| 热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响 |
王悦1,2, 王继杰1, 张昊2, 赵泓博2, 倪丁瑞2( ), 肖伯律2, 马宗义2 |
1.沈阳航空航天大学 材料科学与工程学院 沈阳 110136 2.中国科学院金属研究所 沈阳 110016 |
|
| Effects of Heat Treatments on Microstructure and Mechanical Properties of AlSi10Mg Alloy Produced by Selective Laser Melting |
WANG Yue1,2, WANG Jijie1, ZHANG Hao2, ZHAO Hongbo2, NI Dingrui2( ), XIAO Bolv2, MA Zongyi2 |
1.College of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110136, China 2.Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
王悦, 王继杰, 张昊, 赵泓博, 倪丁瑞, 肖伯律, 马宗义. 热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响[J]. 金属学报, 2021, 57(5): 613-622.
Yue WANG,
Jijie WANG,
Hao ZHANG,
Hongbo ZHAO,
Dingrui NI,
Bolv XIAO,
Zongyi MA.
Effects of Heat Treatments on Microstructure and Mechanical Properties of AlSi10Mg Alloy Produced by Selective Laser Melting[J]. Acta Metall Sin, 2021, 57(5): 613-622.
| 1 |
Thijs L, Kempen K, Kruth J P, et al. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder [J]. Acta Mater., 2013, 61: 1809
|
| 2 |
Geng Y X, Fan S M, Jian J L, et al. Mechanical properties of AlSiMg alloy specifically designed for selective laser melting [J]. Acta Metall. Sin., 2020, 56: 821
|
| 2 |
耿遥祥, 樊世敏, 简江林等. 选区激光熔化专用AlSiMg合金成分设计及力学性能 [J]. 金属学报, 2020, 56: 821
|
| 3 |
Yu J, Wang J J, Ni D R, et al. Microstructure and mechanical properties of additive manufactured 2319 alloy by electron beam freeform fabrication [J]. Acta Metall. Sin., 2018, 54: 1725
|
| 3 |
于 菁, 王继杰, 倪丁瑞等. 电子束熔丝沉积快速成形2319铝合金的微观组织与力学性能 [J]. 金属学报, 2018, 54: 1725
|
| 4 |
Calignano F. Design optimization of supports for overhanging structures in aluminum and titanium alloys by selective laser melting [J]. Mater. Des., 2014, 64: 203
|
| 5 |
Uddin S Z, Murr L E, Terrazas C A, et al. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing [J]. Addit. Manuf., 2018, 22: 405
|
| 6 |
Prashanth K G, Scudino S, Eckert J. Defining the tensile properties of Al-12Si parts produced by selective laser melting [J]. Acta Mater., 2017, 126: 25
|
| 7 |
Wang L F, Sun J, Yu X L, et al. Enhancement in mechanical properties of selectively laser-melted AlSi10Mg aluminum alloys by T6-like heat treatment [J]. Mater. Sci. Eng., 2018, A734: 299
|
| 8 |
Han Q Q, Jiao Y. Effect of heat treatment and laser surface remelting on AlSi10Mg alloy fabricated by selective laser melting [J]. Int. J. Adv. Manuf. Technol., 2019, 102: 3315
|
| 9 |
Zhang H, Zhu H H, Qi T, et al. Selective laser melting of high strength Al-Cu-Mg alloys: Processing, microstructure and mechanical properties [J]. Mater. Sci. Eng., 2016, A656: 47
|
| 10 |
Sun S Y, Liu P, Hu J Y, et al. Effect of solid solution plus double aging on microstructural characterization of 7075 Al alloys fabricated by selective laser melting (SLM) [J]. Opt. Laser Technol., 2019, 114: 158
|
| 11 |
Kempen K, Thijs L, Van Humbeeck J, et al. Processing AlSi10Mg by selective laser melting: Parameter optimisation and material characterisation [J]. Mater. Sci. Technol., 2015, 31: 917
|
| 12 |
Zhuo L C, Wang Z Y, Zhang H J, et al. Effect of post-process heat treatment on microstructure and properties of selective laser melted AlSi10Mg alloy [J]. Mater. Lett., 2019, 234: 196
|
| 13 |
Aboulkhair N T, Everitt N M, Ashcroft I, et al. Reducing porosity in AlSi10Mg parts processed by selective laser melting [J]. Addit. Manuf., 2014, 1-4: 77
|
| 14 |
Aboulkhair N T, Maskery I, Tuck C, et al. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment [J]. Mater. Sci. Eng., 2016, A667: 139
|
| 15 |
Casati R, Hamidi Nasab M, Coduri M, et al. Effects of platform pre-heating and thermal-treatment strategies on properties of AlSi10Mg alloy processed by selective laser melting [J]. Metals, 2018, 8: 954
|
| 16 |
Maamoun A H, Elbestawi M, Dosbaeva G K, et al. Thermal post-processing of AlSi10Mg parts produced by Selective Laser Melting using recycled powder [J]. Addit. Manuf., 2018, 21: 234
|
| 17 |
Das M, Balla V K, Basu D, et al. Laser processing of SiC-particle-reinforced coating on titanium [J]. Scr. Mater., 2010, 63: 438
|
| 18 |
Zeng X H, Xue P, Wu L H, et al. Achieving an ultra-high strength in a low alloyed Al alloy via a special structural design [J]. Mater. Sci. Eng., 2019, A755: 28
|
| 19 |
Takata N, Kodaira H, Sekizawa K, et al. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments [J]. Mater. Sci. Eng., 2017, A704: 218
|
| 20 |
Li Y L, Gu D D. Parametric analysis of thermal behavior during selective laser melting additive manufacturing of aluminum alloy powder [J]. Mater. Des., 2014, 63: 856
|
| 21 |
Wei P, Wei Z Y, Chen Z, et al. The AlSi10Mg samples produced by selective laser melting: Single track, densification, microstructure and mechanical behavior [J]. Appl. Surf. Sci., 2017, 408: 38
|
| 22 |
Read N, Wang W, Essa K, et al. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development [J]. Mater. Des., 2015, 65: 417
|
| 23 |
Fousová M, Dvorský D, Michalcová A, et al. Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures [J]. Mater. Charact., 2018, 137: 119
|
| 24 |
Larrosa N O, Wang W, Read N, et al. Linking microstructure and processing defects to mechanical properties of selectively laser melted AlSi10Mg alloy [J]. Theor. Appl. Fract. Mech., 2018, 98: 123
|
| 25 |
Li W, Li S, Liu J, et al. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism [J]. Mater. Sci. Eng., 2016, A663: 116
|
| 26 |
Liu Y J, Liu Z, Jiang Y, et al. Gradient in microstructure and mechanical property of selective laser melted AlSi10Mg [J]. J. Alloys Compd., 2018, 735: 1414
|
| 27 |
Li W C, Zou Y Z, Zeng J M. Influence of solution temperature and time on microstructure of ZL114A alloy [J]. Mater. Mech. Eng., 2008, 32(11): 25
|
| 27 |
李卫超, 邹勇志, 曾建民. 固溶温度和时间对ZL114A合金组织的影响 [J]. 机械工程材料, 2008, 32(11): 25
|
| 28 |
Yu K B, Liu Y Z, Yang C Y. Effects of heat treatment on microstructures and mechanical properties of AlSi10Mg alloy produced by selective laser melting [J]. Mater. Sci. Eng. Powder Metall., 2018, 23: 298
|
| 28 |
余开斌, 刘允中, 杨长毅. 热处理对选区激光熔化成形AlSi10Mg合金显微组织及力学性能的影响 [J]. 粉末冶金材料科学与工程, 2018, 23: 298
|
| 29 |
Li Z H, Li B Q, Bai P K, et al. Research on the thermal behaviour of a selectively laser melted aluminium alloy: Simulation and experiment [J]. Materials, 2018, 11: 1172
|
| 30 |
Hadadzadeh A, Amirkhiz B S, Mohammadi M. Contribution of Mg2Si precipitates to the strength of direct metal laser sintered AlSi10Mg [J]. Mater. Sci. Eng., 2019, A739: 295
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|