Acta Metall Sin  1993, Vol. 29 Issue (2): 31-36    DOI:
Current Issue | Archive | Adv Search |
MECHANICAL PROPERTIES AND б-PHASE EMBRITTLEMENT IN A FERRITE-AUSTENITE STAINLESS STEEL AT ELEVATED TEMPERATURES
WU Tiyan;WU Qibai;Y. Riquier Central-South University of Technology; Changsha; Faculte Polytechnique de Mons; Belgium
Cite this article: 

WU Tiyan;WU Qibai;Y. Riquier Central-South University of Technology; Changsha; Faculte Polytechnique de Mons; Belgium. MECHANICAL PROPERTIES AND б-PHASE EMBRITTLEMENT IN A FERRITE-AUSTENITE STAINLESS STEEL AT ELEVATED TEMPERATURES. Acta Metall Sin, 1993, 29(2): 31-36.

Download:  PDF(2141KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The mechanical properties of a ferritic-austenitic duplex stainless steel has beeninvestigated in the temperature range between 600 to 1100℃. The variation of ductilityagainst temperature has a minimum at 800--900℃. While at about 600℃ ferrite deformedcooperatively with austenite. With increasing temperature the coordination decreased. Evenat 1100℃ ferrite dominated the deformation process. The kinetics of σ-phase precipitationand the effect of σ-phase on tensile properties have also been revealed. The ductility of spec-imens deformed at about 600℃ was largely reduced by σ-phase and the effects of σ-phaseincreased with increasing σ-phase fraction but exhibit significant temperature dependence.When a specimen consisting of 16% σ-phase was tested at 900℃, σ-phase particle bandswere realigned parallel to the shearinng directions. Final fracture was preceded by plasticdeformation. At about 1000℃ the effect of σ-phase precipitation on tensile properties disap-peared, while fine dispersion of secondary austenite within ferrite strengthened the materialslightly.
Key words:  duplex stainless steel      σ-phase      mechanical property     
Received:  18 February 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I2/31

1 Hayden H W, Floreen S. Metall Trans, 1973; 4A: 561
2 Maehara Y, Ohmori Y, Kunitake T. Met Technol, 1983; 10: 296
3 Maehara Y, Koike M, Fujino N, Kunitake T. Trans Iron Steel Inst Jpn, 1983; 23: 240
4 Beetge F G E, Robinson F P A. Met Mater, 1973; 7 (9) 408
5 DeBold T A. J Met, 1989; 41 (3) : 12
6 Norstrom L A, Pettersson S, Nordin S. Z Werkstofftech, 1981; 23: 229
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[9] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[10] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[11] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[12] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[13] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[14] LI Shujun, HOU Wentao, HAO Yulin, YANG Rui. Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique[J]. 金属学报, 2023, 59(4): 478-488.
[15] WANG Hu, ZHAO Lin, PENG Yun, CAI Xiaotao, TIAN Zhiling. Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition[J]. 金属学报, 2023, 59(2): 226-236.
No Suggested Reading articles found!