| INFLUENCE OF INTERFACE EFFECT ON ADHESION OF CHLORELLA ON TITANIUM ALLOY SURFACE |
LIAN Feng( ), REN Hongmei, GUAN Shankun, ZHANG Huichen |
| College of Transportation Equipments and Ocean Engineering, Dalian Maritime University, Dalian 116026 |
|
Cite this article:
LIAN Feng, REN Hongmei, GUAN Shankun, ZHANG Huichen. INFLUENCE OF INTERFACE EFFECT ON ADHESION OF CHLORELLA ON TITANIUM ALLOY SURFACE. Acta Metall Sin, 2014, 50(9): 1146-1152.
|
|
|
Abstract Laser etching technique was used to build three microstructures of grid, line and dot on Ti6Al4V alloy surface, and sol-gel method was used to coat SiO2 nanoparticles on the microstructure to build the hydrophobic/superhydrophobic surface with the micro/micro-nano structure. Adhesion area of the chlorella on the surfaces was used to evaluate the antifouling performance of the halobios, and dynamic wash test was used to evaluate the adhesion strength of the chlorella. It is shown that the hydrophobic/superhydrophobic surfaces with the microstructure are in accordance with Wenzel model, the superhydrophobic surfaces with the micro-nano structure are in accordance with Cassie model, and have stronger antifouling and less adhesion strength. The grid surfaces have the strongest superhydrophobic and self-cleaning performance, flowed by the line surfaces and then the dot surfaces. The contact angles decrease, the roll angles increase, the antifouling performance gets small and the adhesion strength increase with the increment of space of the microstructure.
|
|
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.51275064 and 50975036), Fundamental Research Funds for the Central Universities (No.3132014303) and Industrial Research Program of Liaoning Province (No.2012220006) |
| [1] |
Venkatesan P, Palaniswamy N, Rajagopal K. Prog Org Coat, 2006; 56: 8
|
| [2] |
Kiil S, Dam-Johansen K, Weinell C E. Biofouling, 2003; 19(suppl): 37
|
| [3] |
Alzieu C. Ecotoxicology, 2000; 9: 71
|
| [4] |
Garaventa F, Pellizzato F, Faimali M. Hydrobiologia, 2006; 22(suppl): 163
|
| [5] |
Brady R F, Singer I L. Biofouling, 2000; 15: 73
|
| [6] |
Jiang L. Chem Ind Eng Pro, 2003; 22: 1258
|
|
(江 雷. 化工进展, 2003; 22: 1258)
|
| [7] |
Papastamatiou Y P, Meyer C G. Coral Reefs, 2007; 26: 277
|
| [8] |
Chen M L, Qu Y Y, Yang L, Gao H. Sci China, 2008; 51B: 848
|
|
(陈美玲, 曲圆圆, 杨 莉, 高 宏. 中国科学, 2008; 51B: 848)
|
| [9] |
Ganesh V A, Raut H K, Nair A S. J Mater Chem, 2011; 21: 16304
|
| [10] |
Orchard M J, Kohonen M, Humphries S. J Exp Biol, 2012; 215: 279
|
| [11] |
Zheng Y, Gao X, Jiang L. Soft Mater, 2007; 3: 178
|
| [12] |
Wang J D, Chen H S, Sui T. Plant Sci, 2009; 176: 687
|
| [13] |
Scardino A J, Guenther J, de Nys R. Biofouling, 2008; 24: 45
|
| [14] |
Zhang H, Lamb R, Lewis J. Sci Technol Adv Mater, 2005; 6: 236
|
| [15] |
Bechert D W, Bruse M, Hage W. Exp Fluids, 2000; 87: 157
|
| [16] |
Chen M L, Qu Y Y, Yang L, Gao H. New Chem Mater, 2008; 36: 71
|
|
(陈美玲, 曲圆圆, 杨 莉, 高 宏. 化工新型材料, 2008; 36: 71)
|
| [17] |
Schumacher J F, Aldred N, Callow M E, Finlay J A, Callow J A, Clare A S, Brennan A B. Biofouling, 2007; 23: 307
|
| [18] |
Wang H, Dai D, Wu X D. Appl Surf Sci, 2008; 254: 5599
|
| [19] |
Guo Z G, Zhou F, Hao J C, Liu W M. J Am Chem Soc, 2005; 127: 15670
|
| [20] |
Sarkar D K, Farzaneh M, Paynter R W. Mater Lett, 2008; 62: 1226
|
| [21] |
Sarkar D K, Farzaneh M, Paynter R W. Appl Surf Sci, 2010; 256: 3698
|
| [22] |
Thieme M, Frenzel R, Schmidt S, Simon F, Hennig A, Worch H, Lunkwitz K, Scharnweber D. Adv Eng Mater, 2001; 3: 691
|
| [23] |
Dong C S, Gu Y, Zhong L L, Sezer K, Ma M X, Liu W J. J Mater Prog Technol, 2011; 211: 1234
|
| [24] |
Wenzel R N. Ind Eng Chem, 1936; 28: 988
|
| [25] |
Cassie A B D, Baxter S. Trans Faraday Soc, 1944; 40: 546
|
| [26] |
Yamamoto K, Ogata S. J Coll Inter Sci, 2008; 326: 471
|
| [27] |
Gao L C, McCarthy T J. Langmuir, 2007; 23: 3762
|
| [28] |
Wang B, Nian J Y, Tie L. Acta Phys Sin, 2013; 62: 146801
|
|
(王 奔, 念敬研, 铁 路. 物理学报, 2013; 62: 146801)
|
| [29] |
Jain A, Bhosle N B. Biofouling, 2009; 25: 13
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|