Abstract The motion, microgravity level, and temperature of the Fe-66.7%Si
(atomic fraction) droplets free falling in a drop tube filled
with various inert gases under different pressures were computed.
Based on the computation, the principle of choosing the
proper inert gas and gas pressure was discussed in view
of the gravity level and the melt
cooling rate.
|
|
Received: 20 January 2005
|
|
|
[1] Tani J, Kido H. J Appl Phys, 1999; 86: 464 [2] Leong D, Harry M, Reason K J, Homewood K P. Nature, 1997; 387: 686 [3] Kubaschewski O. Iron-Binary Phase Diagram. Berlin: Springer, 1982: 138 [4] Yamauchi I, Ueyama S, Ohnaka I. Mater Sci Eng, 1996; A208: 108 [5] Yamauchi I, Nagase T, Ohnaka I. J Alloy Compd, 1999; 292: 181 [6] Yamauchi I, Okamoto T, Ohata H, Ohnaka I. J Alloy Compd, 1997; 260: 162 [7] McCoy J K, Markworth A J, Brodkey R S, Collings E W. Mater Res Soc Symp Proc, 1987; 87: 163 [8] Evans N D, Hofmeister W H, Bayuzick R J, Robinson M B. Metall Trans, 1986; 17A: 973 [9] Lacy L L, Robinson M B, Evans N D, Bayuzick R J, Rathz T J. Mater Res Soc Symp Proc, 1982; 9: 87 [10] Pan M X, Chen X C. Physics, 1988; 17: 475 (潘明祥,陈熙琛.物理, 1988;17:475) [11] Cliff R, Grace J R, Weber M E. Bubbles, Drops and Particles. New York: Academic Press, 1978: 111 [12] Brazhkin V V, Larchev V I, Popova S V, Skrotskaya G G. Phys Scr, 1989; 39: 338 [13] White F M. Viscous Fluid Flow. New York: McGrawHill, 1974: 35 |