| RE对过共晶Al-80%Si合金凝固特性的影响* |
文强, 坚增运( ), 朱满, 常芳娥, 党博 |
| 西安工业大学陕西省光电功能材料与器件重点实验室, 西安 710021 |
|
| EFFECTS OF RE ON THE SOLIDIFICAIION CHARACTERISTICS OF Al-80%Si ALLOY |
WEN Qiang, JIAN Zengyun( ), ZHU Man, CHANG Fang'e, DANG Bo |
| Shaanxi Province Key Laboratory of Photoelectric Functional Materials and Devices, Xi'an Technological University, Xi'an 710021 |
引用本文:
文强, 坚增运, 朱满, 常芳娥, 党博. RE对过共晶Al-80%Si合金凝固特性的影响*[J]. 金属学报, 2014, 50(5): 610-618.
Qiang WEN,
Zengyun JIAN,
Man ZHU,
Fang'e CHANG,
Bo DANG.
EFFECTS OF RE ON THE SOLIDIFICAIION CHARACTERISTICS OF Al-80%Si ALLOY[J]. Acta Metall Sin, 2014, 50(5): 610-618.
| [1] |
Zuo M, Jiang K F, Liu X F. J Alloys Compd, 2010; 503: L26
|
| [2] |
Faraji M, Todd I, Jones H. J Mater Sci, 2005; 40: 6363
|
| [3] |
Jiang Q C, Xu C L, Lu M, Wang H Y. Mater Lett, 2005; 59: 624
|
| [4] |
Yi H, Zhang D. Mater Lett, 2003; 57: 2523
|
| [5] |
Ohmi T, Matsuura K, Kudoh M. J Jpn Inst Light Met, 1998; 48: 618
|
| [6] |
Jian Z Y, Zhu M, Jie W Q. Mater China, 2010; 29: 20
|
| [6] |
(坚增运, 朱 满, 介万奇. 中国材料进展, 2010; 29: 20)
|
| [7] |
Hernandez F C R, Sokolowski J H. J Alloys Compd, 2006; 426: 205
|
| [8] |
Jin F W, Ren Z M, Ren W L, Deng K, Zhong Y B, Yu J B. Sci Technol Adv Mater, 2008; 9: 024202
|
| [9] |
Xu C L, Wang H Y, Yang F Y, Jiang Q C. Mater Sci Eng, 2007; A452: 341
|
| [10] |
Zuo M, Liu X F, Sun Q Q, Jiang K. J Mater Process Technol, 2009; 209: 5504
|
| [11] |
Zhang Q, Liu X F, Dai H S. J Alloys Compd, 2009; 480: 376
|
| [12] |
Yu L N, Liu X F, Ding H M, Bian X F. J Alloys Compd, 2007; 432: 156
|
| [13] |
Zuo M, Zhao D G, Teng X Y, Geng H R, Zhang Z S. Mater Des, 2013; 47: 857
|
| [14] |
Wu Y P, Wang S J, Li H, Liu X F. J Alloys Compd, 2009; 477: 139
|
| [15] |
Shi W X, Gao B, Tu G F, Li S W, Hao Y, Yu F X. J Rare Earth, 2010; 28: 367
|
| [16] |
Chang J Y, Kim G H, Moon I G, Choi C S. Scr Mater, 1998; 39: 307
|
| [17] |
Chen C, Liu Z X, Ren B, Wang M X, Weng Y G, Liu Z Y. Trans Nonferrous Met Soc China, 2007; 17: 301
|
| [18] |
Li Q L, Xia T D, Lan Y F, Li P F, Fan L. Mater Sci Eng, 2013; A588: 97
|
| [19] |
Wei B K, Lin H T, Liu J M, Cai Q Z, Tong X L, Mao Y F. Spec Cast Nonferrous Alloys, 1993; (3): 6
|
| [19] |
(魏伯康, 林汉同, 刘俊明, 蔡启舟, 童杏林, 毛玉凤. 特种铸造及有色合金, 1993; (3): 6)
|
| [20] |
Xu C L, Jiang Q C, Yang Y F, Wang H Y, Wang J G. J Alloys Compd, 2006; 422: L1
|
| [21] |
Shi W X, Gao B, Tu G F, Li S W. J Alloys Compd, 2010; 508: 480
|
| [22] |
Li Q L, Xia T D, Lan Y F, Zhao W J, Fan L, Li P F. J Alloys Compd, 2013; 562: 25
|
| [23] |
Jian Z Y, Nagashio K, Kuribayashi K. Metall Mater Trans, 2002; 33A: 2947
|
| [24] |
Jian Z Y, Kuribayashi K, Jie W Q, Chang F E. Acta Mater, 2006; 54: 3227
|
| [25] |
Liu R P, Volkmann T, Herlach D M. Acta Mater, 2001; 49: 439
|
| [26] |
Wang Q, Liu R P, Qian Y Q, Lou D C, Su Z B, Ma M Z, Wang W K, Panofen C, Herlach D M. Scr Mater, 2006; 54: 37
|
| [27] |
Lu S Z, Hellawell A. Metall Mater Trans, 1987; 18A: 1721
|
| [28] |
Jian Z Y, Yang X Q, Chang F E, Jie W Q. Metall Mater Trans, 2010; 41A: 1826
|
| [29] |
David R L. CRC Handbook of Chemistry and Physics. Tokyo: CRC Press, 1989: B2
|
| [30] |
Jian Z Y, Kuribayashi K, Jie W Q. Acta Mater, 2004; 52: 3323
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|