铝合金/镁合金搅拌摩擦焊接界面处Mg/Al反应及接头力学性能 |
王东1); 刘杰2); 肖伯律1); 马宗义1) |
1) 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016
2) 中航工业黎明公司; 沈阳 110043 |
|
Mg/Al REACTION AND MECHANICAL PROPERTIES OF Al ALLOY/Mg ALLOY FRICTION STIR WELDING JOINTS |
WANG Dong1); LIU Jie2); XIAO Bolv1); MA Zongyi1) |
1) Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
2) Shenyang Liming Corporation; Aviation Industry Corporation of China; Shenyang 110043 |
引用本文:
王东 刘杰 肖伯律 马宗义. 铝合金/镁合金搅拌摩擦焊接界面处Mg/Al反应及接头力学性能[J]. 金属学报, 2010, 46(5): 589-594.
,
,
,
.
Mg/Al REACTION AND MECHANICAL PROPERTIES OF Al ALLOY/Mg ALLOY FRICTION STIR WELDING JOINTS[J]. Acta Metall Sin, 2010, 46(5): 589-594.
[1] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37
[2] Hatch J E. Aluminum Properties and Physical Metallurgy, Metals Park, Ohio: American Society for Metals, 1984: 1
[3] Liu P, Li Y J, Geng H R, Wang J. Mater Lett, 2007; 61: 1288
[4] Liu L M, Liu X J, Liu S H. Scr Mater, 2006; 55: 383
[5] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[6] Ren S R, Ma Z Y, Chen L Q. Acta Metall Sin, 2007; 42: 225
(任淑荣, 马宗义, 陈礼清. 金属学报, 2007; 42: 225)
[7] Xie G M, Ma Z Y, Geng L. Acta Metall Sin, 2008; 44: 655
(谢广明, 马宗义, 耿 林. 金属学报, 2008; 44: 655)
[8] Xie G M, Ma Z Y, Geng L. J Mater Sci Technol, 2009; 25: 351
[9] Khodir S A, Shibayanagi T. Mater Trans, 2007; 48: 2501
[10] Somasekharan A C, Murr L E. Mater Charact, 2004; 52: 49
[11] Yan J C, Xu Z W, Li Z Y, Li L, Yang S Q. Scr Mater, 2005; 53: 585
[12] Kostka A, Coelho R S, Santos J D, Pyzallac A R. Scr Mater, 2009; 60: 953
[13] Sato Y S, Park S H C, Michiuchi M, Kokawa H. Scr Mater, 2004; 50: 1233
[14] Chen Z W, Cui S. Scr Mater, 2008; 58: 417
[15] Prangnell P B, Heason C P. Acta Mater, 2005; 53: 3179
[16] Fatemi–Varzaneh S M, Zarei–Hanzaki A, Haghshenas M. Mater Sci Eng, 2008; A497: 438
[17] Wang Z T, Tian R Z. Handbook of Aluminum Alloy and Processing. 3rd, Changsha: Central South University Press, 2005: 317
(王祝堂, 田荣璋. 铝合金及其加工手册(第3版). 长沙: 中南大学出版社, 2005: 317)
[18] Feng A H, Ma Z Y. Scr Mater, 2007; 56: 397
[19] Mahoney M W, Rhodes C G, Flintoff J G, Spurling R A, Bingel W H. Metall Mater Trans, 1998; 29A: 1955
[20] Yang J, Xiao B L, Wang D, Ma Z Y. Mater Sci Eng, 2010; A527: 708
[21] Liu F C, Ma Z Y. Metall Mater Trans, 2008; 39A: 2378 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|