| Nb/Ti比对铸造镍基高温合金长期时效组织演化的影响* |
| 孙文1,2, 秦学智2, 郭永安2, 郭建亭2, 楼琅洪2, 周兰章2 |
1 中国科学技术大学, 合肥 230022 2 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECTS OF Nb/Ti RATIOS ON THE MICROSTRUCTURAL EVOLUTIONS OF CAST Ni-BASED SUPERALLOYS DURING LONG-TERM THERMAL EXPOSURE |
| SUN Wen1,2, QIN Xuezhi2, GUO Yongan2, GUO Jianting2, LOU Langhong2, ZHOU Lanzhang2 |
1 University of Science and Technology of China, Hefei 230022 2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
孙文, 秦学智, 郭永安, 郭建亭, 楼琅洪, 周兰章. Nb/Ti比对铸造镍基高温合金长期时效组织演化的影响*[J]. 金属学报, 2014, 50(6): 744-752.
Wen SUN,
Xuezhi QIN,
Yongan GUO,
Jianting GUO,
Langhong LOU,
Lanzhang ZHOU.
EFFECTS OF Nb/Ti RATIOS ON THE MICROSTRUCTURAL EVOLUTIONS OF CAST Ni-BASED SUPERALLOYS DURING LONG-TERM THERMAL EXPOSURE[J]. Acta Metall Sin, 2014, 50(6): 744-752.
| [1] |
Ross E W, Sims C T. In: Sims C T, Stoloff N S, Hagel W C eds., Superalloys II, NY: Wiley, 1987: 97
|
| [2] |
Pollock T M. Mater Sci Eng, 1999; B32: 255
|
| [3] |
Giamei A F, Anton D L. Metall Trans, 1985; 16A: 1997
|
| [4] |
Rae C M F, Karunaratne M S A, Small C J, Broomfiels C N, Jones C N, Reed R C. Superalloys. Warrendale: TMS, 2000: 767
|
| [5] |
Koul A K, Castillo R. Metall Trans, 1988; 19A: 2049
|
| [6] |
Qin X Z, Guo J T, Yuan C, Chen C L, Ye H Q. Metall Mater Trans, 2007; 38A: 3014
|
| [7] |
Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 258
|
| [8] |
Qin X Z, Guo J T, Yuan C, Hou J S, Ye H Q. Mater Lett, 2008; 62: 2275
|
| [9] |
Qin X Z, Guo J T, Yuan C, Yang G X, Zhou L Z, Ye H Q. J Mater Sci, 2009; 44: 4840
|
| [10] |
Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; A37: 237
|
| [11] |
Choi B G, Kim I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329
|
| [12] |
Lvov G, Levit V I, Kaufman M J. Metall Mater Trans, 2004; 35A: 1669
|
| [13] |
Wang J, Zhou L Z, Qin X Z, Sheng L Y, Hou J S, Guo J T. Mater Sci Eng, 2012; A553: 14
|
| [14] |
Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Acta Metall Sin, 2010; 46: 213
|
| [14] |
(秦学智, 郭建亭, 袁超, 候介山, 周兰章, 叶恒强. 金属学报, 2010; 46: 213)
|
| [15] |
Ricks R, Porter A, Ecob R. Acta Metall, 1983; 31: 43
|
| [16] |
Gomez-Acebo T, Navarcorena B, Castro F. J Phase Equilibria, 2004; 25: 237
|
| [17] |
Japan Institute of Metals. Kinzoku Data Book. Tokyo: Maruzen, 1974: 24
|
| [18] |
ISIJ. Iron and Steel Handbook, Vol.I Fundamental. 3rd Ed, Tokyo: Maruzen, 1981: 350
|
| [19] |
Guo J T. Materials Science and Engineering for Superalloys, Vol.1. Beijing: Science Press, 2008: 126
|
| [19] |
(郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 126)
|
| [20] |
Jo T S, Kim S H, Kim D G, Park J Y, Kim Y D. Metall Mater Int, 2008; 14: 739
|
| [21] |
Mohammad A G, Mohsen M. Mater Des, 2011; 32: 2695
|
| [22] |
Cai Y L, Zheng Y R. Acta Metall Sin, 1982; 18: 30
|
| [22] |
(蔡榆林, 郑运荣. 金属学报, 1983; 18: 30)
|
| [23] |
Pessah-Simonetti M, Caron P, Khan T. Superalloys. Warrendale: TMS, 1992: 567
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|