| 690TT合金划痕显微组织及划伤诱发的应力腐蚀 |
| 孟凡江1), 王俭秋1), 韩恩厚1), 庄子哲雄2), 柯伟1) |
1) 中国科学院金属研究所腐蚀与防护国家重点实验室, 沈阳 110016
2) 日本东北大学断裂与可靠性研究中心, 仙台 980-8579 |
|
| MICROSTRUCTURE NEAR SCRATCH ON ALLOY 690TT AND STRESS CORROSION INDUCED BY SCRATCHING |
| MENG Fanjiang1), WANG Jianqiu1), HAN En-Hou1), SHOJI Testuo2), KE Wei1) |
1) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2) Fracture and Reliability Research Institute, Tohoku University, Sendai 980-8579, Japan |
引用本文:
孟凡江 王俭秋 韩恩厚 庄子哲雄 柯伟. 690TT合金划痕显微组织及划伤诱发的应力腐蚀[J]. 金属学报, 2011, 47(7): 839-846.
,
.
MICROSTRUCTURE NEAR SCRATCH ON ALLOY 690TT AND STRESS CORROSION INDUCED BY SCRATCHING[J]. Acta Metall Sin, 2011, 47(7): 839-846.
| [1] Ding X S. Nucl Power Plants, 2003; 4: 11(丁训慎. 核电站, 2003; 4: 11)[2] Blanchet J, Coriou H, Grall L, Mahieu C, Otter C, Turluer G. In: Staehle R W, Hochmann J, McCright R D, Slater J E, eds., Stress Corrosion Cracking and Hydrogen Embrittlement of Iron Base Alloys, No.5, Houston: NACE, 1977: 1149[3] Staehle R W, Gorman J A. Corrosion, 2003; 59: 931[4] Laboratory Evaluation of Steam Generator Tube Sections from the McGuire Nuclear Station. Babcock & Wilcox, Report RDD:91:5087–01:01, October, 1990: 1[5] Examination of Steam Generator Tube Sections from the McGuire Unit 2 Nuclear Station. Babcock & Wilcox–NESI, Report LTC:93:0021–01:01, January, 1993: 1[6] Analysis of Steam Generator Tubing from Oconee Unit 1 Nuclear Station. EPRI report TR–106484[7] Oconee 2 Steam Generator Tube Examination. EPRI report TR–106863[8] MacDonald P E, Shah V N,Ward LW, Ellison P G. Steam Generator Tube Failures. NUREG/CR–6365[9] Rochester D P. Water Chemistry of Nuclear Reactor Systems. 1st Ed., London: Thomas Telford Publishing, 2001: 1[10] Staehle R W, Gorman J A. Corrosion, 2004; 60: 115[11] Staehle R W, Gorman J A. Corrosion, 2004; 60: 5[12] Meng F J, Wang J Q, Han E H, Ke W. Corros Sci, 2009; 51: 2761[13] Tkaya M B, Zidi M, Mezlini S, Zahouani H, Kapsa P. Mater Des, 2008; 29: 98[14] Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K. Acta Mater, 2002; 50: 4603[15] Symons D. Metall Mater Trans, 1997; 28A: 655[16] Tao N R, Zhang H W, Lu J, Lu K. Metall Trans, 2003; 44: 1919[17] Hwang S, Kim H, Lim Y, Kim Y, Thomas L. Corros Sci, 2007; 49: 3797[18] Hwang S, Kim H, Lee D, Kim U, Kim J. J Nucl Mater, 1999; 275: 28[19] Lumsden J, McIlree A, Eaker R, Thompson R, Slosnerick S. Proc 12th Int Conf Environmental Degradation of Materials in Nuclear Power System–Water Reactors, Salt Lake City, Utah, USA, 2005: 1[20] Meng F J, Han E H, Wang J Q, Zhang Z M, Ke W. Electrochim Acta, 2011; 56: 1781 |
|