z F, Jia N, Ma D, et al. Joint contribution of transformation and twinning to the high strength-ductility combination of a FeMnCoCr high entropy alloy at cryogenic temperatures [J]. Mater. Sci. Eng., 2019, A759: 437
|
| 32 |
Wang M M, Li Z M, Raabe D. In-situ SEM observation of phase transformation and twinning mechanisms in an interstitial high-entropy alloy [J]. Acta Mater., 2018, 147: 236
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|