砂型铸造Mg-6Al-xZn合金凝固行为及晶粒尺寸*
侯丹辉1,2, 梁松茂3, 陈荣石2(), 董闯1
1 大连理工大学材料科学与工程学院, 大连116024
2 中国科学院金属研究所, 沈阳110016
3 Institute of Metallurgy, Clausthal University of Technology, Clausthal-Zellerfeld, Germany, 38678
SOLIDIFICATION BEHAVIOR AND GRAIN SIZE OF SAND CASTING Mg-6Al-xZn ALLOYS
HOU Danhui1,2, LIANG Songmao3, CHEN Rongshi2(), DONG Chuang1
1 Institute of Material Science and Engineering, Dalian University of Techonlogy, Dalian 116024
2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3 Institute of Metallurgy, Clausthal University of Technology, Clausthal-Zellerfeld, Germany, 38678
引用本文:

侯丹辉, 梁松茂, 陈荣石, 董闯. 砂型铸造Mg-6Al-xZn合金凝固行为及晶粒尺寸*[J]. 金属学报, 2014, 50(5): 601-609.
Danhui HOU, Songmao LIANG, Rongshi CHEN, Chuang DONG. SOLIDIFICATION BEHAVIOR AND GRAIN SIZE OF SAND CASTING Mg-6Al-xZn ALLOYS[J]. Acta Metall Sin, 2014, 50(5): 601-609.

全文: PDF(9805 KB)   HTML
摘要: 

采用双电偶热分析技术和SEM表征了Mg-6Al-xZn合金(简称AZ6x合金, x=0, 2, 4, 6, 质量分数, %) 在砂型铸造过程中的凝固行为和显微组织; 采用背散射电子衍射(EBSD)分析对合金的晶粒尺寸进行定量表征. 利用Pandat热力学软件计算了合金的平衡截面相图、非平衡Scheil模型凝固过程, 以及枝晶生长抑制因子(growth restriction factor, 或称为Q值). 结果表明, 在AZ6x合金的砂型铸造凝固过程中, AZ60合金中只有非平衡凝固的γ-Mg17Al12, 而AZ62~AZ66合金的铸态组织中除了γ-Mg17Al12相, 还出现了Φ-Mg21(Al, Zn)17相, 并且随着Zn含量的增加, γ-Mg17Al12相减少而Φ-Mg21(Al, Zn)17相增多. 热力学计算结果表明, AZ60~AZ64合金中γ-Mg17Al12相和Φ-Mg21(Al,Zn)17相在一定温度下能够完全固溶到α-Mg中, 而AZ66合金中的Φ-Mg21(Al, Zn)17相在任何温度下都不可能完全固溶. 研究结果还表明, Zn含量高的合金具有高的Q 值、小的晶粒尺寸及低的枝晶相干点固相分数?sDCP; 并讨论了Q 值、晶粒尺寸与?sDCP的关系.

关键词 : Mg-Al-Zn合金,  砂型铸造,  晶粒尺寸,  枝晶生长抑制因子,  枝晶相干点固相分数    
Abstract:

The solidification behavior and microstructure evolution of sand cast Mg-6Al-xZn alloy (named as AZ6x alloys, x=0, 2, 4, 6, mass fraction, %) were characterized by two-thermocouple thermal analysis technology and SEM. The grain sizes of the alloys were quantitatively determined by EBSD technology. Thermodynamic calculations were applied in Pandat software for phase diagram calculation, Scheil model solidification simulation and growth restriction factor values (GRF or values). The results show that solidification of AZ6x alloys follows non-equilibrium solidification paths. Besides the γ-Mg17Al12 phase, which is the only secondary phase in AZ60 alloy, another Φ-Mg21(Al, Zn)17 phase appears in the as-cast microstructure of AZ62 to AZ66 alloys. With the increase of the Zn content, the amount of γ-Mg17Al12 phase decreases and while increase the amount of Φ-Mg21(Al, Zn)17 phase. Calculated equilibrium phase diagram shows that in the AZ60~AZ64 alloys both γ-Mg17Al12 phase and Φ-Mg21(Al, Zn)17 phase can be dissolved into α-Mg under proper heat treatment conditions. However, Φ-Mg21(Al, Zn)17 phase in AZ66 alloy can not be completely dissolved into a-Mg for any temperature. The results also indicate that higher Zn content alloys have higher values and smaller grain size, and lower solid fraction at dendrite coherency point (?sDCP). The relationship of values, grain size and ?sDCP has been also discussed.

Key words: Mg-Al-Zn alloy    sand casting    grain size    growth restriction factor    solid fraction at dendrite coherency point
收稿日期: 2013-09-05     
ZTFLH:  TG146.2  
基金资助:*国家重点基础研究发展计划项目2013CB632202及国家自然科学基金项目51105350和51301173资助
Alloy Al Zn Mn Mg
AZ60 5.74 - 0.22 Bal.
AZ62 5.79 1.90 0.21 Bal.
AZ64 5.69 3.70 0.24 Bal.
AZ66 5.82 5.66 0.28 Bal.
表1  合金的化学成分
图1  热分析实验装置图和双电偶热分析确定枝晶相干点示意图
图2  AZ6x合金的热分析结果及对应的铸态显微组织.
图3  热力学计算垂直截面Mg-5.76Al -0.24Mn-xZn四元平衡相图与AZ6x合金的冷却曲线热分析所得的相变温度点对比
Alloy Peak A TDCP Peak B Peak C
Tonset Tpeak Tonset Tpeak Tonset Tpeak
AZ60 617 614 610 439 436 - -
AZ62 610 608 604 407 404 - -
AZ64 602 599 593 389 385 361 359
AZ66 598 594 587 372 369 362 360
表2  从中心电偶热分析曲线中获得的凝固过程中对应的关键温度点(℃)
图4  利用Scheil模型计算以及热分析法得到的AZ6x合金凝固曲线
图5  Mg-6Al-xZn合金的EBSD图
图6  Mg-6Al-xZn合金枝晶相干温度的确定
图7  Zn含量对枝晶相干点固相分数?sDCP的影响
Alloy Average grain size / μm Q fsDCP-Scheil / % fsDCP-TA / %
AZ60 557 21 36 35
AZ62 275 28 27 27
AZ64 271 34 31 26
AZ66 235 43 23 25
表3  AZ6x合金中平均晶粒尺寸、枝晶生长抑制因子( Q 值)和枝晶相干点固相分数?sDCP
图8  不同溶质含量时枝晶形貌模拟图
[1] Luo A A. J Magnesium Alloys, 2013; 1: 2
[2] Ma Y Q, Chen R S, Han E H. Mater Lett, 2007; 61: 2527
[3] Maxwell I, Hellawell A. Acta Metall, 1975; 23: 229
[4] Greer A L, Bunn A M, Tronche A, Evans P V, Bristow D J. Acta Mater, 2000; 48: 2823
[5] St John D H, Qian M, Easton M A, Cao P, Hildebrand Z. Metall Mater Trans, 2005; 36A: 1669
[6] Schmid-Fetzer R, Kozlov A. Acta Mater, 2011; 59: 6133
[7] Veldman N L M, Dahle A K, St John D H, Arnberg L. Metall Mater Trans, 2001; 32A: 147
[8] Liang S M, Chen R S, Blandin J J, Suery M, Han E H. Mater Sci Eng, 2008; A480: 365
[9] Arnberg L, Chai G, Backerud L. Mater Sci Eng, 1993; A173: 101
[10] Dahle A K, Arnberg L. Mater Sci Eng, 1997; A225: 38
[11] Chai G, Bäckerud L, RØlland T, Arnberg L. Metall Mater Trans, 1995; 26A: 965
[12] Malekan M, Shabestari S G. Metall Mater Trans, 2009; 40A: 3196
[13] Liang S M. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009
[13] (梁松茂. 中国科学院金属研究所博士学位论文, 沈阳, 2009)
[14] Bäckerud L, Krol E, Tamminen J. Solidification Characteristics of Aluminium Alloys. Vol.1, Oslo: Skan Aluminium, 1986: 65
[15] Chang H W, Qiu D, Taylor J A, Easton M A, Zhang M X. J Magnesium Alloys, 2013; 1: 115
[16] Kierkus W T, Solokowski J H. AFS Trans, 1999; 107: 161
[17] Cao W, Chen S L, Zhang F, Wu K, Yang Y, Chang Y A, Schmid-Fetzer R, Oates W A. Calphad, 2009; 33: 328
[18] Liang P, Tarfa T, Robinson J A, Wagner S, Ochin P, Harmelin M G, Seifert H J, Lukas H L, Aldinger F. Thermochim Acta, 1998; 314: 87
[19] Ohno M, Schmid-Fetzer R. Z Metallkd, 2005; 96: 857
[20] Ohno M, Mirković D, Schmid-Fetzer R. Mater Sci Eng, 2006; A421: 328
[21] Ohno M, Schmid-Fetzer R. Int J Mater Res, 2006; 97: 526
[22] Ohno M, Mirković D, Schmid-Fetzer R. Acta Mater, 2006; 54: 3883
[23] Thorvaldsen A, Aliravci C A. In: Proc International Symposium, Montreal, Canada: Metallurgical of CIM, 1992: 277
[24] Tamura Y, Yagi J, Haitani T, Motegi T, Kono N, Tamehiro H, Saito H. Mater Trans, 2003; 44: 552
[25] Liang S M, Ma Y Q, Chen R S, Han E H. Mater Trans, 2008; 49: 986
[1] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[2] 王春辉, 杨光昱, 阿热达克·阿力玛斯, 李晓刚, 介万奇. 砂型3DP打印参数对ZL205A合金铸造性能的影响[J]. 金属学报, 2022, 58(7): 921-931.
[3] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.
[4] 李晓倩, 王富国, 梁爱民. 喷涂工艺对Ta2O5原位复合钽基纳米晶涂层微观结构及摩擦磨损性能的影响[J]. 金属学报, 2021, 57(2): 237-246.
[5] 张守清, 胡小锋, 杜瑜宾, 姜海昌, 庞辉勇, 戎利建. 海洋平台用Ni-Cr-Mo-B超厚钢板的截面效应[J]. 金属学报, 2020, 56(9): 1227-1238.
[6] 许占一, 沙玉辉, 张芳, 章华兵, 李国保, 储双杰, 左良. 取向硅钢二次再结晶过程中的取向选择行为[J]. 金属学报, 2020, 56(8): 1067-1074.
[7] 和淑文, 王鸣华, 白琴, 夏爽, 周邦新. WC-TiC-TaC-Co硬质合金中TaC含量对其显微组织和力学性能的影响[J]. 金属学报, 2020, 56(7): 1015-1024.
[8] 华涵钰,谢君,舒德龙,侯桂臣,盛乃成,于金江,崔传勇,孙晓峰,周亦胄. W含量对一种高W镍基高温合金显微组织的影响[J]. 金属学报, 2020, 56(2): 161-170.
[9] 李鑫,董月成,淡振华,常辉,方志刚,郭艳华. 等通道角挤压制备超细晶纯Ti的腐蚀性能研究[J]. 金属学报, 2019, 55(8): 967-975.
[10] 梅益, 孙全龙, 喻丽华, 王传荣, 肖华强. 基于GA-ELM的铝合金压铸件晶粒尺寸预测[J]. 金属学报, 2017, 53(9): 1125-1132.
[11] 张明, 刘国权, 胡本芙. 镍基粉末高温合金热加工变形过程中显微组织不稳定性对热塑性的影响[J]. 金属学报, 2017, 53(11): 1469-1477.
[12] 付全,沙玉辉,和正华,雷蕃,张芳,左良. Fe81Ga19二元合金薄板的再结晶织构与磁致伸缩性能[J]. 金属学报, 2017, 53(1): 90-96.
[13] 宋永锋, 李雄兵, 吴海平, 司家勇, 韩晓芹. In718晶粒尺寸对超声背散射信号的影响及其无损评价方法*[J]. 金属学报, 2016, 52(3): 378-384.
[14] 刘觐,朱国辉. 超细晶粒钢中晶粒尺寸对塑性的影响模型*[J]. 金属学报, 2015, 51(7): 777-783.
[15] 赵清,夏爽,周邦新,白琴,苏诚,王宝顺,蔡志刚. 形变及热处理对825合金管材晶界特征分布的影响*[J]. 金属学报, 2015, 51(12): 1465-1471.