| 应变速率对奥氏体不锈钢应变诱发α'--马氏体转变和力学行为的影响 |
| 刘伟1;李志斌2;王翔3;邹骅1;王立新2 |
1 北京交通大学机械与电子控制工程学院; 北京 100044
2 太原钢铁(集团)有限公司; 太原 030003
3 Department of Materials Science and Engineering; McMaster University; Hamilton; ON.; L8S 4L7; Canada |
|
| EFFECT OF STRAIN RATE ON STRAIN INDUCED α'--MARTENSITE TRANSFORMATION AND MECHANICAL RESPONSE OF AUSTENITIC STAINLESS STEELS |
| LIU Wei 1;LI Zhibin2; WANG Xiang3;ZOU Hua1;WANG Lixin2 |
1 School of Mechanical; Electronic and Control Engineering; Beijing Jiaotong University; Beijing 100044
2 Taiyuan Iron and Steel (Group) Co.; Taiyuan 030003
3 Department of Materials Science and Engineering; McMaster University; Hamilton; ON.; L8S 4L7; Canada |
引用本文:
刘伟 李志斌 王翔 邹骅 王立新. 应变速率对奥氏体不锈钢应变诱发α'--马氏体转变和力学行为的影响[J]. 金属学报, 2009, 45(3): 285-291.
.
EFFECT OF STRAIN RATE ON STRAIN INDUCED α'--MARTENSITE TRANSFORMATION AND MECHANICAL RESPONSE OF AUSTENITIC STAINLESS STEELS[J]. Acta Metall Sin, 2009, 45(3): 285-291.
| [1] Lichtenfeld J A, Mataya M C, Tyne C J V. Metall Mater Trans, 2006; 37A: 147
[2] Talonen J, Nenonen P, Pape G, Hanninen H. Metall Mater Trans, 2005; 36A: 421
[3] Kumar A, Singha L K. Metall Mater Trans, 1989; 20A: 2857
[4] Talonen J, Hanninen H. Acta Mater, 2007; 55: 6108
[5] Byun T S, Hashimoto N, Farrell K. Acta Mater, 2004; 52: 3889
[6] Angel T. J Iron Steel Inst, 1954; 177: 165
[7] Nohara K, Ono Y, Ohasi N. J Iron Steel Inst, 1977; 63: 772
[8] Schramm R E, Reed R P. Metall Trans, 1975; 6A: 1345
[9] Liu W , Li Q, Jiao D Z, Zheng Y, Li G P. Acta Metall Sin, 2008; 44: 775
(刘伟, 李强, 焦德志, 郑毅, 李国平. 金属学报, 2008; 44: 775)
[10] Zhang H W, Hei Z K, Liu G, Lu J, Lu K. Acta Mater, 2003; 51: 1871
[11] Lee W S, Lin C F. Metall Mater Trans, 2002; 35A: 2801
[12] Byun T S. Acta Mater, 2003; 51: 3063
[13] Spencer K. PhD Thesis, McMaster University, Ontario, 2002
[14] Ferreira P J, Sande J B V, Amaral M. Metall Mater Trans, 2004; 35A: 3091
[15] Sinclair C W, Embury J D, Weatherly G C. Mater Sci Eng, 1999; A272: 90
[16] Han H N, Lee C G, Oh C S, Lee T H, Kim S J. Acta Mater, 2004; 52: 5203
[17] Olson G B, Cohen M. Metall Trans, 1982; 13A: 1907
[18] Olson G B, Azrin M. Metall Trans, 1978; 9A: 731
[19] Sinclair C W, Hoagland R G. Acta Mater, 2008; 56: 4160
[20] De A K, Speer J G, Matlock D K, Murdock D C, Mataya M C, Comstock R J. Metall Mater Trans, 2006; 37A: 1875
[21] Das A, Sivaprasad S, Ghosh M, Chakraborti P C, Tarafder S. Mater Sci Eng, 2008; A486: 283 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|