脉冲电流作用下TiAl合金凝固组织演变及形成机理 |
陈占兴,丁宏升(),陈瑞润,郭景杰,傅恒志 |
1. 哈尔滨工业大学材料科学与工程学院金属精密热加工国家级重点实验室 哈尔滨 150001 |
|
Microstructural Evolution and Mechanism of Solidified TiAl Alloy Applied Electric Current Pulse |
Zhanxing CHEN,Hongsheng DING(),Ruirun CHEN,Jingjie GUO,Hengzhi FU |
1. National Key Laboratory for Precision Hot Processing of Metals, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China |
引用本文:
陈占兴,丁宏升,陈瑞润,郭景杰,傅恒志. 脉冲电流作用下TiAl合金凝固组织演变及形成机理[J]. 金属学报, 2019, 55(5): 611-618.
Zhanxing CHEN,
Hongsheng DING,
Ruirun CHEN,
Jingjie GUO,
Hengzhi FU.
Microstructural Evolution and Mechanism of Solidified TiAl Alloy Applied Electric Current Pulse[J]. Acta Metall Sin, 2019, 55(5): 611-618.
[1] | AsaiS. Recent development and prospect of electromagnetic processing of materials[J]. Sci. Technol. Adv. Mater., 2000, 1: 191 | [2] | AsaiS. Electromagnetic Processing of Materials[M]. Dordrecht: Springer, 2012: 87 | [3] | WangR Z, QiJ G, WangB, et al. Solidification behavior and crystal growth mechanism of aluminum under electric pulse[J]. J. Mater. Process. Technol., 2016, 237: 235 | [4] | TangY F, QiuS, MiaoQ, et al. Fabrication of lamellar porous alumina with axisymmetric structure by directional solidification with applied electric and magnetic fields[J]. J. Eur. Ceram. Soc., 2016, 36: 1233 | [5] | LiC S, HuS D, RenZ M, et al. Effect of the simultaneous application of a high static magnetic field and a low alternating current on grain structure and grain boundary of pure aluminum[J]. J. Mater. Sci. Technol., 2018, 34: 2431 | [6] | LiY Z, Mangelinck-No?lN, ZimmermannG, et al. Effect of solidification conditions and surface pores on the microstructure and columnar-to-equiaxed transition in solidification under microgravity[J]. J. Alloys Compd., 2018, 749: 344 | [7] | RuanY, WangQ Q, ChangS Y, et al. Structural evolution and micromechanical properties of ternary Al-Ag-Ge alloy solidified under microgravity condition[J]. Acta Mater., 2017, 141: 456 | [8] | XuanY, NastacL. The role of ultrasonic cavitation in refining the microstructure of aluminum based nanocomposites during the solidification process[J]. Ultrasonics, 2018, 83: 94 | [9] | ChenZ X, DingH S, ChenR R, et al. An innovative method for the microstructural modification of TiAl alloy solidified via direct electric current application[J]. J. Mater. Sci. Technol., 2019, 35: 23 | [10] | LiJ, MaJ H, SongC J, et al. Columnar to equiaxed transition during solidification of small ingot by using electric current pulse[J]. J. Iron Steel Res., Int., 2009, 16: 7 | [11] | LiJ Y, NiP, WangL, et al. Influence of direct electric current on solidification process of Al-Si alloy[J]. Mater. Sci. Semicond. Process., 2017, 61: 79 | [12] | YangJ R, ChenR R, GuoJ J, et al. Temperature distribution in bottomless electromagnetic cold crucible applied to directional solidification[J]. Int. J. Heat Mass Transfer, 2016, 100: 131 | [13] | YangJ R, ChenR R, SuY Q, et al. Optimization of electromagnetic energy in cold crucible used for directional solidification of TiAl alloy[J]. Energy, 2018, 161: 143 | [14] | ErdelyP, StaronP, MaawadE, et al. Design and control of microstructure and texture by thermomechanical processing of a multi-phase TiAl alloy[J]. Mater. Des., 2017, 131: 286 | [15] | WangX D, LuoR C, LiuF, et al. Characterization of Gd-rich precipitates in a fully lamellar TiAl alloy[J]. Scr. Mater., 2017, 137: 50 | [16] | ZhangT B, WuZ E, HuR, et al. Influence of nitrogen on the microstructure and solidification behavior of high Nb containing TiAl alloys[J]. Mater. Des., 2016, 103: 100 | [17] | ZollingerJ, LapinJ, DalozD, et al. Influence of oxygen on solidification behaviour of cast TiAl-based alloys[J]. Intermetallics, 2007, 15: 1343 | [18] | JungI S, JangH S, OhM H, et al. Microstructure control of TiAl alloys containing β stabilizers by directional solidification[J]. Mater. Sci. Eng., 2002, A329-331: 13 | [19] | ChenZ X, DingH S, LiuS Q, et al. Effects of direct current on microstructure and properties of Ti-48Al-2Cr-2Nb alloy[J].Acta Metall. Sin., 2017, 53: 583 | [19] | (陈占兴, 丁宏升, 刘石球等. 直流电流对Ti-48Al-2Cr-2Nb合金组织和性能的影响 [J]. 金属学报, 2017, 53: 583) | [20] | LiX Z, FanJ L, SuY Q, et al. Lamellar orientation and growth direction of α phase in directionally solidified Ti-46Al-0.5W-0.5Si alloy[J]. Intermetallics, 2012, 27: 38 | [21] | BarnakJ P, SprecherA F, ConradH. Colony (grain) size reduction in eutectic Pb-Sn castings by electroplusing[J]. Scr. Metall. Mater., 1995, 32: 879 | [22] | ZhaiQ J. Foundamentals of Structure Refinement Technology for Metal Solidification[M]. Beijing: Science Press, 2018: 145 | [22] | (翟启杰. 金属凝固组织细化技术基础 [M]. 北京: 科学出版社, 2018: 145) | [23] | GaoM, HeG H, YangF, et al. Effect of electric current pulse on tensile strength and elongation of casting ZA27 alloy[J]. Mater. Sci. Eng., 2002, A337: 110 | [24] | NakadaM, ShioharaY, FlemingsM C. Modification of solidification structures by pulse electric discharging[J]. ISIJ Int., 1990, 30: 27 | [25] | ZhangW, SuiM L, ZhouY Z, et al. Electropulsing-induced evolution of microstructures in materials[J].Acta Metall. Sin., 2003, 39: 1009 | [25] | (张 伟, 隋曼龄, 周亦胄等. 高密度电脉冲下材料微观结构的演变 [J]. 金属学报, 2003, 39: 1009) | [26] | TangJ C, HuangB Y, ZhouK C, et al. Factors affecting the lamellar spacing in two-phase TiAl alloys with fully lamellar microstructures[J]. Mater. Res. Bull., 2001, 36: 1737 | [27] | LapinJ, Ondrú?L', NazmyM. Directional solidification of intermetallic Ti-46Al-2W-0.5Si alloy in alumina moulds[J]. Intermetallics, 2002, 10: 1019 | [28] | ClemensH, BartelsA, BystrzanowskiS, et al. Grain refinement in γ-TiAl-based alloys by solid state phase transformations[J]. Intermetallics, 2006, 14: 1380 | [29] | InuiH, OhM H, NakamuraA, et al. Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl[J]. Acta Metall. Mater., 1992, 40: 3095 | [30] | JungI S, OhM H, ParkN J, et al. Lamellar boundary alignment of DS-processed TiAl-W alloys by a solidification procedure[J]. Met. Mater. Int., 2007, 13: 455 |
|
|
Viewed |
|
|
|