| Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究 |
李亚敏( ), 张瑶瑶, 赵旺, 周生睿, 刘洪军 |
| 兰州理工大学 省部共建有色金属先进加工与再利用国家重点实验室 兰州 730050 |
|
| First-Principles Study on the Effect of Cu on Nb Segregation in Inconel 718 Alloy |
LI Yamin( ), ZHANG Yaoyao, ZHAO Wang, ZHOU Shengrui, LIU Hongjun |
| State Key Laboratory of Advanced Processing and Reuse of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China |
引用本文:
李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究[J]. 金属学报, 2022, 58(2): 241-249.
Yamin LI,
Yaoyao ZHANG,
Wang ZHAO,
Shengrui ZHOU,
Hongjun LIU.
First-Principles Study on the Effect of Cu on Nb Segregation in Inconel 718 Alloy[J]. Acta Metall Sin, 2022, 58(2): 241-249.
| 1 |
Pereira J M , Lerch B A . Effects of heat treatment on the ballistic impact properties of Inconel 718 for jet engine fan containment applications [J]. Int. J. Impact Eng., 2001, 25: 715
|
| 2 |
Qi H . Review of INCONEL 718 alloy: Its history, properties, processing and developing substitutes [J]. J. Mater. Eng., 2012, (8): 92
|
| 2 |
齐 欢 . INCONEL 718(GH4169)高温合金的发展与工艺 [J]. 材料工程, 2012, (8): 92
|
| 3 |
Tian Y , Zhao M C . Segregation of Nb and its formation mechanism of high strength casing steel [J]. J. Iron Steel Res., 2020, 32: 344
|
| 3 |
田 研, 赵明纯 . 高强度油井管钢中的Nb偏析及形成机制分析 [J]. 钢铁研究学报, 2020, 32: 344
|
| 4 |
Sun K , Lin H B , He Y B , et al . Microscopic inspection and improvement of GH4169G alloy forging banded structure defects [J]. Spec. Cast. Nonferrous Alloys, 2020, 40: 694
|
| 4 |
孙 凯, 蔺虹宾, 何跃斌 等 . GH4169G合金锻件条带缺陷微观检测及改进 [J]. 特种铸造及有色合金, 2020, 40: 694
|
| 5 |
Chen Y , Guo Y B , Xu M J , et al . Study on the element segregation and Laves phase formation in the laser metal deposited IN718 superalloy by flat top laser and gaussian distribution laser [J]. Mater. Sci. Eng., 2019, A754: 339
|
| 6 |
Zhang Y , Li X X , Wei K , et al . Element segregation in GH4169 Superalloy large-scale ingot and billet manufactured by triple-melting [J]. Acta Metall. Sin., 2020, 56: 1123
|
| 6 |
张 勇, 李鑫旭, 韦 康 等 . 三联熔炼GH4169合金大规格铸锭与棒材元素偏析行为 [J]. 金属学报, 2020, 56: 1123
|
| 7 |
DuPont J N , Rohino C V . The influence of Nb and C on the solidification microstructures of Fe-Ni-Cr alloys [J]. Scr. Mater., 1999, 41: 449
|
| 8 |
Li A L , Tang X , Gai Q D , et al . Effect of heat treatment on microstructure of K4169 superalloy [J]. J. Aeronaut. Mater., 2006, 26: 311
|
| 8 |
李爱兰, 汤 鑫, 盖其东 等 . 热处理工艺对K4169合金微观组织的影响 [J]. 航空材料学报, 2006, 26: 311
|
| 9 |
Long Y T , Nie P L , Li Z G , et al . Segregation of niobium in laser cladding Inconel 718 superalloy [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 431
|
| 10 |
Zhang M C , Zheng L , Yao Z H , et al . Effect of Nb content on micro-segregation evolution of GH4169 ingots [J]. Hot Work. Technol., 2013, 42(10): 45
|
| 10 |
张麦仓, 郑 磊, 姚志浩 等 . Nb含量对GH4169合金钢锭偏析规律的影响 [J]. 热加工工艺, 2013, 42(10): 45
|
| 11 |
Mo Y , Wang D Z , Jiang B , et al . Effect of micro alloying vanadium on micro-segregation behavior of niobium in 718 alloy [J]. Heat Treat. Met., 2017, 42(4): 37
|
| 11 |
莫 燕, 王东哲, 蒋 斌 等 . 钒微合金化对718合金中铌元素偏析行为的影响 [J]. 金属热处理, 2017, 42(4): 37
|
| 12 |
Sun W R , Guo S R , Lu D Z , et al . Effect of Si on solidification and segregation in Inconel 718 alloy [J]. J. Aeronaut. Mater., 1996, 16(2): 7
|
| 12 |
孙文儒, 郭守仁, 卢德忠 等 . Si对In718合金凝固过程及元素偏析的影响 [J]. 航空材料学报, 1996, 16(2): 7
|
| 13 |
Meng F X , Li J H , Zhao X . First-principles study on the effects of Zn-segregation in CuΣ5 grain boundary [J]. Acta Phys. Sin., 2014, 63: 237102
|
| 13 |
孟凡顺, 李久会, 赵 星 . 第一性原理研究Zn偏析对CuΣ5晶界的影响 [J]. 物理学报, 2014, 63: 237102
|
| 14 |
Wang J L , Enomoto M , Shang C J . First-principles study on the interfacial segregation at coherent Cu precipitate/Fe matrix interface [J]. Scr. Mater., 2020, 185: 42
|
| 15 |
Peng L J . Study on microstructure evolution of Cu-Cr-Zr system alloys and interaction mechanism between alloying elements [D]. Beijing: General Research Institute for Nonferrous Metals, 2014
|
| 15 |
彭丽军 . Cu-Cr-Zr系合金微观组织演变规律及合金元素交互作用机理的研究 [D]. 北京: 北京有色金属研究总院, 2014
|
| 16 |
Huang Z W , Zhao Y H , Hou H , et al . Point defects structure and alloying effects of V atoms into Ni3Al alloy: A first-principles study [J]. Rare Met. Mater. Eng., 2011, 40: 2136
|
| 16 |
黄志伟, 赵宇宏, 侯 华 等 . V掺杂Ni3Al点缺陷结构及合金化效应的第一性原理研究 [J]. 稀有金属材料与工程, 2011, 40: 2136
|
| 17 |
Perdew J P , Wang Y . Accurate and simple analytic representation of the electron-gas correlation energy [J]. Phys. Rev., 1992, 45B: 13244
|
| 18 |
Li Y M , Jiang L , Zhao W , et al . First-principle study of the effects of Cu doped on γ' phase [J]. Mater. Rev., 2019, 33: 3085
|
| 18 |
李亚敏, 江 璐, 赵 旺 等 . 铜掺杂对γ′相影响的第一性原理研究 [J]. 材料导报, 2019, 33: 3085
|
| 19 |
Zhao Y H , Huang Z W , Li A H , et al . First principles study on substitution behavior and alloying effects of Nb in Ni3Al [J]. Acta Phys. Sin., 2011, 60: 047103
|
| 19 |
赵宇宏, 黄志伟, 李爱红 等 . Nb在Ni3Al中取代行为及合金化效应的第一性原理研究 [J]. 物理学报, 2011, 60: 047103
|
| 20 |
Zhang X Y , Zheng B J , Guo B , et al . Theoretical study on bonding characteristics of Cr, Mn, Mo and N in high nitrogen austenitic stainless steel [J]. Mater. Rev., 2017, 31(18): 146
|
| 20 |
张旭昀, 郑冰洁, 郭 斌 等 . 高氮奥氏体不锈钢中N与Cr、Mn、Mo键合性质研究 [J]. 材料导报, 2017, 31(18): 146
|
| 21 |
Chen Z M , Yu W Q . Principle of Solidification of Casting Metal [M]. Beijing: Peking University Press, 2014: 116
|
| 21 |
陈宗民, 于文强 . 铸造金属凝固原理 [M]. 北京: 北京大学出版社, 2014: 116
|
| 22 |
Hu Z Q , Sun W R , Guo S R , et al . Effect of trace P on Fe-Ni based wrought superalloy [J]. Chin. J. Nonferrous Met., 2001, 11: 947
|
| 22 |
胡壮麒, 孙文儒, 郭守仁 等 . 微量元素磷在铁镍基变形高温合金中的作用 [J]. 中国有色金属学报, 2001, 11: 947
|
| 23 |
Xu Z L . Performance, Strength Design and Engineering Application of High Temperature Metal Materials [M]. Beijing: Chemical Industry Press, 2006: 77
|
| 23 |
徐自立 . 高温金属材料的性能、强度设计及工程应用 [M]. 北京: 化学工业出版社, 2006: 77
|
| 24 |
Zhang Q C . A new type of turbine disc and blade material—low segregation superalloy [J]. Aeroengine, 1995, (2): 14
|
| 24 |
张庆春 . 新型涡轮盘及叶片材料——低偏析高温合金 [J]. 航空发动机, 1995, (2): 14
|
| 25 |
Zhu Y X . Low segregation superalloys [J]. Trans. Mater. Heat Treat., 1997, 18(3): 16
|
| 25 |
朱耀霄 . 低偏析高温合金 [J]. 金属热处理学报, 1997, 18(3): 16
|
| 26 |
Wang A C , Li Y Y , Li D F , et al . Effect of Nb and Ti contents on micro-segregation of J-90 alloy [J]. Acta Metall. Sin., 1995, 31: 216
|
| 26 |
王安川, 李依依, 李冬法 等 . Nb, Ti含量对J-90合金凝固偏析的影响 [J]. 金属学报, 1995, 31: 216
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|