| TiN夹杂物对690合金管在高温高压水中的腐蚀和应力腐蚀行为的影响 |
| 郦晓慧, 黄发, 王俭秋, 韩恩厚, 柯伟 |
| 中国科学院金属研究所腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER |
| LI Xiaohui, HUANG Fa, WANG Jianqiu, HAN En--Hou, KE Wei |
| State Key laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
郦晓慧 黄发 王俭秋 韩恩厚 柯伟. TiN夹杂物对690合金管在高温高压水中的腐蚀和应力腐蚀行为的影响[J]. 金属学报, 2011, 47(7): 847-852.
,
.
INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. Acta Metall Sin, 2011, 47(7): 847-852.
| [1] Crum J R. Corrosion, 1986; 42: 368[2] Dutta R S, Tewari R, De P K. Corros Sci, 2007; 49: 303[3] Dutta R S, Tewari R. Br Corros J, 1999; 34: 201[4] Cheung C, Erb U, Palumbo G. Mater Sci Eng, 1994; A185: 39[5] Ahn S, Rao V S, Kwon H, Kim U. Corros Sci, 2006; 48: 1137[6] Fairchild D P, Howden D G, Clark W A T. Metall Mater Trans, 2000; 31A: 641[7] Yan W, Shan Y Y, Yang K. Metall Mater Trans, 2006; 37A: 2147[8] Lim Y S, Kim J S, Kwon H S. J Nucl Mater, 2005; 336: 65[9] Meng F, Wang J, Han E H, Ke W. Corros Sci, 2009; 52: 927[10] Macdonald D D, Scot A C, Wentrcek P. J Electrochem Soc, 1979; 126: 908[11] Dutta R S, Lobo A, Purandare R, Kulkarni S K, Dey G K. Metall Mater Trans, 2002; 33A: 1437[12] Kuo T Y, Lee H T. Mater Sci Eng, 2002; A338: 202[13] Dutta R S, Purandare R, Lobo A, Kulkarni S K, Dey G K. Corros Sci, 2004; 46: 2937[14] Was G S, Kruger R M. Acta Metall, 1985; 33: 841[15] Kai J, Yu G, Tsai C, Liu M, Yao S. Metall Mater Trans, 1989; 20A: 2057[16] In C B, Kim Y I, KimW W, Kim J S, Chun S S, LeeW J. J Nucl Mater, 1995; 224: 71[17] Feron D, Lambert I. In: Proc 12th Int Conf Properties of Water and Steam, IAPWS, Orlando, FL, USA, 1994: 783[18] Yamanaka K. In: Proc 5th Int Symp Enviromental Degradation of Materials in Nuclear Power Systems–Water Reactors, California: American Nuclear Society, TMS, NACE, 1991: 773[19] Was G, Tischner H, Latanision R. Metall Mater Trans, 1981; 12A: 1397[20] Yu G P, Yao H C. Corrosion, 1990; 46: 391 |
|