| 高温时效处理对S31042耐热钢组织和蠕变性能的影响 |
郭倩颖1, 李彦默2, 陈斌2, 丁然1, 余黎明1, 刘永长1( ) |
1.天津大学 材料科学与工程学院 水利工程仿真与安全国家重点实验室 天津 300354 2.中国船舶集团有限公司 第七二五研究所 洛阳 471023 |
|
| Effect of High-Temperature Ageing on Microstructure and Creep Properties of S31042 Heat-Resistant Steel |
GUO Qianying1, LI Yanmo2, CHEN Bin2, DING Ran1, YU Liming1, LIU Yongchang1( ) |
1.State Key Laboratory of Hydraulic Engineering Simulation and Safety, School of Materials Science and Engineering, Tianjin University, Tianjin 300354, China 2.Luoyang Ship Material Research Institute, Luoyang 471023, China |
引用本文:
郭倩颖, 李彦默, 陈斌, 丁然, 余黎明, 刘永长. 高温时效处理对S31042耐热钢组织和蠕变性能的影响[J]. 金属学报, 2021, 57(1): 82-94.
Qianying GUO,
Yanmo LI,
Bin CHEN,
Ran DING,
Liming YU,
Yongchang LIU.
Effect of High-Temperature Ageing on Microstructure and Creep Properties of S31042 Heat-Resistant Steel[J]. Acta Metall Sin, 2021, 57(1): 82-94.
| 1 |
Zhu Z L, Xu H, Khan H I, et al. Effect of exposure temperature on oxidation of austenitic steel HR3C in supercritical water [J]. Oxid. Met., 2019, 91: 77
|
| 2 |
Liu P, Chu Z K, Yuan Y, et al. Microstructures and mechanical properties of a newly developed austenitic heat resistant steel [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 517
|
| 3 |
Du H, Cheng Y, Hou L, et al. Evolution of intergranular corrosion resistance for HR3C heat-resistant austenitic stainless steel at elevated temperature [J]. Corros. Eng. Sci. Technol., 2017, 52: 343
|
| 4 |
Zhou Y H, Liu Y C, Zhou X S, et al. Processing maps and microstructural evolution of the type 347H austenitic heat-resistant stainless steel [J]. J. Mater. Res., 2015, 30: 2090
|
| 5 |
Zieliński A, Sroka M, Hernas A, et al. The effect of long-term impact of elevated temperature on changes in microstructure and mechanical properties of HR3C Steel [J]. Arch. Metall. Mater., 2016, 61: 761
|
| 6 |
Li Y M, Liu Y C, Liu C X, et al. Microstructure evolution and mechanical properties of linear friction welded S31042 heat-resistant steel [J]. J. Mater. Sci. Technol., 2018, 34: 653
|
| 7 |
Wang B, Liu Z D, Cheng S C, et al. Microstructure evolution and mechanical properties of HR3C steel during long-term aging at high temperature [J]. J. Iron Steel Res. Int., 2014, 21: 765
|
| 8 |
Yang Y H, Zhu L H, Wang Q J, et al. Microstructural evolution and the effect on hardness and plasticity of S31042 heat-resistant steel during creep [J]. Mater. Sci. Eng., 2014, A608: 164
|
| 9 |
Zhou Y H, Liu Y C, Zhou X S, et al. Precipitation and hot deformation behavior of austenitic heat-resistant steels: A review [J]. J. Mater. Sci. Technol., 2017, 33: 1448
|
| 10 |
Wang J, Yu L M, Li C, et al. Effect of different temperatures on He atoms behavior in α-Fe with and without dislocations [J]. Acta Metall. Sin., 2019, 55: 274
|
| 10 |
王 瑾, 余黎明, 李 冲等. 不同温度对含与不含位错α-Fe中He原子行为的影响 [J]. 金属学报, 2019, 55: 274
|
| 11 |
Zhou Y H, Liu C X, Liu Y C, et al. Coarsening behavior of MX carbonitrides in type 347H heat-resistant austenitic steel during thermal aging [J]. Int. J. Miner. Metall. Mater., 2016, 23: 283
|
| 12 |
Hu G D, Wang P, Li D Z, et al. Precipitate evolution in a modified 25Cr-20Ni austenitic heat resistant stainless steel during creep rupture test at 750oC [J]. Acta Metall. Sin., 2018, 54: 1705
|
| 12 |
胡国栋, 王 培, 李殿中等. 新型25Cr-20Ni奥氏体耐热不锈钢750℃持久实验过程中析出相演变 [J]. 金属学报, 2018, 54: 1705
|
| 13 |
Wang J Z, Liu Z D, Bao H S, et al. Effect of ageing at 700oC on microstructure and mechanical properties of S31042 heat resistant steel [J]. J. Iron Steel Res. Int., 2013, 20: 54
|
| 14 |
Zhou C, Zhan L H, Shen R L, et al. Creep behavior and mechanical properties of Al-Li-S4 alloy at different aging temperatures [J]. J. Cent. South Univ., 2020, 27: 1168
|
| 15 |
Duan Y H, Zhang P, Li J, et al. Influence of long-term isothermal aging on microstructure and creep rupture properties of Ni-base superalloy M4706 [J]. J. Cent. South Univ., 2020, 27: 1168
|
| 16 |
Wu J, Li C, Liu Y C, et al. Precipitation of intersected plate-like γ′ phase in β and its effect on creep behavior of multiphase Ni3Al-based intermetallic alloy [J]. Mater. Sci. Eng., 2019, A767: 138439
|
| 17 |
Fang Y Y, Zhao J, Li X N. Precipitates in HR3C steel aged at high temperature [J]. Acta Metall. Sin., 2010, 46: 844
|
| 17 |
方圆圆, 赵 杰, 李晓娜. HR3C钢高温时效过程中的析出相 [J]. 金属学报, 2010, 46: 844
|
| 18 |
Li Y M, Liu C X, Yu L M, et al. Effect of high-temperature ageing on microstructure and mechanical properties of linear friction welded S31042 steel joint [J]. Acta Metall. Sin., 2018, 54: 981
|
| 18 |
李彦默, 刘晨曦, 余黎明等. 高温时效对S31042钢线性摩擦焊接头组织和力学性能的影响 [J]. 金属学报, 2018, 54: 981
|
| 19 |
Bai X, Pan J, Chen G, et al. Effect of high temperature aging on microstructure and mechanical properties of HR3C heat resistant steel [J]. Mater. Sci. Technol., 2013, 30: 205
|
| 20 |
Vujic S, Sandström R, Sommitsch C. Precipitation evolution and creep strength modelling of 25Cr20NiNbN austenitic steel [J]. Mater. High Temp., 2015, 32: 607
|
| 21 |
Zhang Y H, Feng Q. Effects of W on creep behaviors of novel Nb-bearing austenitic heat-resistant cast steels at 1000oC [J]. Acta Metall. Sin., 2017, 53: 1025
|
| 21 |
张银辉, 冯 强. W对新型Nb稳定化奥氏体耐热铸钢1000℃蠕变行为的影响 [J]. 金属学报, 2017, 53: 1025
|
| 22 |
Zhang X, Li D Z, Li Y Y, et al. Effect of aging treatment on the microstructures and mechanical properties evolution of 25Cr-20Ni austenitic stainless steel weldments with different Nb contents [J]. J. Mater. Sci. Technol., 2019, 35: 520
|
| 23 |
Peng Z F, Ren W, Yang C, et al. Relationship between the evolution of phase parameters of grain boundary M23C6 and embrittlement of HR3C super-heater tubes in service [J]. Acta Metall. Sin., 2015, 51: 1325
|
| 23 |
彭志方, 任 文, 杨 超等. HR3C钢运行过热器管的脆化与晶界M23C6相参量演化的关系 [J]. 金属学报, 2015, 51: 1325
|
| 24 |
Lv Z Q, Dong F, Zhou Z A, et al. Structural properties, phase stability and theoretical hardness of Cr23-xMxC6 (M=Mo, W; x=0-3) [J]. J. Alloys Compd., 2014, 607: 207
|
| 25 |
Kaneko K, Fukunaga T, Yamada K, et al. Formation of M23C6-type precipitates and chromium-depleted zones in austenite stainless steel [J]. Scr. Mater., 2011, 65: 509
|
| 26 |
Medvedeva N I, Van Aken D C, Medvedeva J E. Stability of binary and ternary M23C6 carbides from first principles [J]. Comput. Mater. Sci., 2015, 96: 159
|
| 27 |
Alomari A S, Kumar N, Murty K L. Creep behavior and microstructural evolution of a Fe-20Cr-25Ni (mass percent) austenitic stainless steel (alloy 709) at elevated temperatures [J]. Metall. Mater. Trans., 2019, 50A: 641
|
| 28 |
Fukunaga T, Kaneko K, Kawano R, et al. Formation of intergranular M23C6 in sensitized type-347 stainless steel [J]. ISIJ Int., 2014, 54: 148
|
| 29 |
Shao Y, Li Y M, Liu C X, et al. Annealing process optimization of high frequency longitudinal resistance welded low-carbon ferritic stainless steel pipe [J]. Acta Metall. Sin., 2019, 55: 1367
|
| 29 |
邵 毅, 李彦默, 刘晨曦等. 低碳铁素体不锈钢高频直缝电阻焊管退火工艺优化 [J]. 金属学报, 2019, 55: 1367
|
| 30 |
Zheng L, Hu X, Kang X, et al. Precipitation of M23C6 and its effect on tensile properties of 0.3C-20Cr-11Mn-1Mo-0.35N steel [J]. Mater. Des., 2015, 78: 42
|
| 31 |
Dong J, Zhou X S, Liu Y C, et al. Carbide precipitation in Nb-V-Ti microalloyed ultra-high strength steel during tempering [J]. Mater. Sci. Eng., 2017, A683: 215
|
| 32 |
Zhang Z, Hu Z F, Tu H Y, et al. Microstructure evolution in HR3C austenitic steel during long-term creep at 650oC [J]. Mater. Sci. Eng., 2017, A681: 74
|
| 33 |
Zhou Q W, Ping S B, Meng X B, et al. Precipitation kinetics of M23C6 carbides in the Super304H austenitic heat-resistant steel [J]. J. Mater. Eng. Perform., 2017, 26: 6130
|
| 34 |
Yan J B, Gu Y F, Sun F, et al. Evolution of microstructure and mechanical properties of a 25Cr-20Ni heat resistant alloy after long-term service [J]. Mater. Sci. Eng., 2016, A675: 289
|
| 35 |
Wang W, Wang Z W, Li W S, et al. Evolution of M23C6 phase in HR3C steel aged at 650oC [J]. Mater. High Temp., 2016, 33: 276
|
| 36 |
Zhang X, Li H W, Zhan M, et al. Electron force-induced dislocations annihilation and regeneration of a superalloy through electrical in-situ transmission electron microscopy observations [J]. J. Mater. Sci. Technol., 2020, 36: 79
|
| 37 |
Wu J, Liu Y C, Li C, et al. Recent progress of microstructure evolution and performance of multiphase Ni3Al-based intermetallic alloy with high Fe and Cr contents [J]. Acta Metall. Sin., 2020, 56: 21
|
| 37 |
吴 静, 刘永长, 李 冲等. 高Fe、Cr含量多相Ni3Al基高温合金组织与性能研究进展 [J]. 金属学报, 2020, 56: 21
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|