| 相场法模拟Fe-C合金中奥氏体-铁素体等温相变过程* |
张军1,2,郑成武2( ),李殿中2 |
1) 中国科学技术大学化学与材料科学学院, 合肥 230026 2) 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| MODELING OF ISOTHERMAL AUSTENITE TO FERRITE TRANSFORMATION IN A Fe-CALLOY BY PHASE-FIELD METHOD |
Jun ZHANG1,2,Chengwu ZHENG2( ),Dianzhong LI2 |
1 School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230026, China 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China; |
引用本文:
张军,郑成武,李殿中. 相场法模拟Fe-C合金中奥氏体-铁素体等温相变过程*[J]. 金属学报, 2016, 52(11): 1449-1458.
Jun ZHANG,
Chengwu ZHENG,
Dianzhong LI.
MODELING OF ISOTHERMAL AUSTENITE TO FERRITE TRANSFORMATION IN A Fe-CALLOY BY PHASE-FIELD METHOD[J]. Acta Metall Sin, 2016, 52(11): 1449-1458.
| [1] | Offerman S E, van Dijk N H, Sietsma J, Lauridsen E M, Margulies L, Grigull S, Poulsen H F, van der Zwaag S.Acta Mater, 2004; 52: 4757 | | [2] | Zener C. J Appl Phys, 1949; 20: 950 | | [3] | Christian J W.The Theory of Transformations in Metals and Alloys. 3rd Ed., Oxford: Elsevier Science, 2002: 1 | | [4] | Sietsma J, van der Zwaag S.Acta Mater, 2004; 52: 4143 | | [5] | Kumar M, Sasikumar R, Nair P K.Acta Mater, 1998; 46: 6291 | | [6] | Zhang L, Zhang C B, Wang Y M, Wang S Q, Ye H Q.Acta Mater, 2003; 51: 5519 | | [7] | Lan Y J, Li D Z, Li Y Y.Acta Mater, 2004; 52: 1721 | | [8] | Tong M M, Li D Z, Li Y Y.Acta Mater, 2005; 53: 1485 | | [9] | Steinbach I, Pezzolla F, Nestler B, See?elberg M, Prieler R, Schmitz G J, Rezende J L L.Physica, 1996; 94D: 135 | | [10] | Chen L Q.Annu Rev Mater Res, 2002; 32: 113 | | [11] | Warren J A, Kobayashi R, Lobovsky A E, Carter W C.Acta Mater, 2003; 51: 6035 | | [12] | Boettger B, Apel M, Eiken J, Schaffnit P, Steinbach I.Steel Res Int, 2008; 79: 608 | | [13] | Gao Y J, Luo Z R, Hu X Y, Huang C G.Acta Metall Sin, 2010; 46: 1161 | | [13] | (高英俊, 罗志荣, 胡项英, 黄创高. 金属学报, 2010; 46: 1161) | | [14] | Zhao Y, Zhang H Y, Wei H, Zheng Q, Jin T, Sun X F.Acta Metall Sin, 2013; 49: 981 | | [14] | (赵彦, 张宏宇, 韦华, 郑启, 金涛, 孙晓峰. 金属学报, 2013; 49: 981) | | [15] | Ke C B, Ma X, Zhang X P.Acta Metall Sin, 2010; 46: 84 | | [15] | (柯常波, 马骁, 张新平. 金属学报, 2010; 46: 84) | | [16] | Zhou G Z, Wang Y X, Chen Z.Acta Metall Sin, 2012; 48: 485 | | [16] | (周广钊, 王永欣, 陈铮. 金属学报, 2012; 48: 485) | | [17] | Loginova I, ?gren J, Amberg G.Acta Mater, 2004; 52: 4055 | | [18] | Mecozzi M G, Sietsma J, van der Zwaag S, Apel M, Schaffnit P, Steinbach I.Metall Mater Trans, 2005; 36A: 2327 | | [19] | Huang C J, Browne D J, McFadden S.Acta Mater, 2006; 54: 11 | | [20] | Moelans N.Acta Mater, 2011; 59: 1077 | | [21] | Moelans N, Blanpain B, Wollants P.Phys Rev, 2008; 78B: 1098 | | [22] | Eiken J, B?ttger B, Steinbach I.Phys Rev, 2006; 73E: 066122 | | [23] | Gustafson P.Metall Trans, 1987; 18A: 175 | | [24] | Umemoto M, Hiramatsu A, Moriya A, Watanabe T, Nanba S, Nakajima N, Anan G, Higo Y.ISIJ Int, 1992; 32: 306 | | [25] | Zheng C W, Xiao N M, Hao L H, Li D Z, Li Y Y.Acta Mater, 2009; 57: 2956 | | [26] | Du Q, Faber V, Gunzburger M.SIAM Rev, 1999; 41: 637 | | [27] | Chandra R, Dagum L, Kohr D, Maydan D, McDonald J, Menon R. Parallel Programming in Open MP. San Mateo: Morgan Kaufmann Publishers, 2000: 1 | | [28] | Chen H, van der Zwaag S.Acta Mater, 2014; 72: 1 | | [29] | van Leeuwen Y, Sietsma J, van der Zwaag S.ISIJ Int, 2003; 43: 767 | | [30] | van Bohemen S M C, Bos C, Sietsma J.Metall Mater Trans, 2011; 42A: 2609 |
|
|