| (Au, Ag, Cu)/SiO2二元金属单分散复合薄膜非线性光吸收性的Mie理论模拟 |
| 严丽平, 张波萍, 王士京, 赵翠华, 李顺 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| SIMULATION ON NONLINEAR OPTICAL ABSORPTION OF BINARY METALS DISPERSED (Au, Ag, Cu)/SiO2 NANO-COMPOSITE FILMS BY MODIFIED MIE THEORY |
| YAN Liping, ZHANG Boping, WANG Shijing, ZHAO Cuihua, LI Shun |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
严丽平 张波萍 王士京 赵翠华 李顺. (Au, Ag, Cu)/SiO2二元金属单分散复合薄膜非线性光吸收性的Mie理论模拟[J]. 金属学报, 2011, 47(2): 203-208.
,
,
,
,
.
SIMULATION ON NONLINEAR OPTICAL ABSORPTION OF BINARY METALS DISPERSED (Au, Ag, Cu)/SiO2 NANO-COMPOSITE FILMS BY MODIFIED MIE THEORY[J]. Acta Metall Sin, 2011, 47(2): 203-208.
| [1] Ni X Y, Lu J X, Wei J D. Acta Opt Sin, 2004; 24: 433(倪星元, 吕俊霞, 魏建东. 光学学报, 2004; 24: 433)[2] Li Y, Sun X W, Wang J. Acta Opt Sin, 2005; 25: 77(李 燕, 孙小伟, 王 建. 光学学报, 2005; 25: 77)[3] Wang W T, Yang G, Chen Z H. J Appl Phys, 2002; 92: 7242[4] Yu B L, Zhu C S, Gan F X. Acta Phys Sin, 1997; 46: 2394(于保龙, 朱从善, 干福熙. 物理学报, 1997; 46: 2394)[5] Bohren C F. Absorption and Scattering of Light by Small Particles. New York: Wiley, 1983: 130[6] Huang W Y, Qian W, El–Sayed M A. Nano Lett, 2004; 4: 1741[7] Feldheim D L, Colby A F. Metal Nanoparticles: Synthesis, Characterization and Applications. New York: Marcel Dekker, 2002: 89[8] Gao L Z, Zhang X T, Dai S X. Acta Phys–Chim Sin, 2004; 20: 647(高丽珍, 张兴堂, 戴树玺. 物理化学学报, 2004; 20: 647)[9] Liu L, Su X R. Chin Phys, 2008; 17B: 2170[10] Zhao C H, Zhang B P, Shang P P. Chin Phys, 2009; 18B: 5539[11] Yang P F, Cu Y, Gong Q H. Chin Phys, 2008; 17B: 3880[12] Yang G, Chen Z |. Acta Phys Sin, 2006; 55: 4342(杨 光, 陈正豪. 物理学报, 2006; 55: 4342)[13] Shi H Z, Zhang L, Cai W P. J Appl Phys, 2000; 87: 1572[14] Sun X F, Wei C P, Li Q Y. Acta Phys Sin, 2009; 58: 5816(孙小飞, 魏长平, 李启源. 物理学报, 2009; 58: 5816)[15] Lei D Y, Li J, Ong H C. Appl Phys Lett, 2007; 91: 021112[16] De G, Tapfer L, Catalano M. Appl Phys Lett, 1996; 68: 3820[17] Kreibig U, Vollmer M. Optical Properties of Metal Clusters. Berlin: Springer, 1995: 379[18] Arnold G W, Bordes J A. J Appl Phys, 1977; 48: 1488[19] Halperin W P. Rev Mod Phys, 1986; 58: 533[20] Liao H B, Wen W J, Wong G K. J Appl Phys, 2003; 93: 4485[21] Tanahashi I, Manabe Y, Tohda T. J Appl Phys, 1996; 79: 1244[22] Babapour A, Akhavan O, Moshfegh A Z. Thin Solid Films, 2006; 515: 77[23] Beckers L, Schubert J, Zander W. J Appl Phys, 1998; 83: 3305[24] Palik E D. Handbook of Optical Constants of Solids. San Diego: Academic Press, 1985: 735 |
|