| 超高压凝固Mg82.13Zn13.85Y4.02合金的组织及室温压缩性能* |
董允1, 林小娉1( ), 徐瑞2, 樊志斌1, 叶杰1, 王哲2 |
1 东北大学材料与冶金学院, 沈阳 110819 2 燕山大学材料科学与工程学院, 亚稳材料制备技术与科学国家重点实验室, 秦皇岛 066004 |
|
| MICROSTRUCTURE AND ROOM TEMPERATURE COMPRESSION PROPERTIES OF Mg82.13Zn13.85Y4.02 ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE |
DONG Yun1, LIN Xiaoping1( ), XU Rui2, FAN Zhibin1, YE Jie1, WANG Zhe2 |
1 Department of Materials Science and Engineering, Northeastern University, Shenyang 110819 2 State Key Laboratory of Metastable Materials Science and Technology, School of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004 |
引用本文:
董允, 林小娉, 徐瑞, 樊志斌, 叶杰, 王哲. 超高压凝固Mg82.13Zn13.85Y4.02合金的组织及室温压缩性能*[J]. 金属学报, 2014, 50(5): 594-600.
Yun DONG,
Xiaoping LIN,
Rui XU,
Zhibin FAN,
Jie YE,
Zhe WANG.
MICROSTRUCTURE AND ROOM TEMPERATURE COMPRESSION PROPERTIES OF Mg82.13Zn13.85Y4.02 ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE[J]. Acta Metall Sin, 2014, 50(5): 594-600.
| [1] |
Somekawa H, Watanabe H, Mukai T. Mater Lett, 2011; 65: 3251
|
| [2] |
Xu S W, Zheng M Y, Kamado S, Wu K, Wang G J, Lv X Y. Mater Sci Eng, 2011; A528: 4055
|
| [3] |
Luo S Q, Tang A T, Pan F S, Song K, Wang W Q. Trans Nonferrous Met Soc China, 2011; 21: 795
|
| [4] |
Chen B, Chen L, Lin D L, Zeng X Q. Trans Nonferrous Met Soc China, 2012; 22: 773
|
| [5] |
Wang J F, Gao S, Song P F, Huang X F, Shi Z Z, Pan F S. J Alloys Compd, 2011; 509: 8567
|
| [6] |
Yang W P, Guo X F, Lu Z X. Trans Nonferrous Met Soc China, 2012; 22: 786
|
| [7] |
Lee J Y, Kim D H, Lim H K, Kim D H. Mater Lett, 2005; 59: 3801
|
| [8] |
Tong J, Huang H, Yuan G Y, Ding W J. Acta Metall Sin, 2011; 47:1520
|
| [8] |
(童 健, 黄 华, 袁广银,丁文江. 金属学报, 2011; 47: 1520)
|
| [9] |
Somekawa H, Singh A, Mukai T. Adv Eng Mater, 2009; 11: 782
|
| [10] |
Luo Z P, Zhang S Q, Tang Y L, Zhao D S. Scr Metall Mater, 1993; 28: 1513
|
| [11] |
Tsai A, Niikura A, Inoue A. J Mater Res, 1997; 12: 565
|
| [12] |
Батншeв А И,translated byZhang J S. Crystallization of Metal and Alloys Under Pressure. Harbin: Harbin University of Techonology Press, 1987: 23
|
| [12] |
(Батншeв А И 著,张锦升 译. 金属和合金在压力下结晶. 哈尔滨: 哈尔滨工业大学出版社, 1987: 23)
|
| [13] |
Qu Y D, Li R D, Yuan X G, Li C X, Xiang Q C. Foundry, 2005; 54: 539
|
| [13] |
(曲迎东, 李荣德, 袁晓光, 李晨曦, 向青春. 铸造, 2005; 54: 539)
|
| [14] |
Zhang G Z, Yu X F, Wang X Y, Jia G L, Gao Y Y. Acta Metall Sin, 1999; 35: 285
|
| [14] |
(张国志, 于溪凤, 王向阳, 贾光霖, 高允彦. 金属学报, 1999; 35: 285)
|
| [15] |
Jie J C, Zou C M, Wang H W, Wei Z J. J Alloys Compd, 2010; 506: L12
|
| [16] |
Chen Y, Liu L, Wang Y H, Liu J H, Zhang R J. Trans Nonferrous Met Soc China, 2011; 21: 2205
|
| [17] |
Wang Z X, Lu J B, Xi Y J, Fan J W. J Alloys Compd, 2010; 492: 529
|
| [18] |
Wang D Q, Yang G C, Lin L, Feng Z G. Mater Lett, 2008; 62: 1711
|
| [19] |
Wang Z L, Zhang T, Li L, Zhou Y B, Wang H W, Wei Z J. Chin J Nonferrous Met, 2012; 22: 1006
|
| [19] |
(王振玲, 张 涛, 李 莉, 周月波, 王宏伟, 魏尊杰. 中国有色金属学报, 2012; 22: 1006)
|
| [20] |
Sun S H,Li J,Xu R,Zhao H L,Liu R P. Chin J High Pressure Phys, 2008; 22: 434
|
| [20] |
(孙淑华, 李 杰, 徐 瑞, 赵海丽, 刘日平. 高压物理学报, 2008; 22: 434)
|
| [21] |
Lin X P, Dong Y, Xu R, Sun G F, Jiao S H. Acta Metall Sin, 2011; 47: 1550
|
| [21] |
(林小娉, 董 允, 徐 瑞, 孙桂芳, 焦世辉. 金属学报, 2011; 47: 1550)
|
| [22] |
Lin X P, Dong Y, Xu R, Zheng R G. Rare Met Mater Eng, 2013; 42: 2309
|
| [22] |
(林小娉, 董 允, 徐 瑞, 郑润国. 稀有金属材料与工程, 2013; 42: 2309 )
|
| [23] |
Li B, Wang H W, Jie J C, Wei Z J. J Alloys Compd, 2011; 509: 3387
|
| [24] |
Ding W J. The Science and Technology of Mg Alloy. Beijing: Science Press, 2007: 1
|
| [24] |
(丁文江. 镁合金科学与技术. 北京: 科学出版社, 2007: 1)
|
| [25] |
Jiang X S,Zhao H. Quick Reference for Microscopic Fracture of Steel. Beijing: Machinery Industry Press, 2010: 45
|
| [25] |
(姜锡山,赵 晗. 钢铁显微断口速查手册. 北京: 机械工业出版社, 2010: 45)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|