| 多维度碳纳米相增强铝基复合材料研究进展 |
赵乃勤( ), 刘兴海, 蒲博闻 |
| 天津大学材料科学与工程学院 天津 300350 |
|
| Progress on Multi-Dimensional Carbon Nanomaterials Reinforced Aluminum Matrix Composites: A Review |
Naiqin ZHAO( ), Xinghai LIU, Bowen PU |
| School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China |
引用本文:
赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展[J]. 金属学报, 2019, 55(1): 1-15.
Naiqin ZHAO,
Xinghai LIU,
Bowen PU.
Progress on Multi-Dimensional Carbon Nanomaterials Reinforced Aluminum Matrix Composites: A Review[J]. Acta Metall Sin, 2019, 55(1): 1-15.
| [1] | Guo W H, Liu C, Sun X M, et al.Aligned carbon nanotube/polymer composite fibers with improved mechanical strength and electrical conductivity[J]. J. Mater. Chem., 2012, 22: 903 | | [2] | Murakami K, Nishida N, Osamura K, et al.Aluminization of high purity iron and stainless steel by powder liquid coating[J]. Acta Mater., 2004, 52: 2173 | | [3] | Tian F, He C N.Fabrication and growth mechanism of carbon nanospheres by chemical vapor deposition[J]. Mater. Chem. Phys., 2010, 123: 351 | | [4] | Miki-Yoshid M, Castillo R, Ramos S, et al.High resolution electron microscopy studies in carbon soots[J]. Carbon, 1994, 32: 231 | | [5] | Wang Z X, Yu L P, Zhang W, et al.Carbon spheres synthesized by ultrasonic treatment[J]. Phys. Lett., 2003, 307A: 249 | | [6] | Ugarte D.Curling and closure of graphitic networks under electron-beam irradiation[J]. Nature, 1992, 359: 707 | | [7] | Sun X M, Li Y D.Colloidal carbon spheres and their core/shell structures with noble-metal nanoparticles[J]. Angew. Chem., Int. Ed., 2004, 43: 597 | | [8] | Miao J Y, Hwang D W, Chang C C, et al.Uniform carbon spheres of high purity prepared on kaolin by CCVD[J]. Diam. Relat. Mater., 2003, 12: 1368 | | [9] | Robles Hernández F C, Calderon H A. Nanostructured Al/Al4C3 composites reinforced with graphite or fullerene and manufactured by mechanical milling and spark plasma sintering[J]. Mater. Chem. Phys., 2012, 132: 815 | | [10] | Umemoto M, Masuyama K, Raviprasad K. Mechanical alloying of fullerene with metals [J]. Mater. Sci. Forum, 1997, 235-238: 47 | | [11] | Harris P J F. Carbon Nanotubes and Related Structures [M]. Cambridge: Cambridge University Press, 1999: 1 | | [12] | de Heer W A, Ugarte D. Carbon onions produced by heat treatment of carbon soot and their relation to the 217.5 nm interstellar absorption feature[J]. Chem. Phys. Lett., 1993, 207: 480 | | [13] | Hou J G, Li X, Wang H Q, et al.Cu-C60 interaction and nano-composite structures[J]. J. Phys. Chem. Solids, 2000, 61: 995 | | [14] | Khalid F A, Beffort O, Klotz U E, et al.Study of microstructure and interfaces in an aluminium-C60 composite material[J]. Acta Mater., 2003, 51: 4575 | | [15] | Watanabe H, Sugioka M, Fukusumi M, et al.Mechanical and damping properties of fullerene-dispersed AZ91 magnesium alloy composites processed by a powder metallurgy route[J]. Mater. Trans., 2006, 47: 999 | | [16] | He C N, Zhao N Q, Du X W, et al.Low-temperature synthesis of carbon onions by chemical vapor deposition using a nickel catalyst supported on aluminum[J]. Scr. Mater., 2006, 54: 689 | | [17] | Zhao R Y, Xu R, Fan G L, et al.Reinforcement with in-situ synthesized carbon nano-onions in aluminum composites fabricated by flake powder metallurgy[J]. J. Alloys Compd., 2015, 650: 217 | | [18] | He C N, Zhao N Q, Shi C S, et al.Fabrication of nanocarbon composites using in situ chemical vapor deposition and their applications[J]. Adv. Mater., 2015, 27: 5422 | | [19] | Oh S I, Lim J Y, Kim Y C, et al.Fabrication of carbon nanofiber reinforced aluminum alloy nanocomposites by a liquid process[J]. J. Alloys Compd., 2012, 542: 111 | | [20] | Iijima S.Helical microtubules of graphitic carbon[J]. Nature, 1991, 354: 56 | | [21] | Golberg D, Bai X D, Mitome M, et al.Structural peculiarities of in situ deformation of a multi-walled BN nanotube inside a high-resolution analytical transmission electron microscope[J]. Acta Mater., 2007, 55: 1293 | | [22] | Bakshi S R, Lahiri D, Agarwal A.Carbon nanotube reinforced metal matrix composites—A review[J]. Int. Mater. Rev., 2010, 55: 41 | | [23] | So K P, Lee I H, Duong D L, et al.Improving the wettability of aluminum on carbon nanotubes[J]. Acta Mater., 2011, 59: 3313 | | [24] | Liu Z Y, Xiao B L, Wang W G, et al.Modelling of carbon nanotube dispersion and strengthening mechanisms in Al matrix composites prepared by high energy ball milling-powder metallurgy method[J]. Composites, 2017, 94A: 189 | | [25] | Lahiri D, Bakshi S R, Keshri A K, et al.Dual strengthening mechanisms induced by carbon nanotubes in roll bonded aluminum composites[J]. Mater. Sci. Eng., 2009, A523: 263 | | [26] | Bakshi S R, Agarwal A.An analysis of the factors affecting strengthening in carbon nanotube reinforced aluminum composites[J]. Carbon, 2011, 49: 533 | | [27] | Park J G, Keum D H, Lee Y H.Strengthening mechanisms in carbon nanotube-reinforced aluminum composites[J]. Carbon, 2015, 95: 690 | | [28] | Zhou W W, Yamaguchi T, Kikuchi K, et al.Effectively enhanced load transfer by interfacial reactions in multi-walled carbon nanotube reinforced Al matrix composites[J]. Acta Mater., 2017, 125: 369 | | [29] | Park J G, Keum D H, Lee Y H.Strengthening mechanisms in carbon nanotube-reinforced aluminum composites[J]. Carbon, 2015, 95: 690 | | [30] | Kwon H, Estili M, Takagi K, et al.Combination of hot extrusion and spark plasma sintering for producing carbon nanotube reinforced aluminum matrix composites[J]. Carbon, 2009, 47: 570 | | [31] | Zare H, Jahedi M, Toroghinejad M R, et al.Microstructure and mechanical properties of carbon nanotubes reinforced aluminum matrix composites synthesized via equal-channel angular pressing[J]. Mater. Sci. Eng., 2016, A670: 205 | | [32] | Liu Z Y, Xiao B L, Wang W G, et al.Singly dispersed carbon nanotube/aluminum composites fabricated by powder metallurgy combined with friction stir processing[J]. Carbon, 2012, 50: 1843 | | [33] | Choi H J, Shin J H, Bae D H.The effect of milling conditions on microstructures and mechanical properties of Al/MWCNT composites[J]. Composites, 2012, 43A: 1061 | | [34] | Jiang L, Fan G L, Li Z Q, et al.An approach to the uniform dispersion of a high volume fraction of carbon nanotubes in aluminum powder[J]. Carbon, 2011, 49: 1965 | | [35] | Liu Z Y, Zhao K, Xiao B L, et al.Fabrication of CNT/Al composites with low damage to CNTs by a novel solution-assisted wet mixing combined with powder metallurgy processing[J]. Mater. Des., 2016, 97: 424 | | [36] | Chen B, Li S F, Imai H, et al.An approach for homogeneous carbon nanotube dispersion in Al matrix composites[J]. Mater. Des., 2015, 72: 1 | | [37] | Guo B S, Zhang X M, Cen X, et al.Enhanced mechanical properties of aluminum based composites reinforced by chemically oxidized carbon nanotubes[J]. Carbon, 2018, 139: 459 | | [38] | Subrahmanyam J, Vijayakumar M.Self-propagating high-temperature synthesis[J]. J. Mater. Sci., 1992, 27: 6249 | | [39] | He C N, Zhao N Q, Shi C S, et al.An Approach to obtaining homogeneously dispersed carbon nanotubes in Al powders for preparing reinforced Al-matrix composites[J]. Adv. Mater., 2007, 19: 1128 | | [40] | Yang X D, Liu E Z, Shi C S, et al.Fabrication of carbon nanotube reinforced Al composites with well-balanced strength and ductility[J]. J. Alloys Compd., 2013, 563: 216 | | [41] | Palermo V, Kinloch I A, Ligi S, et al.Nanoscale mechanics of graphene and graphene oxide in composites: A scientific and technological perspective[J]. Adv. Mater., 2016, 28: 6232 | | [42] | Xue C, Bai H, Tao P F, et al.Analysis on thermal conductivity of graphite/Al composite by experimental and modeling study[J]. J. Mater. Eng. Perform., 2017, 26: 327 | | [43] | Wang J W, Zhang X Z, Xue C, et al.Effects of Si coated on graphite surface on the thermal and mechanical properties of graphite/Al composites[J]. Acta Mater. Compos. Sin., 2017, 34: 836(王俊伟, 张现周, 薛晨 等. 石墨表面镀Si对石墨/Al复合材料热物理性能的影响 [J]. 复合材料学报, 2017, 34: 836) | | [44] | Wang C, Bai H, Xue C, et al.On the influence of carbide coating on the thermal conductivity and flexural strength of X (X=SiC, TiC) coated graphite/Al composites[J]. RSC Adv., 2016, 6: 107483 | | [45] | Akhlaghi F, Pelaseyyed S A.Characterization of aluminum/graphite particulate composites synthesized using a novel method termed "in-situ powder metallurgy"[J]. Mater. Sci. Eng., 2004, A385: 258 | | [46] | Novoselov K S, Geim A K, Morozov S V, et al.Electric field effect in atomically thin carbon films[J]. Science, 2004, 306: 666 | | [47] | Cao Y C, Guo M M.Graphene materials and its applications[J]. Petrochem. Technol., 2016, 45: 1149(曹宇臣, 郭鸣明. 石墨烯材料及其应用 [J]. 石油化工, 2016, 45: 1149) | | [48] | Stankovich S, Dikin D A, Dommett G H B, et al. Graphene-based composite materials[J]. Nature, 2006, 442: 282 | | [49] | Ramanathan T, Abdala A A, Stankovich S, et al.Functionalized graphene sheets for polymer nanocomposites[J]. Nat. Nanotechnol., 2008, 3: 327 | | [50] | Liang J J, Xu Y F, Huang Y, et al.Infrared-triggered actuators from graphene-based nanocomposites[J]. J. Phys. Chem., 2009, 113C: 9921 | | [51] | Ji F, Li Y L, Feng J M, et al.Electrochemical performance of graphene nanosheets and ceramic composites as anodes for lithium batteries[J]. J. Mater. Chem., 2009, 19: 9063 | | [52] | Walker L S, Marotto V R, Rafiee M A, et al.Toughening in graphene ceramic composites[J]. ACS Nano, 2011, 5: 3182 | | [53] | Fan Y C, Wang L J, Li J L, et al.Preparation and electrical properties of graphene nanosheet/Al2O3 composites[J]. Carbon, 2010, 48: 1743 | | [54] | Choi H, Kim H, Hwang S, et al.Electrochemical electrodes of graphene-based carbon nanotubes grown by chemical vapor deposition[J]. Scr. Mater., 2011, 64: 601 | | [55] | Chen C, Zhuo W T, Zheng W G, et al.Preparation and characterization of water-soluble graphene and highly conducting films[J]. J. Inorg. Mater., 2011, 26: 707 | | [56] | Yuan X Y.Progress in preparation of graphene[J]. J. Inorg. Mater., 2011, 26: 561 | | [57] | Wang L, Tian L H, Wei G D, et al.Epitaxial growth of graphene and their applications in devices[J]. J. Inorg. Mater., 2011, 26: 1009 | | [58] | Bartolucci S F, Paras J, Rafiee M A, et al.Graphene-aluminum nanocomposites[J]. Mater. Sci. Eng., 2011, A528: 7933 | | [59] | Li G, Xiong B W.Effects of graphene content on microstructures and tensile property of graphene-nanosheets/aluminum composites[J]. J. Alloys Compd., 2017, 697: 31 | | [60] | Shao P Z, Yang W S, Zhang Q, et al.Microstructure and tensile properties of 5083 Al matrix composites reinforced with graphene oxide and graphene nanoplates prepared by pressure infiltration method[J]. Composites, 2018, 109A: 151 | | [61] | Rashad M, Pan F S, Tang A T, et al.Effect of graphene nanoplatelets addition on mechanical properties of pure aluminum using a semi-powder method[J]. Prog. Nat. Sci.: Mater. Int., 2014, 24: 101 | | [62] | Yolshina L A, Muradymov R V, Korsun I V, et al.Novel aluminum-graphene and aluminum-graphite metallic composite materials: Synthesis and properties[J]. J. Alloys Compd., 2016, 663: 449 | | [63] | Gao X, Yue H Y, Guo E J, et al.Preparation and tensile properties of homogeneously dispersed graphene reinforced aluminum matrix composites[J]. Mater. Des., 2016, 94: 54 | | [64] | Zhang Z W, Liu Z Y, Xiao B L, et al.High efficiency dispersal and strengthening of graphene reinforced aluminum alloy composites fabricated by powder metallurgy combined with friction stir processing[J]. Carbon, 2018, 135: 215 | | [65] | Wang J Y, Li Z Q, Fan G L, et al.Reinforcement with graphene nanosheets in aluminum matrix composites[J]. Scr. Mater., 2012, 66: 594 | | [66] | Li Z, Guo Q, Li Z Q, et al.Enhanced mechanical properties of graphene (reduced graphene oxide)/aluminum composites with a bioinspired nanolaminated structure[J]. Nano Lett., 2015, 15: 8077 | | [67] | Liu X H, Li J J, Sha J W, et al.In-situ synthesis of graphene nanosheets coated copper for preparing reinforced aluminum matrix composites[J]. Mater. Sci. Eng., 2018, A709: 65 | | [68] | Liu G, Zhao N Q, Shi C S, et al.In-situ synthesis of graphene decorated with nickel nanoparticles for fabricating reinforced 6061Al matrix composites[J]. Mater. Sci. Eng., 2017, A699: 185 | | [69] | Zhao D M, Li Z W, Liu L D, et al.Progress of preparation and application of graphene/carbon nanotube composite materials[J]. Acta Chim. Sin., 2014, 72: 185(赵冬梅, 李振伟, 刘领弟等. 石墨烯/碳纳米管复合材料的制备及应用进展[J]. 化学学报, 2014, 72: 185) | | [70] | Wang M Z, Tang M, Chen S L, et al.Graphene-armored aluminum foil with enhanced anticorrosion performance as current collectors for lithium-ion battery[J]. Adv. Mater., 2017, 29: 1703882 | | [71] | Qi J L, Lin J H, Wang X, et al.Low resistance VFG-microporous hybrid Al-based electrodes for supercapacitors[J]. Nano Energy, 2016, 26: 657 | | [72] | Kwon H, Park D H, Silvain J F, et al.Investigation of carbon nanotube reinforced aluminum matrix composite materials[J]. Compos. Sci. Technol., 2010, 70: 546 | | [73] | Jiang L, Li Z Q, Fan G L, et al.Strong and ductile carbon nanotube/aluminum bulk nanolaminated composites with two-dimensional alignment of carbon nanotubes[J]. Scr. Mater., 2012, 66: 331 | | [74] | Yoo S J, Han S H, Kim W J.Strength and strain hardening of aluminum matrix composites with randomly dispersed nanometer-length fragmented carbon nanotubes[J]. Scr. Mater., 2013, 68: 711 | | [75] | Wei H, Li Z Q, Xiong D B, et al.Towards strong and stiff carbon nanotube-reinforced high-strength aluminum alloy composites through a microlaminated architecture design[J]. Scr. Mater., 2014, 75: 30 | | [76] | Mansoor M, Shahid M.Carbon nanotube-reinforced aluminum composite produced by induction melting[J]. J. Appl. Res. Technol., 2016, 14: 215 | | [77] | Meng X, Liu T, Shi C S, et al.Synergistic effect of CNTs reinforcement and precipitation hardening in in-situ CNTs/Al-Cu composites[J]. Mater. Sci. Eng., 2015, A633: 103 | | [78] | Yan H, Qiu H X.Fabrication of carbon nanotube reinforced A356 nanocomposites[J]. J. Mater. Res., 2016, 31: 2277 | | [79] | Chen B, Kondoh K, Imai H, et al.Simultaneously enhancing strength and ductility of carbon nanotube/aluminum composites by improving bonding conditions[J]. Scr. Mater., 2016, 113: 158 | | [80] | He T B, He X L, Tang P J, et al.The use of cryogenic milling to prepare high performance Al2009 matrix composites with dispersive carbon nanotubes[J]. Mater. Des., 2017, 114: 373 | | [81] | Xu R, Tan Z Q, Xiong D B, et al.Balanced strength and ductility in CNT/Al composites achieved by flake powder metallurgy via shift-speed ball milling[J]. Composites, 2017, 96A: 57 | | [82] | Zhao K, Liu Z Y, Xiao B L, et al.Origin of insignificant strengthening effect of CNTs in T6-treated CNT/6061Al composites[J]. Acta Metall. Sin.(Eng. Lett.), 2018, 31: 134 | | [83] | Fadavi Boostani A, Tahamtan S, Jiang Z Y, et al.Enhanced tensile properties of aluminium matrix composites reinforced with graphene encapsulated SiC nanoparticles[J]. Composites, 2015, 68A: 155 | | [84] | Shin S E, Bae D H.Deformation behavior of aluminum alloy matrix composites reinforced with few-layer graphene[J]. Composites, 2015, 78A: 42 | | [85] | Fadavi Boostani A, Yazdani S, Taherzadeh Mousavian R, et al.Strengthening mechanisms of graphene sheets in aluminium matrix nanocomposites[J]. Mater. Des., 2015, 88: 983 | | [86] | Shin S E, Choi H J, Shin J H, et al.Strengthening behavior of few-layered graphene/aluminum composites[J]. Carbon, 2015, 82: 143 | | [87] | Zhang H P, Xu C, Xiao W L, et al.Enhanced mechanical properties of Al5083 alloy with graphene nanoplates prepared by ball milling and hot extrusion[J]. Mater. Sci. Eng., 2016, A658: 8 | | [88] | Sun Y H, Zhang C, Liu B C, et al.Reduced graphene oxide reinforced 7075 Al matrix composites: Powder synthesis and mechanical properties[J]. Metals, 2017, 7: 499 | | [89] | Zhao M, Xiong D B, Tan Z Q, et al.Lateral size effect of graphene on mechanical properties of aluminum matrix nanolaminated composites[J]. Scr. Mater., 2017, 139: 44 | | [90] | Mukherjee B, Kumar R, Islam A, et al.Evaluation of strength-ductility combination by in-situ tensile testing of graphene nano platelets reinforced shroud plasma sprayed nickel-aluminium coating[J]. J. Alloys Compd., 2018, 765: 1082 | | [91] | Prashantha Kumar H G, Prabhakaran S, Anthony Xavior M, et al. Enhanced surface and mechanical properties of bioinspired nanolaminate graphene-aluminum alloy nanocomposites through laser shock processing for engineering applications[J]. Mater. Today, 2018, 16: 81 | | [92] | Jiang Y Y, Tan Z Q, Xu R, et al.Tailoring the structure and mechanical properties of graphene nanosheet/aluminum composites by flake powder metallurgy via shift-speed ball milling[J]. Composites, 2018, 111A: 73 | | [93] | Zhou W W, Fan Y C, Feng X P, et al.Creation of individual few-layer graphene incorporated in an aluminum matrix[J]. Composites, 2018, 112A: 168 | | [94] | Yang W S, Zhao Q Q, Xin L, et al.Microstructure and mechanical properties of graphene nanoplates reinforced pure Al matrix composites prepared by pressure infiltration method[J]. J. Alloys Compd., 2018, 732: 748 | | [95] | Dixit S, Mahata A, Mahapatra D R, et al.Multi-layer graphene reinforced aluminum—Manufacturing of high strength composite by friction stir alloying[J]. Composites, 2018, 136B: 63 | | [96] | Jo I, Cho S, Kim H, et al.Titanium dioxide coated carbon nanofibers as a promising reinforcement in aluminum matrix composites fabricated by liquid pressing process[J]. Scr. Mater., 2016, 112: 87 | | [97] | Romano M S, Li N, Antiohos D, et al.Carbon nanotube-reduced graphene oxide composites for thermal energy harvesting applications[J]. Adv. Mater., 2013, 25: 6602 | | [98] | Zhang C, Ren L L, Wang X Y, et al.Graphene oxide-assisted dispersion of pristine multiwalled carbon nanotubes in aqueous media[J]. J. Phys. Chem., 2010, 114C: 11435 | | [99] | Shin M K, Lee B, Kim S H, et al.Synergistic toughening of composite fibres by self-alignment of reduced graphene oxide and carbon nanotubes[J]. Nat. Commun., 2012, 3: 650 | | [100] | Li W K, Dichiara A, Bai J B.Carbon nanotube-graphene nanoplatelet hybrids as high-performance multifunctional reinforcements in epoxy composites[J]. Compos. Sci. Technol., 2013, 74: 221 | | [101] | Rashad M, Pan F S, Tang A T, et al.Synergetic effect of graphene nanoplatelets (GNPs) and multi-walled carbon nanotube (MW-CNTs) on mechanical properties of pure magnesium[J]. J. Alloys Compd., 2014, 603: 111 | | [102] | Li Z, Fan G L, Guo Q, et al.Synergistic strengthening effect of graphene-carbon nanotube hybrid structure in aluminum matrix composites[J]. Carbon, 2015, 95: 419 | | [103] | Nieto A, Dua R, Zhang C, et al.Three dimensional graphene foam/polymer hybrid as a high strength biocompatible scaffold[J]. Adv. Funct. Mater., 2015, 25: 3916 | | [104] | Lin Y, Liu S Q, Liu L.A new approach to construct three dimensional segregated graphene structures in rubber composites for enhanced conductive, mechanical and barrier properties[J]. J. Mater. Chem., 2016, 4C: 2353 | | [105] | Chen Z P, Ren W C, Gao L B, et al.Three-dimensional flexible and conductive interconnected graphene networks grown by chemical vapour deposition[J]. Nat. Mater., 2011, 10: 424 | | [106] | Jia J J, Sun X Y, Lin X Y, et al.Exceptional electrical conductivity and fracture resistance of 3D interconnected graphene foam/epoxy composites[J]. ACS Nano, 2014, 8: 5774 | | [107] | Chen Y K, Zhang X, Liu E Z, et al.Fabrication of in-situ grown graphene reinforced Cu matrix composites[J]. Sci. Rep., 2016, 6: 19363 | | [108] | Wang X F, Chen Y C, Li B Y.Aligning 3D nanofibrous networks from self-assembled phenylalanine nanofibers[J]. RSC Adv., 2015, 5: 8022 | | [109] | Zhang X, Shi C S, Liu E Z, et al.Achieving high strength and high ductility in metal matrix composites reinforced with a discontinuous three-dimensional graphene-like network[J]. Nanoscale, 2017, 9: 11929 | | [110] | Yang M, Weng L, Zhu H X, et al.Simultaneously enhancing the strength, ductility and conductivity of copper matrix composites with graphene nanoribbons[J]. Carbon, 2017, 118: 250 | | [111] | Kosynkin D V, Higginbotham A L, Sinitskii A, et al.Longitudinal unzipping of carbon nanotubes to form graphene nanoribbons[J]. Nature, 2009, 458: 872 | | [112] | Jiao L Y, Zhang L, Wang X R, et al.Narrow graphene nanoribbons from carbon nanotubes[J]. Nature, 2009, 458: 877 | | [113] | Zhang X, Shi C S, Liu E Z, et al.In-situ space-confined synthesis of well-dispersed three-dimensional graphene/carbon nanotube hybrid reinforced copper nanocomposites with balanced strength and ductility[J]. Composites, 2017, 103A: 178 | | [114] | Sha J W, Salvatierra R V, Dong P, et al.Three-dimensional rebar graphene[J]. ACS Appl. Mater. Interfaces, 2017, 9: 7376 | | [115] | Yan Z, Peng Z W, Casillas G, et al.Rebar graphene[J]. ACS Nano, 2014, 8: 5061 |
|
|