| 新型超高强度钢Cr12Ni4Mo2Co14在酸性环境中的应力腐蚀行为* |
孙敏1( ),李晓刚2,李劲3 |
| 1 宝山钢铁股份有限公司研究院, 上海 2019002 北京科技大学材料科学与工程学院, 北京 1000833 复旦大学材料科学系, 上海 200433 |
|
| STRESS CORROSION CRACKING BEHAVIOR OF A NEW KIND OF ULTRAHIGH STRENGTH STEEL Cr12Ni4Mo2Co14 IN ACID ENVIRONMENT |
Min SUN1( ),Xiaogang LI2,Jin LI3 |
1 Research Institute, Baoshan Iron & Steel Co., Ltd., Shanghai 201900, China; 2 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 3 Department of Materials Science, Fudan University, Shanghai 200433, China ; |
引用本文:
孙敏,李晓刚,李劲. 新型超高强度钢Cr12Ni4Mo2Co14在酸性环境中的应力腐蚀行为*[J]. 金属学报, 2016, 52(11): 1372-1378.
Min SUN,
Xiaogang LI,
Jin LI.
STRESS CORROSION CRACKING BEHAVIOR OF A NEW KIND OF ULTRAHIGH STRENGTH STEEL Cr12Ni4Mo2Co14 IN ACID ENVIRONMENT[J]. Acta Metall Sin, 2016, 52(11): 1372-1378.
| [1] | Malakondaian G, Srinivas M, Rama R P.Prog Mater Sci, 1997; 42: 209 | | [2] | Hu Y B, Dong C F, Sun M, Xiao K, Zhong P, Li X G.Corros Sci, 2011; 53: 4159 | | [3] | Sundarama P A, Marble D K,J Alloys Compd, 2003; 360: 90 | | [4] | Ramadan S, Gaillet L, Tessier C, Idrissi H.Appl Surf Sci, 2008; 254: 2255 | | [5] | Eliaz N, Shachar A, Tal B, Eliezer D.Eng Fail Anal, 2002; 9: 167 | | [6] | Yang W, Ni R C, Hua H Z, Pourbaix A.Corro Sci, 1984; 24: 691 | | [7] | Zhong J Y, Sun M, Liu D B, Li X G, Liu T Q.Int J Miner Metall Mater, 2010; 17: 282 | | [8] | Liao Q C, Sun F Y, Lan F L,Acta Metall Sin, 1979; 15: 259 | | [8] | (廖乾初, 孙福玉, 蓝芬兰. 金属学报, 1979; 15: 259) | | [9] | Nagao A, Smith C D, Dadfarnia M, Sofronis P, Robertson I M.Procedia Mater Sci, 2014; 3: 1700 | | [10] | Shi X B, Yan W, Wang W, Zhao L Y, Shan Y Y, Yang K.J Iron Steel Res Int, 2015; 22: 937 | | [11] | Zhang Y, Chu W Y, Yuan R Z, Wang Y B, Ouyang S X, Xiao J M.Acta Metall Sin, 1995; 31: 406 | | [11] | (张跃, 褚武扬, 袁润章, 王燕斌, 欧阳世翕, 肖纪美. 金属学报, 1995; 31: 406) | | [12] | Rajabipour A, Melchers R E.Int J Hydrogen Energy, 2015; 40: 9388 | | [13] | Xie Y, Zhang J S.J Nucl Mater, 2015; 466: 85 | | [14] | Panda B, Sujata M, Madan M, Bhaumik S K.Eng Fail Anal, 2014; 36: 379 | | [15] | Lin B J.Acta Metall Sin, 1982; 18: 350(林保军. 金属学报, 1982; 18: 350) | | [16] | Ye D, Li S H, Li J, Jiang W, Su J, Zhao K Y.Mater Charact, 2015; 109: 100 | | [17] | Li M, Wang L, Almer J D.Acta Mater, 2014; 76: 381 | | [18] | Zhang G M, Zhou Z J, Mo K, Miao Y B, Liu X, Almer J, Stubbins J F.J Nucl Mater, 2015; 467: 50 | | [19] | Djukic M B, Zeravcic V S, Bakic G M, Sedmak A, Rajicic B.Eng Fail Anal, 2015; 58: 485 | | [20] | Weber S, Martin M, Theisen W.Mater Sci Eng, 2011; A528: 7688 | | [21] | Martin M, Weber S, Izawa C, Wagner S, Pundt A, Theisen W.Int J Hydrogen Energy, 2011; 36: 11195 | | [22] | Qiao L J, Zeng Y M, Chu W Y.J Chin Soc Corros Prot, 1998; 18: 233 | | [22] | (乔利杰, 曾一民, 褚武扬. 中国腐蚀与防护学报, 1998; 18: 233) |
|
|