| SURFACE STATE AND OXIDATION BEHAVIOUR OF AMORPHOUS Ni_(63)Zr_(37) ALLOY |
| WANG Xike;SHEN Ningfu;SHI Guangxin;ZHANG Haifeng;GU Haicheng Zhengzhou Institute of Technology; Luoyang Ship Materials Research Institute; Xi'an Jiaotong University |
|
Cite this article:
WANG Xike;SHEN Ningfu;SHI Guangxin;ZHANG Haifeng;GU Haicheng Zhengzhou Institute of Technology; Luoyang Ship Materials Research Institute; Xi'an Jiaotong University. SURFACE STATE AND OXIDATION BEHAVIOUR OF AMORPHOUS Ni_(63)Zr_(37) ALLOY. Acta Metall Sin, 1993, 29(2): 24-30.
|
|
|
Abstract Investigations were made of the surface state of amorphous Ni_(63)Zr_(37) alloyribbon and affected by heating under vacuum or in air, prior to grinding or not, by means ofAES, XPS, SAM and SEM combined in situ with Ar ion bombardent. The selective oxidationand surface segregation of Zr were observed on surface layer of as-received ribbon. Highertemperature and higher oxygen pressure are beneficial to oxidation and surface segregation ofNi. Grinding pretreatment may reduce the size of Ni oxide and its precipiation temperatureon ribbon surface. Selective oxidation and surface segregation of Zr may cause the cracking ofribbon surface during oxidation.
|
|
Received: 18 February 1993
|
1 沈宁福,吴智信,孔秀兰,刘迪明,王西科.功能材料,1991;22(2) :78 2 Yamashita H, Yoshikawa M, Funabiki T, Yoshida S. J Chem Soc Faraday Trans I, 1985; 81: 2485 3 Baiker A, Gasser D, Lenzner J, Reller A, Schlogl R. J Catal, 1990; 126: 555 4 Sen P, Sarma D D, Budhani R C, Chopra K L, Rao C N R. J Phys F: Metal Phys, 1984; 14: 565 5 Wagner C D, Riggs W M, Davis L E, Moulder J F, Muilenberg G E. Handbook of X-ray Photoelectron Spectroscopy. Eden Prairie, Minnesota: Perkin-Elmer Corporation, Physical Electronic Division, 1979 6 Bertolini J C, Brissot J, Lemogne T, Montes H, Calvayrac Y, Bigot J. Appl Surf Sci, 1987; 29: 29 7 Cocke D L, Owens M S, Wright R B. Appl Surf Sci, 1988; 31: 341 8 Cocke D L, Liang G, Owens M S, Halverson D E, Naugle D G. Mater Sci Eng, 1988; 99: 497 9 Smithells C J. Metuls Reference Handbook. 5th ed, London: Butterworths, 1976 10 Koster U. Mater Sci Eng, 1988; 97: 233 11 Wise H, Oudar J. Material Concepts in Surface Reactivity and Catalysis. California: Academic, 1990: 225n |
| No Suggested Reading articles found! |
|
|