Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (10): 475-478    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF HEATING RATE AND STRAIN RATE ON TENSILE STRENGTH OF 30CrMnSi
WANG Chunkui; HUANG Chenguang; SUN Yuanlong; DUAN Zhuping; (Institute of Mechanics; Chinese Academy of Sciences; Beijing 100080)(Manuscript received 1995-01-26; in revised form 1995-06-16)
Cite this article: 

WANG Chunkui; HUANG Chenguang; SUN Yuanlong; DUAN Zhuping; (Institute of Mechanics; Chinese Academy of Sciences; Beijing 100080)(Manuscript received 1995-01-26; in revised form 1995-06-16). INFLUENCE OF HEATING RATE AND STRAIN RATE ON TENSILE STRENGTH OF 30CrMnSi. Acta Metall Sin, 1995, 31(10): 475-478.

Download:  PDF(328KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of temperature, heating rate and strain rate on the tensile and yield strength of 30CrMnSi at the temperature range from 100℃ to 900℃ has been investigated. At low temperature region the performance parameters of material with a rise of temperature is dropped slowly and the heat treated condition has a great effect on the behavior of material, but the effect of elevating temperature rate can not be neglected. At high temperature region the material strength reduced greatly is not changed notably with the increase of temperature, heating rate and the heat treated condition. At the middle temperature region,the performance of material is fast dropped with the increase of temperature and the effects of the elevating temperature rate and the heat treated condition are not obvious.Correspondent: WANG Chunkui, associate professor,Institute of Mechanics, Chinese Academy of Sciences,Beijing ,100080
Key words:  30CrMnSi      mechanical property      heating rate      strain rate     
Received:  18 October 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I10/475

1孙承伟.强激光引起材料和结构破坏的机理分析,1991年激光的热和力学效应学术会议论文集,中国科学院上海光学精密机械研究所主编,上海嘉定,1991:12刘仓理,刘绪发,张宁,张可星,李齐民,王春彦,袁永华,桂元珍,李晓兰,李建民.CW//COIL激光热效应实验综述,1993年激光的热和力学效应学术会议论文集,国防科技大学光子对抗研究中心主编,长沙,1993:3733刘绪发.铝合金柱壳、板的8KWCWCO2激光热─力耦合破坏演示,1992年激光的热和力学效应学术会议论文集,中国工程物理研究院流体物理研究所主编,绵阳,1992:1
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[8] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[9] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[10] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[11] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[12] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[13] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[14] LI Shujun, HOU Wentao, HAO Yulin, YANG Rui. Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique[J]. 金属学报, 2023, 59(4): 478-488.
[15] WANG Hu, ZHAO Lin, PENG Yun, CAI Xiaotao, TIAN Zhiling. Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition[J]. 金属学报, 2023, 59(2): 226-236.
No Suggested Reading articles found!