| 纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究 |
李海勇1, 李赛毅1,2( ) |
1.中南大学 材料科学与工程学院 长沙 410083 2.中南大学 有色金属材料科学与工程教育部重点实验室 长沙 410012 |
|
| Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations |
LI Haiyong1, LI Saiyi1,2( ) |
1.School of Materials Science and Engineering, Central South University, Changsha 410083, China 2.Key Laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University, Changsha 410012, China |
引用本文:
李海勇, 李赛毅. 纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究[J]. 金属学报, 2022, 58(2): 250-256.
Haiyong LI,
Saiyi LI.
Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations[J]. Acta Metall Sin, 2022, 58(2): 250-256.
| 1 |
Gottstein G , Shvindlerman L S . Grain Boundary Migration in Metals: Thermodynamics, Kinetics, Applications [M]. 2nd Ed., Boca Raton: Taylor & Francis, 2010: 145
|
| 2 |
Winning M , Gottstein G , Shvindlerman L S . Stress induced grain boundary motion [J]. Acta Mater., 2001, 49: 211
|
| 3 |
Winning M , Rollett A D , Gottstein G , et al . Mobility of low-angle grain boundaries in pure metals [J]. Philos. Mag., 2010, 90: 3107
|
| 4 |
Shivindlerman L S , Gottstein G , Molodov D A . Grain boundary motion in pure metals: Effect of interaction between adsorbed atoms at moving boundaries [J]. Phys. Status Solidi, 1997, 160a: 419
|
| 5 |
Molodov D A , Czubayko U , Gottstein G , et al . Mobility of <111> tilt grain boundaries in the vicinity of the special misorientation ∑ = 7 in bicrystals of pure aluminium [J]. Scr. Metall. Mater., 1995, 32: 529
|
| 6 |
Upmanyu M , Srolovitz D J , Shvindlerman L S , et al . Misorientation dependence of intrinsic grain boundary mobility: Simulation and experiment [J]. Acta Mater., 1999, 47: 3901
|
| 7 |
Kopetsky C V , Shvindlerman L S , Sursaeva V G . Effect of athermal motion of grain boundaries [J]. Scr. Metall., 1978, 12: 953
|
| 8 |
Rheinheimer W , Hoffmann M J . Non-Arrhenius behavior of grain growth in strontium titanate: New evidence for a structural transition of grain boundaries [J]. Scr. Mater., 2015, 101: 68
|
| 9 |
Homer E R , Holm E A , Foiles S M , et al . Trends in grain boundary mobility: Survey of motion mechanisms [J]. JOM, 2014, 66: 114
|
| 10 |
Priedeman J L , Olmsted D L , Homer E R . The role of crystallography and the mechanisms associated with migration of incoherent twin grain boundaries [J]. Acta Mater., 2017, 131: 553
|
| 11 |
Humberson J , Holm E A . Anti-thermal mobility in the Σ3 [111] 60° {11 8 5} grain boundary in nickel: Mechanism and computational considerations [J]. Scr. Mater., 2017, 130: 1
|
| 12 |
Bair J L , Homer E R . Antithermal mobility in ∑7 and ∑9 grain boundaries caused by stick-slip stagnation of ordered atomic motions about coincidence site lattice atoms [J]. Acta Mater., 2019, 162: 10
|
| 13 |
Yu T T , Yang S , Deng C . Survey of grain boundary migration and thermal behavior in Ni at low homologous temperatures [J]. Acta Mater., 2019, 177: 151
|
| 14 |
Han J , Thomas S L , Srolovitz D J . Grain-boundary kinetics: A unified approach [J]. Prog. Mater. Sci., 2018, 98: 386
|
| 15 |
Homer E R , Patala S , Priedeman J L . Grain boundary plane orientation fundamental zones and structure-property relationships [J]. Sci. Rep., 2015, 5: 15476.
|
| 16 |
Olmsted D L , Holm E A , Foiles S M . Survey of computed grain boundary properties in face-centered cubic metals—II: Grain boundary mobility [J]. Acta Mater., 2009, 57: 3704
|
| 17 |
Yang L , Lai C M , Li S Y . A survey of the crystallography-dependency of twist grain boundary mobility in Al based on atomistic simulations [J]. Mater. Lett., 2020, 263: 127293.
|
| 18 |
Yang L , Lai C M , Li S Y . Statistical analysis of grain boundary mobility in Al simulated using a modified synthetic driving force molecular dynamics method [J]. Mater. Lett., 2018, 227: 90
|
| 19 |
Beck P A , Sperry P R , Hu H . The orientation dependence of the rate of grain boundary migration [J]. J. Appl. Phys., 1950, 21: 420
|
| 20 |
Lücke K , Rixen R , Senna M . Formation of recrystallization textures in rolled aluminum single crystals [J]. Acta Metall., 1976, 24: 103
|
| 21 |
Plimpton S . Fast parallel algorithms for short-range molecular dynamics [J]. J. Comput. Phys., 1995, 117: 1
|
| 22 |
Liu X Y , Ercolessi F , Adams J B . Aluminium interatomic potential from density functional theory calculations with improved stacking fault energy [J]. Modell. Simul. Mater. Sci. Eng., 2004, 12: 665
|
| 23 |
Adlakha I , Solanki K N . Structural stability and energetics of grain boundary triple junctions in face centered cubic materials [J]. Sci. Rep., 2015, 5: 8692
|
| 24 |
Men H , Fan Z . Molecular dynamic simulation of the atomic structure of aluminum solid-liquid interfaces [J]. Mater. Res. Express, 2014, 1: 025705
|
| 25 |
Tschopp M A , McDowell D L . Structures and energies of Σ3 asymmetric tilt grain boundaries in copper and aluminium [J]. Philos. Mag., 2007, 87: 3147
|
| 26 |
Janssens K G F , Olmsted D , Holm E A , et al . Computing the mobility of grain boundaries [J]. Nat. Mater., 2006, 5: 124
|
| 27 |
Yang L , Li S Y . A modified synthetic driving force method for molecular dynamics simulation of grain boundary migration [J]. Acta Mater., 2015, 100: 107
|
| 28 |
Stukowski A . Visualization and analysis of atomistic simulation data with OVITO—The Open Visualization Tool [J]. Modell. Simul. Mater. Sci. Eng., 2009, 18: 015012
|
| 29 |
Sutton A P , Vitek V . On the structure of tilt grain boundaries in cubic metals I. Symmetrical tilt boundaries [J]. Philos. Trans. R. Soc. London, 1983, 309A: 1
|
| 30 |
Zhou J , Mohles V . Towards realistic molecular dynamics simulations of grain boundary mobility [J]. Acta Mater., 2011, 59: 5997
|
| 31 |
Holm E A , Foiles S M , Homer E R , et al . Comment on “Toward realistic molecular dynamics simulations of grain boundary mobility” by Zhou and Mohles [J]. Scr. Mater., 2012, 66: 714
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|