感应加热异温轧制制备钢/铝复合板 |
肖宏,许朋朋,祁梓宸(),吴宗河,赵云鹏 |
燕山大学国家冷轧板带装备及工艺工程技术研究中心 秦皇岛 066004 |
|
Preparation of Steel/Aluminum Laminated Composites by Differential Temperature Rolling with Induction Heating |
XIAO Hong,XU Pengpeng,QI Zichen(),WU Zonghe,ZHAO Yunpeng |
National Engineering Research Center for Equipment and Technology of Cold Strip Rolling, Yanshan University, Qinhuangdao 066004, China |
引用本文:
肖宏,许朋朋,祁梓宸,吴宗河,赵云鹏. 感应加热异温轧制制备钢/铝复合板[J]. 金属学报, 2020, 56(2): 231-239.
Hong XIAO,
Pengpeng XU,
Zichen QI,
Zonghe WU,
Yunpeng ZHAO.
Preparation of Steel/Aluminum Laminated Composites by Differential Temperature Rolling with Induction Heating[J]. Acta Metall Sin, 2020, 56(2): 231-239.
[1] | Liu G. Applications of steel-aluminum compound track in construction of line Daxing in Beijing urban mass transit [J]. Rail. Stand. Des., 2011, (1): 119 | [1] | (刘 岗. 钢铝复合轨在北京市轨道交通大兴线工程中的应用 [J]. 铁道标准设计, 2011, (1): 119) | [2] | Wang C, Wang L Y, Zhao H Q, et al. Application of steel-aluminum composite plate-beam structure in car body [J]. Sci. Technol. Inform., 2012, (35): 140 | [2] | (王 冲, 王立颖, 赵鹤群等. 钢铝复合板梁式结构在车体上的应用 [J]. 科技信息, 2012, (35): 140) | [3] | Han H D, Zhang P, Du Y H, et al. Research on manufacture for steel-backed aluminum-matrix bearing material [J]. Intern. Combust. Eng. Parts, 2008, (3): 18 | [3] | (韩海东, 张 鹏, 杜云慧等. 钢背铝基轴瓦材料复合新工艺探索 [J]. 内燃机配件, 2008, (3): 18) | [4] | Liu L X. Corrosion and protection of joint of steel-Al explosive cladding [J]. Ordn. Mater. Sci. Eng., 2003, 26(1): 36 | [4] | (刘玲霞. 钢-铝爆炸复合接头材料的腐蚀与防护 [J]. 兵器材料科学与工程, 2003, 26(1): 36) | [5] | Shiran M K G, Khalaj G, Pouraliakbar H, et al. Effects of heat treatment on the intermetallic compounds and mechanical properties of the stainless steel 321-aluminum 1230 explosive-welding interface [J]. Int. J. Min. Met. Mater., 2017, 24: 1267 | [6] | Song L, Sun B Y, Cui P P. Study on steel/aluminum solid-liquid composite casting and rolling [J]. Hot Work. Technol, 2018, 47(4): 126 | [6] | (宋 黎, 孙斌煜, 崔鹏鹏. 钢/铝固液复合铸轧研究 [J]. 热加工工艺, 2018, 47(4): 126) | [7] | Grydin O, Gerstein G, Nürnberger F, et al. Twin-roll casting of aluminum-steel clad strips [J]. J. Manuf. Process., 2013, 15: 501 | [8] | Movahedi M, Kokabi A H, Seyed Reihani S M. Investigation on the bond strength of Al-1100/St-12 roll bonded sheets, optimization and characterization [J]. Mater. Des., 2011, 32: 3143 | [9] | Manesh H D, Taheri A K. Study of mechanisms of cold roll welding of aluminium alloy to steel strip [J]. Mater. Sci. Technol., 2004, 20: 1064 | [10] | Manesh H D, Shahabi H S. Effective parameters on bonding strength of roll bonded Al/St/Al multilayer strips [J]. J. Alloys Compd., 2009, 476: 292 | [11] | Wang C Y, Jiang Y B, Xi J X, et al. Interface formation and bonding mechanism of embedded aluminum-steel composite sheet during cold roll bonding [J]. Mater. Sci. Eng., 2017, A708: 50 | [12] | Wang C Y, Jiang Y B, Xie J X, et al. Effect of the steel sheet surface hardening state on interfacial bonding strength of embedded aluminum-steel composite sheet produced by cold roll bonding process [J]. Mater. Sci. Eng., 2016, A652: 51 | [13] | Wu B, Li L, Xia C D, et al. Effect of surface nitriding treatment in a steel plate on the interfacial bonding strength of the aluminum/steel clad sheets by the cold roll bonding process [J]. Mater. Sci. Eng., 2017, A682: 270 | [14] | Gao C, Li L, Chen X, et al. The effect of surface preparation on the bond strength of Al-St strips in CRB process [J]. Mater. Des., 2016, 107: 205 | [15] | Wang C Y, Liu X H, Jiang Y B, et al. Effects of annealing and cold roll-bonded interface on the microstructure and mechanical properties of the embedded aluminum-steel composite sheet [J]. Sci. Bull., 2018, 63: 1448 | [16] | Chen X, Li L, Zhou D J. Review on the formation and inhibition mechanism of Fe-Al intermetallic compound [J]. Mater. Rev., 2016, 30(13): 125 | [16] | (陈 鑫, 李 龙, 周德敬. 铝钢金属间化合物生长及其抑制机理的研究现状 [J]. 材料导报, 2016, 30(13): 125) | [17] | Tang C L, Xu Q P, Weng H, et al. Influence of the surface treatment process on bonding properties of Al/steel(4A60/08AL) clad sheets by cold roll bonding [J]. Light Alloy Fabric. Technol., 2016, 44(6): 25 | [17] | (唐超兰, 许秋平, 翁 浩等. 表面处理工艺对冷轧铝/钢(4A60/08AL)复合板结合性能的影响 [J]. 轻合金加工技术, 2016, 44(6): 25) | [18] | Li M Q, Jiang F L, Zhang H, et al. Deformation rule of steel/aluminum metal-laminate material during hot roll bonding [J]. Chin. J. Nonferrous Met., 2009, 19: 644 | [18] | (李民权, 蒋福林, 张 辉等. 钢/铝复合板热轧复合变形规律 [J]. 中国有色金属学报, 2009, 19: 644) | [19] | Nezhad M S A, Ardakani A H. A study of joint quality of aluminum and low carbon steel strips by warm rolling [J]. Mater. Des., 2009, 30: 1103 | [20] | Yu J M, Yu Z S, Qi K M, et al. Bonding mechanism of steel-Al clad plate by rolling at different temperature [J]. Iron Steel, 1995, 30(8): 44 | [20] | (于九明, 于长生, 齐克敏等. 钢和铝异温轧制复合机理的研究 [J]. 钢铁, 1995, 30(8): 44) | [21] | Xiao H, Qi Z C, Yu C, et al. Preparation and properties for Ti/Al clad plates generated by differential temperature rolling [J]. J. Mater. Process. Technol., 2017, 249: 285 | [22] | Qi Z C, Yu C, Xiao H. Microstructure and bonding properties of magnesium alloy AZ31/CP-Ti clad plates fabricated by rolling bonding [J]. J. Manuf. Processes., 2018, 32: 175 | [23] | Jiao H, Zhang M, Yan Z J. Study on binding property of steel/aluminum laminated sheets fabricated by two-pass hot rolling [J]. New Technol. New Processes, 2015, (8): 95 | [23] | (焦 宏, 张 敏, 闫中建. 两道次热轧法制备钢/铝复合板的结合性能研究 [J]. 新技术新工艺, 2015, (8): 95) | [24] | Li L, Zeng X Y, Chen X, et al. Influence of heat treatment on microstructure and mechanical properties of 4A60 Al/08Al steel clad strip by cold roll bonding [J]. Heat Treat. Met., 2015, 40(7): 28 | [24] | (李 龙, 曾祥勇, 陈 鑫等. 热处理对冷轧4A60铝/08Al钢复合带材组织及力学性能的影响 [J]. 金属热处理, 2015, 40(7): 28) | [25] | Manesh H D, Taheri A K. Bond strength and formability of an aluminum-clad steel sheet [J]. J. Alloys Compd., 2003, 361: 138 | [26] | Sauvage X, Dinda G P, Wilde G. Non-equilibrium intermixing and phase transformation in severely deformed Al/Ni multilayers [J]. Scr. Mater., 2007, 56: 181 | [27] | Chung C Y, Zhu M, Man C H. Effect of mechanical alloying on the solid state reaction processing of Ni-36.5 at.% Al alloy [J]. Intermetallics, 2002, 10: 865 | [28] | Valiev R Z, Islamgaliev R K, Alexandrov I V. Bulk nanostructured materials from severe plastic deformation [J]. Prog. Mater. Sci., 2000, 45: 103 | [29] | Sauvage X, Wetscher F, Pareige P. Mechanical alloying of Cu and Fe induced by severe plastic deformation of a Cu-Fe composite [J]. Acta Mater., 2005, 53: 2127 | [30] | Sato K, Yoshiie T, Satoh Y, et al. Simulation of vacancy migration energy in Cu under high strain [J]. Mater. Sci. Eng., 2003, A350: 220 |
|
|