坩埚尺寸和电磁频率对半固态A356铝合金浆料流动的影响 |
刘政1( ), 陈志平1, 陈涛2 |
1 江西理工大学机电工程学院 赣州 341000 2 江西理工大学材料科学与工程学院 赣州 341000 |
|
Effects of Crucible Size and Electromagnetic Frequency on Flow During Fabrication of Semisolid A356 Al Alloy Slurry |
Zheng LIU1( ), Zhiping CHEN1, Tao CHEN2 |
1 School of Mechanical and Electronic Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China 2 School of Materials Science and Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China |
引用本文:
刘政, 陈志平, 陈涛. 坩埚尺寸和电磁频率对半固态A356铝合金浆料流动的影响[J]. 金属学报, 2018, 54(3): 435-442.
Zheng LIU,
Zhiping CHEN,
Tao CHEN.
Effects of Crucible Size and Electromagnetic Frequency on Flow During Fabrication of Semisolid A356 Al Alloy Slurry[J]. Acta Metall Sin, 2018, 54(3): 435-442.
[1] | Kang C G, Bae J W, Kim B M. The grain size control of A356 aluminum alloy by horizontal electromagnetic stirring for rheology forging [J]. J. Mater. Process. Technol., 2007, 187-188: 344 | [2] | Chung I G, Bolouri A, Kang C G.A study on semisolid processing of A356 aluminum alloy through vacuum-assisted electromagnetic stirring[J]. Int. J. Adv. Manuf. Technol., 2012, 58: 237 | [3] | Liu Z, Mao W M, Zhao Z D.Effect of pouring temperature on semi-solid slurry of A356 Al alloy prepared by weak electromagnetic stirring[J]. Trans. Nonferrous Met. Soc. China, 2006, 16: 71 | [4] | Barman N, Kumar P, Dutta P.Studies on transport phenomena during solidification of an aluminum alloy in the presence of linear electromagnetic stirring[J]. J. Mater. Process. Technol., 2009, 209: 5912 | [5] | Dao V L, Zhao S D, Lin W J.Numerical and experimental study on effect of process parameters on preparation of A356 aluminum alloy semi-solid slurry by electromagnetic stirring[J]. Int. J. Appl. Electrom., 2013, 41: 153 | [6] | Zhang Z F, Chen X R, Xu J, et al.Numerical simulation on electromagnetic field, flow field and temperature field in semisolid slurry preparation by A-EMS[J]. Rare Met., 2010, 29: 635 | [7] | Liu Z, Zhang J Y.Research on morphology evolution of different rare-earth elements on primary phase in semisolid aluminum alloy under chaotic advection[J]. J. Mech. Eng., 2016, 52(16): 77(刘政, 张嘉艺. 混沌对流中不同稀土元素对半固态铝合金初生相形貌研究 [J]. 机械工程学报, 2016, 52(16): 77) | [8] | Xu J F, Wei B B.Liquid phase flow and microstructure formation during rapid solidification[J]. Acta. Phys. Sin., 2004, 53: 1909(徐锦锋, 魏炳波. 急冷快速凝固过程中液相流动与组织形成的相关规律 [J]. 物理学报, 2004, 53: 1909) | [9] | Wang J, Zhou Y, Lan S, et al.Numerical simulation and chaotic analysis of an aluminum holding furnace[J]. Metall. Mater. Trans., 2014, 45B: 2194 | [10] | Liu Z, Liu X M, Hu C H, et al.Research on fractal characteristics of primary phase morphology in semi-solid A356 alloy[J]. Acta Metall. Sin.(Engl. Lett.), 2009, 22: 421 | [11] | Hu Z H, Wu G H, Zhang P, et al.Primary phase evolution of rheo-processed ADC12 aluminum alloy[J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 19 | [12] | Nikrityuk P A, Eckert K, Grundmann R.A numerical study of unidirectional solidification of a binary metal alloy under influence of a rotating magnetic field[J]. Int. J. Heat Mass Transfer, 2006, 49: 1501 | [13] | Dadzis K, Lukin G, Meier D, et al.Directional melting and solidification of gallium in a traveling magnetic field as a model experiment for silicon processes[J]. J. Cryst. Growth, 2016, 445: 90 | [14] | Zhao J Z, Li H L, Zhao L.Effects of convections and motions of minority phase droplets on solidification of monotectic alloys[J]. Acta Metall. Sin., 2009, 45: 1435(赵九洲, 李海丽, 赵雷. 对流和弥散相液滴运动对偏晶合金凝固的影响 [J]. 金属学报, 2009, 45: 1435) | [15] | Wang J, Fautrelle Y, Nguyen-Thi H, et al.Thermoelectric magnetohydrodynamic flows and their induced change of solid-liquid interface shape in static magnetic field-assisted directional solidification[J]. Metall. Mater. Trans., 2016, 47A: 1169 | [16] | Wang B, Wang X D, Etay J, et al.Flow driven by an archimedean helical permanent magnetic field. Part I: Flow patterns and their transitions[J]. Metall. Mater. Trans., 2016, 47B: 1369 | [17] | Chowdhury J, Ganguly S, Chakraborty S.Numerical simulation of transport phenomena in electromagnetically stirred semi-solid materials processing[J]. J. Phys., 2005, 38D: 2869 | [18] | Chen X R, Zhang Z F, Xu J, et al.Numerical simulation of electromagnetic field, flow field and temperature field in semi-solid slurry preparation by electromagnetic stirring[J]. Chin. J. Nonferrous Met., 2010, 20: 937(陈兴润, 张志峰, 徐骏等. 电磁搅拌法制备半固态浆料过程电磁场、流场和温度场的数值模拟 [J]. 中国有色金属学报, 2010, 20: 937) | [19] | Tao W Y, Zhao S D, Lin W J.Numerical simulation on A356 aluminum alloy semi-solid slurry preparation with electromagnetic stirring[J]. J. Mech. Eng., 2012, 48(14): 50(陶文琉, 赵升吨, 林文捷. A356铝合金半固态浆料电磁搅拌法制备过程的数值模拟 [J]. 机械工程学报, 2012, 48(14): 50) | [20] | Liu Z, Zhang J Y, Yu Z F.Simulation and analysis on chaotic characteristic of flow in Al alloy melt under electromagnetic field[J]. Chin. J. Nonferrous Met., 2015, 25: 3026(刘政, 张嘉艺, 余昭福. 电磁场作用下中铝合金熔体流动的混沌特征的仿真与分析 [J]. 中国有色金属学报, 2015, 25: 3026) | [21] | Liu Z, Liu X M, Zhu T, et al.Effects of electromagnetic stirring with low current frequency on RE distribution in semisolid aluminum alloy[J]. Acta Metall. Sin., 2015, 51: 272(刘政, 刘小梅, 朱涛等. 低频电磁搅拌对半固态铝合金中稀土分布的影响 [J]. 金属学报, 2015, 51: 272) | [22] | Liu Z, Zhang J Y, Luo H L, et al.Research on morphology evolution of primary phase in semisolid A356 alloy under chaotic advection[J]. Acta Metall. Sin., 2016, 52: 177(刘政, 张嘉艺, 罗浩林等. 混沌对流下的半固态A356铝合金初生相形貌演变研究 [J]. 金属学报, 2016, 52: 177) | [23] | Yin J F, You Y X, Li W, et al.Numerical analysis for the characteristics of flow control around a circular cylinder with a turbulent boundary layer separation using the electromagnetic force[J]. Acta Phys. Sin., 2014, 63: 206(尹纪富, 尤云祥, 李巍等. 电磁力控制湍流边界层分离圆柱绕流场特性数值分析 [J]. 物理学报, 2014, 63: 206) | [24] | Bai X W, Zhang H O, Zhou X M, et al.Electromagneto-fluid coupling simulation of arc rapid prototyping process with external high-frequency magnetic field[J]. J. Mech. Eng., 2016, 52(4): 60(柏兴旺, 张海鸥, 周祥曼等. 外加高频磁场下电弧快速成形过程的电磁-流体耦合数值模拟 [J]. 机械工程学报, 2016, 52(4): 60) | [25] | Wang C Z, Liu F G, Zhang Y T, et al.Numerical simulation on electromagnetic, thermal and fluid fields in preparing process of semi-solid slurry[J]. J. Shenyang Univ. Technol., 2010, 32: 279(王承志, 刘凤国, 张玉妥等. 半固态浆料制备过程的电磁热流体数值模拟 [J]. 沈阳工业大学学报, 2010, 32: 279) | [26] | Liu H P, Xu M G, Qiu S T, et al.Numerical simulation of fluid flow in a round bloom mold with in-mold rotary electromagnetic stirring[J]. Metall. Mater. Trans., 2012, 43B: 1657 | [27] | Zhao Q, Zhang X G, Zhang H Y, et al.Numerical simulation of spiral magnetic field of electromgnetic stirring[J]. Chin. J. Nonferrous Met., 2014, 24: 1041(赵倩, 张兴国, 张环月等. 螺旋磁场电磁搅拌的数值模拟 [J]. 中国有色金属学报, 2014, 24: 1041) | [28] | Zhang J, Wang E G, Deng A Y, et al.Effects of mold EMS parameters on distributions of magnetic induction and electromagnetic force during continuous casting[J]. J. Northeastern Univ.(Nat. Sci.), 2010, 31: 1432(张 静, 王恩刚, 邓安元等. 连铸结晶器电磁搅拌参数对磁场分布的影响 [J]. 东北大学学报(自然科学版), 2010, 31: 1432) | [29] | Li N, Zhang R, Zhang L M, et al.Study on grain refinement mechanism of hypoeutectic Al-7%Si alloy under low voltage alternating current pulse[J]. Acta Metall. Sin., 2017, 53: 192(李宁, 张蓉, 张利民等. 低压交流电脉冲下Al-7%Si合金晶粒细化机理研究 [J]. 金属学报, 2017, 53: 192) |
|
|