温度对碳纳米管增强纳米蜂窝镍力学性能的影响 |
李源才, 江五贵( ), 周宇 |
南昌航空大学航空制造工程学院 南昌 330063 |
|
Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs |
LI Yuancai, JIANG Wugui( ), ZHOU Yu |
School of Aeronautical Manufacturing Engineering, Nanchang Hangkong University, Nanchang 330063, China |
引用本文:
李源才, 江五贵, 周宇. 温度对碳纳米管增强纳米蜂窝镍力学性能的影响[J]. 金属学报, 2020, 56(5): 785-794.
Yuancai LI,
Wugui JIANG,
Yu ZHOU.
Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs[J]. Acta Metall Sin, 2020, 56(5): 785-794.
1 |
Ivers-Tiffée E, Weber A, Herbstritt D. Materials and technologies for SOFC-components [J]. J. Eur. Ceram. Soc., 2001, 21: 1805
|
2 |
Xu M, Li T, Yang M, et al. Solid oxide fuel cell interconnect design optimization considering the thermal stresses [J]. Sci. Bull., 2016, 61: 1333
doi: 10.1007/s11434-016-1146-3
pmid: 27635282
|
3 |
Radovic M, Lara-Curzio E. Mechanical properties of tape cast nickel-based anode materials for solid oxide fuel cells before and after reduction in hydrogen [J]. Acta Mater., 2004, 52: 5747
doi: 10.1016/j.actamat.2004.08.023
|
4 |
Frandsen H L, Ramos T, Faes A, et al. Optimization of the strength of SOFC anode supports [J]. J. Eur. Ceram. Soc., 2012, 32: 1041
doi: 10.1016/j.jeurceramsoc.2011.11.015
|
5 |
Yu J H, Park G W, Lee S, et al. Microstructural effects on the electrical and mechanical properties of Ni-YSZ cermet for SOFC anode [J]. J. Power Sources, 2007, 163: 926
|
6 |
Ge X M, Chan S H, Liu Q L, et al. Solid oxide fuel cell anode materials for direct hydrocarbon utilization [J]. Adv. Energy Mater., 2012, 2: 1156
doi: 10.1021/ja206278f
pmid: 22011010
|
7 |
Halmenschlager C M, Korb M D A, Neagu R, et al. Nanostructured YSZ thin film for application as electrolyte in an electrode supported SOFC [J]. Mater. Sci. Forum, 2012, 727-728: 873
|
8 |
Ansar A, Soysal D, Schiller G. Nanostructured functional layers for solid oxide fuel cells [J]. Int. J. Energy Res., 2010, 33: 1191
|
9 |
Tsuchiya M, Lai B K, Ramanathan S. Scalable nanostructured membranes for solid-oxide fuel cells [J]. Nat. Nanotechnol., 2011, 6: 282
doi: 10.1038/nnano.2011.43
pmid: 21460827
|
10 |
Kang S, Su P C, Park Y I, et al. Thin-film solid oxide fuel cells on porous nickel substrates with multistage nanohole array [J]. J. Electrochem. Soc., 2006, 153: A554
|
11 |
Nelson P A, Elliott J M, Attard G S, et al. Mesoporous nickel/nickel oxide—A nanoarchitectured electrode [J]. Chem. Mater., 2002, 14: 524
doi: 10.1021/cm011021a
|
12 |
Nelson P A, Owen J R. A High-performance supercapacitor/battery hybrid incorporating templated mesoporous electrodes [J]. J. Electrochem. Soc., 2003, 150: A1313
|
13 |
Treacy M M J, Ebbesen T W, Gibson J. Exceptionally high Young's modulus observed for individual carbon nanotubes [J]. Nature, 1996, 381: 678
doi: 10.1038/381678a0
|
14 |
Ebbesen T W, Lezec H J, Hiura H, et al. Electrical conductivity of individual carbon nanotubes [J]. Nature, 1996, 382: 54
doi: 10.1038/382054a0
|
15 |
Berber S, Kwon Y K, Tománek D. Unusually high thermal conductivity of carbon nanotubes [J]. Phys. Rev. Lett., 2000, 84: 4613
doi: 10.1103/PhysRevLett.84.4613
pmid: 10990753
|
16 |
Qiao Y, Li C M, Bao S J, et al. Carbon nanotube/polyaniline composite as anode material for microbial fuel cells [J]. J. Power Sources, 2007, 170: 79
doi: 10.1016/j.bioelechem.2019.05.008
pmid: 31158799
|
17 |
Zhu W Z, Deevi S C. A review on the status of anode materials for solid oxide fuel cells [J]. Mater. Sci. Eng, 2003, A362: 228
|
18 |
Xie X, Hu L B, Pasta M, et al. Three-dimensional carbon nanotube-textile anode for high-performance microbial fuel cells [J]. Nano Lett., 2011, 11: 291
doi: 10.1021/nl103905t
pmid: 21158405
|
19 |
Peigney A, Laurent C, Flahaut E, et al. Carbon nanotubes in novel ceramic matrix nanocomposites [J]. Ceram. Int., 2000, 26: 677
doi: 10.1038/nmat793
pmid: 12652671
|
20 |
Qian D, Dickey E C, Andrews R, et al. Load transfer and deformation mechanisms in carbon nanotube-polystyrene composites [J]. Appl. Phys. Lett., 2000, 76: 2868
doi: 10.1046/j.1365-2818.2001.00940.x
pmid: 11580811
|
21 |
Curtin W A, Sheldon B W. CNT-reinforced ceramics and metals [J]. Materialstoday, 2004, 7: 44
|
22 |
Song Q S, Aravindaraj G K, Sultana H, et al. Performance improvement of pasted nickel electrodes with multi-wall carbon nanotubes for rechargeable nickel batteries [J]. Electrochim. Acta, 2007, 53: 1890
|
23 |
Jiang J, Liu J P, Zhou W W, et al. CNT/Ni hybrid nanostructured arrays: synjournal and application as high-performance electrode materials for pseudocapacitors [J]. Energy Environ. Sci., 2011, 4: 5000
|
24 |
Jang J W, Choi H J, Kwon O H, et al. Densification behavior and electrical properties of carbon nanotube-Ni nanocomposite films for co-fireable microcircuit electrodes [J]. Thin Solid Films, 2018, 660: 754
|
25 |
Liu X, Gurel V, Morris D, et al. Bioavailability of nickel in single-wall carbon nanotubes [J]. Adv. Mater., 2007, 19: 2790
|
26 |
Chen Y S, Huang J H. Arrayed CNT-Ni nanocomposites grown directly on Si substrate for amperometric detection of ethanol [J]. Biosens. Bioelectron., 2010, 26: 207
doi: 10.1016/j.bios.2010.06.016
pmid: 20637593
|
27 |
Choi T, Kim S H, Lee C W, et al. Synjournal of carbon nanotube-nickel nanocomposites using atomic layer deposition for high-performance non-enzymatic glucose sensing [J]. Biosens. Bioelectron., 2015, 63: 325
doi: 10.1016/j.bios.2014.07.059
pmid: 25113051
|
28 |
Lin T C, Huang B R. Palladium nanoparticles modified carbon nanotube/nickel composite rods (Pd/CNT/Ni) for hydrogen sensing [J]. Sens. Actuators, 2012, 162B: 108
|
29 |
Esfarjani K, Gorjizadeh N, Nasrollahi Z. Molecular dynamics of single wall carbon nanotube growth on nickel surface [J]. Computat. Mater. Sci., 2006, 36: 117
doi: 10.1166/jnn.2004.063
pmid: 15296231
|
30 |
Shibuta Y, Maruyama S. A molecular dynamics study of the effect of a substrate on catalytic metal clusters in nucleation process of single-walled carbon nanotubes [J]. Chem. Phys. Lett., 2007, 437: 218
doi: 10.1016/j.cplett.2007.02.019
|
31 |
Oguri T, Shimamura K, Shibuta Y, et al. Ab initio molecular dynamics simulation of the dissociation of ethanol on a nickel cluster: Understanding the initial stage of metal-catalyzed growth of carbon nanotubes [J]. J. Phys. Chem., 2013, 117C: 9983
|
32 |
Fukuhara S, Shimojo F, Shibuta Y. Conformation and catalytic activity of nickel-carbon cluster for ethanol dissociation in carbon nanotube synjournal: Ab initio molecular dynamics simulation [J]. Chem. Phys. Lett., 2017, 679: 164
|
33 |
Song H Y, Zha X W. Influence of nickel coating on the interfacial bonding characteristics of carbon nanotube-aluminum composites [J]. Comput. Mater. Sci., 2010, 49: 899
|
34 |
Song H Y, Zha X W. Mechanical properties of nickel-coated single-walled carbon nanotubes and their embedded gold matrix composites [J]. Phys. Lett., 2010, 374A: 1068
|
35 |
Zhou X, Song S Y, Li L, et al. Molecular dynamics simulation for mechanical properties of magnesium matrix composites reinforced with nickel-coated single-walled carbon nanotubes [J]. J. Compos. Mater., 2015, 50: 191
|
36 |
Duan K, Li L, Hu Y J, et al. Enhanced interfacial strength of carbon nanotube/copper nanocomposites via Ni-coating: Molecular-dynamics insights [J]. Physica, 2017, 88E: 259
doi: 10.1111/j.1755-3768.2010.01997.x
pmid: 20977690
|
37 |
Zhang H F, Yan H L, Jia N, et al. Exploring plastic deformation mechanism of multilayered Cu/Ti composites by using molecular dynamics modeling [J]. Acta Metall. Sin., 2018, 54: 1333
|
37 |
张海峰, 闫海乐, 贾 楠等. Cu/Ti纳米层状复合体塑性变形机制的分子动力学模拟研究 [J]. 金属学报, 2018, 54: 1333
|
38 |
Zhou Y, Jiang W G, Li D S, et al. Study on lightweight and strengthening effect of carbon nanotube in highly ordered nanoporous nickel: A molecular dynamics study [J]. Appl. Sci., 2019, 9: 352
|
39 |
Atkinson A, Barnett S, Gorte R J, et al. Advanced anodes for high-temperature fuel cells [J]. Nat. Mater., 2004, 3: 17
doi: 10.1038/nmat1040
pmid: 14704781
|
40 |
Foiles S M, Baskes M I, Daw M S. Embedded-atom-method functions for the fcc metals Cu, Ag, Au, Ni, Pd, Pt, and their alloys [J]. Phys. Rev., 1986, 33B: 7983
|
41 |
Stuart S J, Tutein A B, Harrison J A. A reactive potential for hydrocarbons with intermolecular interactions [J]. J. Chem. Phys., 2000, 112: 6472
|
42 |
Lennard-Jones J E. Cohesion [J]. Proc. Phys. Soc., 1931, 43: 461
|
43 |
Boda D, Henderson D. The effects of deviations from Lorentz-Berthelot rules on the properties of a simple mixture [J]. Mol. Phys., 2008, 106: 2367
|
44 |
Kutana A, Giapis K P. Transient deformation regime in bending of single-walled carbon nanotubes [J]. Phys. Rev. Lett., 2006, 97: 245501
doi: 10.1103/PhysRevLett.97.245501
pmid: 17280296
|
45 |
Jiang L Y, Huang Y, Jiang H, et al. A cohesive law for carbon nanotube/polymer interfaces based on the van der Waals force [J]. J. Mech. Phys. Solids, 2006, 54: 2436
|
46 |
Choi B K, Yoon G H, Lee S. Molecular dynamics studies of CNT-reinforced aluminum composites under uniaxial tensile loading [J]. Composites, 2016, 91B: 119
|
47 |
Yi L J, Chang T C, Feng X Q, et al. Giant energy absorption capacity of graphene-based carbon honeycombs [J]. Carbon, 2017, 118: 348
|
48 |
Zhou Y, Jiang W G, Feng X Q, et al. In-plane compressive behavior of graphene-coated aluminum nano-honeycombs [J]. Comput. Mater. Sci., 2019, 156: 396
|
49 |
Wen Y H, Zhu Z Z, Zhu R Z. Molecular dynamics study of the mechanical behavior of nickel nanowire: Strain rate effects [J]. Comput. Mater. Sci., 2008, 41: 553
|
50 |
Wen Y H, Zhang Y, Zhu Z Z. Size-dependent effects on equilibrium stress and strain in nickel nanowires [J]. Phys. Rev., 2007, 76B: 125423
|
51 |
Rezaei R, Shariati M, Tavakoli-Anbaran H, et al. Mechanical characteristics of CNT-reinforced metallic glass nanocomposites by molecular dynamics simulations [J]. Comput. Mater. Sci., 2016, 119: 19
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|