| EFFECTS OF Ca ADDITION ON THE MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Mg-5Al-0.4Zn BASED CASTING ALLOY |
| YANG Guangyu; HAO Qitang; JIE Wanqi; JIA Wenping; HE Zhi |
| College of Materials Science and Engineering; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
YANG Guangyu; HAO Qitang; JIE Wanqi; JIA Wenping; HE Zhi. EFFECTS OF Ca ADDITION ON THE MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Mg-5Al-0.4Zn BASED CASTING ALLOY. Acta Metall Sin, 2005, 41(9): 933-939 .
|
|
|
Abstract In the sand-casting magnesium alloys Mg-5Al-0.4Zn-0.2Mn-Sr-Ti-xCa , existed α-Mg, (α + Al2Ca) eutectic and Mg17Al12 when x=0.37, 0.70, 0.93, 1.69, or α-Mg and (α+(Mg, Al)2Ca) eutectic when x=2.93. With increasing x, the room temperature mechanical properties (σb, δ) of the alloys decreased, meanwhile the strength at 200 ℃ increased first and then decreased slightly, and the elongation decreased rapidly. The yield strength at 200 ℃ (σ0.2, 200 ℃) of the alloys was greatly
improved with the increase of x value. DSC analysis proved that the thermal stability of Mg17Al12 phase was improved by dissolution of Ca. The grain boundary strength at 200 ℃ was
improved through the formation of the Al2Ca or (Mg, Al)2Ca phases at the grain boundary. TEM analysis shows that the dislocations slip not only at the basal slip plane (0001), but also at the (10-10) prismatic slip plane
and (-1-121) pyramidal slip plane at 200 ℃.
The dislocation can be piled up by Al2Ca phases at the grain boundary resulting in the higher yield strength of the alloy containing Ca than those without Ca at 200 ℃.
|
|
Received: 31 January 2005
|
|
|
[1] Brulower P M. Die Cast Eng, 1997; 41: 68 [2] Polmear I J. Mater Sci Technol, 1994; 10: 1 [3] Lou A A. Int Mater Rev, 2004; 49: 13 [4] Mercer R. SAE Technol Paper Ser, 900788, 1990: 17 [5] Mordlike B L. J Mater Proc Technol, 2001; 117: 391 [6] Luo A A, Balogh M P, Powell B R. Metall Mater Trans, 2002; 33A: 567 [7] Mihriban O P, Eric B, Pierre L. J Adv Mater, 2003; 35: 32 [8] Yang G Y, Hao Q T, Jie W Q. Rare Met Mater Eng, 2005; 34: 380 (杨光昱,郝启堂,介万奇.稀有金属材料与工程, 2005;34: 380) [9] Zeng X Q, Wang Q D, Lu Y Z, Ding W J, Zhu Y P, Zhai C Q, Lu C. Mater Mech Eng, 2001; 25(5): 15 (曾小勤,王渠东,吕宜振,丁文江,朱燕萍,翟春泉,卢晨. 机械工程材料,2001;25(5):15) [10] Ninomiya R, Ojiro T, Kubota K. Acta Metall Mater, 1995; 43: 669 [11] Min X G, Sun Y S, Du W W, Xue F. J Southeast Univ, 2002; 32: 409 (闵学刚,孙扬善,杜温文,薛烽.东南大学学报,2002;32: 409) [12] [13] Hu G X, Qian M G. Metallography. Shanghai: Shanghai Science and Technology Publishers, 1980: 278 (胡赓祥,钱苗根.金属学.上海:上海科学技术出版社,1980: 278) [14] Raynor G V. The Physical Metallurgy of Magnesium and Its Alloys. Oxford: Pergamon, 1959: 103 [15] Lu S S, Gu K D, Zheng L S. Foundry and Melting of Nonferrous Alloys. Beijing: National Defence Industry Press, 1983: 82 (陆树荪,顾开道,郑来苏.有色铸造合金及熔炼.北京:国防 工业出版社,1983:82) [16] Matucha K H. Structure and Properties of Nonferrous Alloys. Vol.8, Weinheim, Germany: VCH Verlagsgesellschaft mbH, 1996: 1268 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|