不锈钢表面Cr-Pd合金电沉积及镀层在强还原性介质中的耐蚀性 |
徐亮, 唐鋆磊, 左禹 |
北京化工大学材料科学与工程学院, 北京 100029 |
|
ELECTROPLATING OF Cr-Pd ALLOY ON 316L STAINLESS STEEL AND ITS CORROSION RESISFANCE IN THE STRONG REDUCING MEDIUMS |
XU Liang, TANG Junlei, ZUO Yu |
School of Materials Science and Engineering, Beijing University of Chemical Technology, Beijing 100029 |
引用本文:
徐亮 唐鋆磊 左禹. 不锈钢表面Cr-Pd合金电沉积及镀层在强还原性介质中的耐蚀性[J]. 金属学报, 2011, 47(2): 209-213.
,
,
.
ELECTROPLATING OF Cr-Pd ALLOY ON 316L STAINLESS STEEL AND ITS CORROSION RESISFANCE IN THE STRONG REDUCING MEDIUMS[J]. Acta Metall Sin, 2011, 47(2): 209-213.
[1] Tang J L, Zuo Y. Corros Sci, 2008; 50: 2873[2] Zuo Y, Tang J L, Fan C Z, Tang Y M, Xiong J P. Thin Solid Films, 2008; 516: 7565[3] Tang J L, Zuo Y,Tang YM,Xiong J P. Surf Coat Technol, 2010; 204: 1637[4] Gao X, Tang J L, Zuo Y, Tang Y M, Xiong J P. Corros Sci, 2009; 51: 1822[5] Samaik K M, Palrecha M M, Dhaneshwar R G. J Electrochem Soc, 1989; 136: 283[6] Hsieh A K, Ee Y H. Met Finish, 1993; 91: 53[7] Zeng Z, Liang A, Zhang J. Electrochim Acta, 2008; 53: 7344[8] Abys J A. US Pat, 6346222, 2002[9] Li B, Lin A, Wu X, Zhang Y, Gan F. J Alloys Compd, 2008; 453: 93[10] Yang F Z, Xu S K, Yao S B, Chen B Y, Zheng X Q, Zhong X H, Zhou S M. Electrochemistry, 1997; 3(1): 107(杨防祖, 许书楷, 姚士冰, 陈秉彝, 郑雪清, 钟晓慧, 周绍民. 电化学, 1997; 3(1): 107)[11] L¨u W, Zhang Y X. J Fujian Norm Univ (Nat Sci), 2002; 18(1): 51(吕玮, 张永祥. 福建师范大学学报(自然科学版), 2002; 18(1): 51)[12] Guan S, Zhang Q, Hu R N. Mater Prot, 2000; 20(3): 1(关 山, 张 琦, 胡如南. 材料保护, 2000; 20(3): 1)[13] Hou J L, Yan X J, Feng L J, Zhu J. Foundry Technol, 2009; 30: 1067(侯娟玲, 闫小军, 冯拉俊, 祝捷. 铸造技术, 2009; 30: 1067)[14] Raub Ch J. Platinum Metals Rev, 1982; 26: 158[15] Hamm D, Olsson C A, Landolt D. Corros Sci, 2002; 44: 1009[16] Hermas A A, Nakayama M, Ogura K. Electrochim Acta, 2005; 50: 2001 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|