| 电解液温度对直流电解沉积纳米孪晶Cu微观结构的影响 |
程钊1,2, 金帅1, 卢磊1( ) |
1 中国科学院金属研究所沈阳材料科学国家(联合)实验室 沈阳 110016 2 中国科学技术大学材料科学与工程学院 沈阳 110016 |
|
| Effect of Electrolyte Temperature on Microstructures of Direct-Current Electrodeposited Nanotwinned Cu |
Zhao CHENG1,2, Shuai JIN1, Lei LU1( ) |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences,Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
程钊, 金帅, 卢磊. 电解液温度对直流电解沉积纳米孪晶Cu微观结构的影响[J]. 金属学报, 2018, 54(3): 428-434.
Zhao CHENG,
Shuai JIN,
Lei LU.
Effect of Electrolyte Temperature on Microstructures of Direct-Current Electrodeposited Nanotwinned Cu[J]. Acta Metall Sin, 2018, 54(3): 428-434.
| [1] | Lu L, Shen Y S, Chen X H, et al.Ultrahigh strength and high electrical conductivity in copper[J]. Science, 2004, 304: 422 | | [2] | Lu L, Chen X H, Huang X, et al.Revealing the maximum strength in nanotwinned copper[J]. Science, 2009, 323: 607 | | [3] | You Z S, Lu L, Lu K.Tensile behavior of columnar grained Cu with preferentially oriented nanoscale twins[J]. Acta Mater., 2011, 59: 6927 | | [4] | Pan Q S, Lu Q H, Lu L.Fatigue behavior of columnar-grained Cu with preferentially oriented nanoscale twins[J]. Acta Mater., 2013, 61: 1383 | | [5] | Pan Q S, Lu L.Strain-controlled cyclic stability and properties of Cu with highly oriented nanoscale twins[J]. Acta Mater., 2014, 81: 248 | | [6] | Chen K C, Wu W W, Liao C N, et al.Observation of atomic diffusion at twin-modified grain boundaries in copper[J]. Science, 2008, 321: 1066 | | [7] | Chen X H, Lu L, Lu K.Grain size dependence of tensile properties in ultrafine-grained Cu with nanoscale twins[J]. Scr. Mater., 2011, 64: 311 | | [8] | Lu K, Lu L, Suresh S.Strengthening materials by engineering coherent internal boundaries at the nanoscale[J]. Science, 2009, 324: 349 | | [9] | Zhang X, Misra A, Wang H, et al.Enhanced hardening in Cu/330 stainless steel multilayers by nanoscale twinning[J]. Acta Mater., 2004, 52: 995 | | [10] | Zhang X, Anderoglu O, Hoagland R G, et al.Nanoscale growth twins in sputtered metal films[J]. JOM, 2008, 60(9): 75 | | [11] | Liu C M, Lin H W, Lu C L, et al.Effect of grain orientations of Cu seed layers on the growth of <111>-oriented nanotwinned Cu[J]. Sci. Rep., 2014, 4: 6123 | | [12] | Liu T C, Liu C M, Hsiao H Y, et al.Fabrication and characterization of (111)-oriented and nanotwinned Cu by Dc electrodeposition[J]. Cryst. Growth Des., 2012, 12: 5012 | | [13] | Jin S, Pan Q S, Lu L.Microstructure dependence of direct-current electrodeposited bulk Cu with preferentially oriented nanotwins on the current densities[J]. Acta Metall. Sin., 2013, 49: 635(金帅, 潘庆松, 卢磊. 电流密度对直流电解沉积纳米孪晶Cu微观结构的影响 [J]. 金属学报, 2013, 49: 635) | | [14] | Hasegawa M, Mieszala M, Zhang Y C, et al.Orientation-controlled nanotwinned copper prepared by electrodeposition[J]. Electrochim. Acta, 2015, 178: 458 | | [15] | Chan T C, Chueh Y L, Liao C N.Manipulating the crystallographic texture of nanotwinned Cu films by electrodeposition[J]. Cryst. Growth Des., 2011, 11: 4970 | | [16] | Jin S, Cheng Z, Pan Q S, et al.Effect of electrolyte additive concentration on microstructure of direct-current electrodeposited nanotwinned Cu[J]. Acta Metall. Sin., 2016, 52: 973(金帅, 程钊, 潘庆松等. 添加剂浓度对直流电解沉积纳米孪晶Cu微观结构的影响 [J]. 金属学报, 2016, 52: 973) | | [17] | Seo S, Jin S, Wang G, et al.The effect of copper dissolution in acidic electrolyte on the formation of nanotwin in pulse electrodeposited copper[J]. J. Electrochem. Soc., 2014, 161: D425 | | [18] | Natter H, Hempelmann R.Nanocrystalline copper by pulsed electrodeposition: The effects of organic additives, bath temperature, and pH[J]. J. Phys. Chem., 1996, 100: 19525 | | [19] | Kang J X, Zhao W Z, Zhang G F.Influence of electrodeposition parameters on the deposition rate and microhardness of nanocrystalline Ni coatings[J]. Surf. Coat. Technol., 2009, 203: 1815 | | [20] | Liao C N, Lin C Y, Huang C L, et al.Morphology, texture and twinning structure of Cu films prepared by low-temperature electroplating[J]. J. Electrochem. Soc., 2013, 160: D3070 | | [21] | Cohen-Atiya M, Mandler D. Studying thiol adsorption on Au, Ag and Hg surfaces by potentiometric measurements [J]. J. Electroanal. Chem., 2003, 550-551: 267 | | [22] | Zhang Q B, Hua Y X, Dong T G, et al.Effects of temperature and current density on zinc electrodeposition from acidic sulfate electrolyte with [BMIM]HSO4 as additive[J]. J. Appl. Electrochem., 2009, 39: 1207 | | [23] | Cifuentes L, Simpson J.Temperature dependence of the cathodic and anodic kinetics in a copper electrowinning cell based on reactive electrodialysis[J]. Chem. Eng. Sci., 2005, 60: 4915 | | [24] | Nikoli? N D, Pavlovi? L J, Pavlovi? M G, et al.Effect of temperature on the electrodeposition of disperse copper deposits[J]. J. Serb. Chem. Soc., 2007, 72: 1369 | | [25] | Gründer Y, Markovic N M, Thompson P, et al.Temperature effects on the atomic structure and kinetics in single crystal electrochemistry[J]. Surf. Sci., 2015, 631: 123 | | [26] | Li D.Principles of Electrochemistry [M]. 3rd Ed., Beijing: Beijing University of Aeronautics and Astronautics Press, 2008: 286(李荻. 电化学原理 [M]. 第3版. 北京: 北京航空航天大学出版社, 2008: 286) | | [27] | Mallik A.An analysis on the effect of temperature on electrocrystallization mechanism during deposition of Cu thin films[J]. Trans. Indian Inst. Met., 2013, 66: 79 | | [28] | Milchev A, Montenegro M I.A galvanostatic study of electrochemical nucleation[J]. J. Electroanal. Chem., 1992, 333: 93 | | [29] | Kanani N.Electroplating: Basic Principles, Processes and Practice[M]. Berlin: Elsevier, 2005: 150 | | [30] | Bufford D C, Wang Y M, Liu Y, et al.Synthesis and microstructure of electrodeposited and sputtered nanotwinned face-centered-cubic metals[J]. MRS Bull., 2016, 41: 286 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|