Acta Metall Sin  1995, Vol. 31 Issue (10): 479-484    DOI:
Current Issue | Archive | Adv Search |
GROWTH BEHAVIOUR OF SHORT CRACK AND FATIGUE DAMAGE UNDER SPECTRUM LOADING
ZHANG Guangping; ZANG Qishan; WANG Zhongguang(State Key Laboratory for Fracture and Fatigue of Materials;Institute of Metal Research; Chinese Academy of Sciences Shenyang 110015)(Manuscript received 1994-08-06; in revised form 1995-06-09)
Cite this article: 

ZHANG Guangping; ZANG Qishan; WANG Zhongguang(State Key Laboratory for Fracture and Fatigue of Materials;Institute of Metal Research; Chinese Academy of Sciences Shenyang 110015)(Manuscript received 1994-08-06; in revised form 1995-06-09). GROWTH BEHAVIOUR OF SHORT CRACK AND FATIGUE DAMAGE UNDER SPECTRUM LOADING. Acta Metall Sin, 1995, 31(10): 479-484.

Download:  PDF(426KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Study has been carried out of the growth behaviour of short crack under spectrum loading. Meanwhile,fatigue damage and life prediction under spectrum loading have also been made.The results show that both single─edge short cracks and short cracks from notchs under spectrum loading can propagate at higher rate below the long crack growth threshold,and indicate the same growth tendency as short cracks under constant amplitude test. However, short crack growth rate under spectrum loading is slightly lower than that of constant amplitude loading. Furthermore, growth rate for long crack under spectrum loading is even lower than that of constant amplitude loading. According to the statistical approach and the constant amplitude fatigue tests, the prediction for fatigue damage under ice spectrum loading has been made, and a reasonable method for fatigue damage under ice spectrum loading has been put forward.Correspondent: ZHANG Guangping,Institute of Metal Research,Chinese Academy of Sciences, Shenyang 110015
Key words:  spectrum loading      short crack      crack growth rate      fatigue damage     
Received:  18 October 1995     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I10/479

1AllenRJ,SinclariJC,FatigueEngMaterStruct,1982;5:3432MillerKJ.FatigueEngMaterStruct,1979;1:1293EIHaddadMH,SmithKN,TopperTH.TransASME,JEngMaterTechnol,1979;101:424PetitJ,DavidsonDL,SureshS,RabbeP.FatigueCrackGrowthUnderVariableAmplitudeLoading,LondonandNewYork:ElsevierAppliedScience,19885AlawiH.TransASME,JEngMaterTechnol,1989;111:3386SureshS著,王中光等译.材料的疲劳.北京:国防工业出版社,19937SunderR.In:MitchellMR,LandgrafRW,eds.,AdvancesinFatigueLifetimePredictiveTechniques.19918ParisPC.Ph.DThesis.TheGrowthofCracksDuetoVariationsinLoad,Bethlehem:LenlghUniversity.1960
[1] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[2] Zhefeng ZHANG, Rui LIU, Zhenjun ZHANG, Yanzhong TIAN, Peng ZHANG. Exploration on the Unified Model for Fatigue Properties Prediction of Metallic Materials[J]. 金属学报, 2018, 54(11): 1693-1704.
[3] Qiliang NAI,Jianxin DONG,Maicang ZHANG,Zhihao YAO. INFLUENCE OF MULTI-MICROSTRUCTURE INTERACTION ON FATIGUE CRACK GROWTH RATE OF GH4738 ALLOY[J]. 金属学报, 2016, 52(2): 151-160.
[4] ZHANG Litao,WANG Jianqiu. STRESS CORROSION CRACK PROPAGATION BEHAVIOR OF DOMESTIC FORGED NUCLEAR GRADE 316L STAINLESS STEEL IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. 金属学报, 2013, 49(8): 911-916.
[5] YANG Bing ZHAO Yongxiang. INFLUENCE OF SURFACE ROLLING ON SHORT FATIGUE CRACK BEHAVIOR FOR LZ50 AXLE STEEL[J]. 金属学报, 2012, 48(8): 922-928.
[6] MA Yingjie LI Jinwei LEI Jiafeng TANG Zhenyun LIU Yuyin YANG Rui. INFLUENCES OF MICROSTRUCTURE ON FATIGUE CRACK PROPAGATING PATH AND CRACK GROWTH RATES IN TC4ELI ALLOY[J]. 金属学报, 2010, 46(9): 1086-1092.
[7] XIONG Ying CHEN Bingbing ZHENG Sanlong GAO Zengliang. STUDY ON FATIGUE CRACK GROWTH BEHAVIOR OF 16MnR STEEL UNDER DIFFERENT CONDITIONS[J]. 金属学报, 2009, 45(7): 849-855.
[8] ZHU Mingliang XUAN Fuzhen ZHU Kuilong WANG Guozhen JIA Tianyao. EFFECT OF HEAT TREATMENT ON FATIGUE BEHAVIOR OF 25Cr2NiMo1V STEEL[J]. 金属学报, 2009, 45(3): 320-325.
[9] ZHANG Jiwang LU Liantao SHEN Xunliang YI Hongfei ZHANG Weihua. EVALUATION METHOD OF FATIGUE DAMAGE UNDER VARIABLE AMPLITUDE STRESS BASED ON PLASTIC STRAIN[J]. 金属学报, 2009, 45(12): 1461-1465.
[10] LU Liantao LI Wei ZHANG Jiwang SHIOZAWA Kazuaki ZHANG Weihua. ANALYSIS OF ROTARY BENDING GIGACYCLE FATIGUE PROPERTIES OF BEARING STEEL GCr15[J]. 金属学报, 2009, 45(1): 73-78.
[11] ZHANG Guangping; TAKASHIMA Kazuki; HIGO Yakichi. Size Effects On Deformation And Fatigue Behavior Of A Micron-Sized Stainless Steel[J]. 金属学报, 2005, 41(4): 337-341 .
[12] ZHANG Guangping; WANG Zhongguang. Progress in Fatigue of Small Dimensional Materials[J]. 金属学报, 2005, 41(1): 1-8 .
[13] CHEN Wenzhe;ZHANG Sa;QIAN Kuangwu (Department of Materials; Fuzhou University; Fuzhou 350002)GU Haicheng (Institute of Materials; Xi'an Jiaotong University; Xi'an 710049)WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). FATIGUE CRACK GROWTH RATES AND FATIGUE THRESHOLDS OF CENTRIFUGAL SPRAY DEPOSITED Ti-48Al-2Mn-2Nb[J]. 金属学报, 1998, 34(1): 70-74.
[14] DING Chuanfu;YU Hui; WU Xueren (Beijing Institute of Aeronautical Materials;Beijing 100095). GROWTH BEHAVIOUR OF SMALL FATIGUE CRACK AND FATIGUE-LIFE PREDICTION FOR HIGH-STRENGTH STEEL 30CrMnSiNi2A[J]. 金属学报, 1997, 33(3): 277-286.
[15] WANG Mingzhang; LIN Shi; LI Jinxu; GUAN Jingjiao; XIAO Jimei (University of Science and Technology Beijing; Beijing 100083). FATIGUE DAMAGE AND CRACK INITIATION IN [112] ALUMINUM SINGLE CRYSTAL[J]. 金属学报, 1997, 33(10): 1015-1020.
No Suggested Reading articles found!