| TiN含量对Ti(C, N)/NiCr金属陶瓷微观结构和力学性能的影响 |
| 王全兆; 刘 越; 关德慧; 于宝海; 陈志亮;毕 敬 |
| 中国科学院金属研究所 |
|
| Effect of tin content on microstructures and mechanical properties of Ti(C,N)/NiCr cermets |
| WANG Quanzhao; LIU Yue; GUAN Dehui;YU Baohai; CHEN Zhiliang; BI Jing |
| Institute of Metal Research; The Chinese Academy of Sciences |
引用本文:
王全兆; 刘越; 关德慧; 于宝海; 陈志亮; 毕敬 . TiN含量对Ti(C, N)/NiCr金属陶瓷微观结构和力学性能的影响[J]. 金属学报, 2005, 41(11): 1121-1126 .
,
,
,
,
,
.
Effect of tin content on microstructures and mechanical properties of Ti(C,N)/NiCr cermets[J]. Acta Metall Sin, 2005, 41(11): 1121-1126 .
[1] Ettmayer P, Lengauer W. Powder Metall Int, 1989; 21(2): 37 [2] Ettmayer P, Kolaska H. Metall, 1989; 43: 742 [3] Ettmayer P, Kolaska H, Legnauer W, Dreyer K. Int J Refract Met Hard Mater, 1995; 13: 343 [4] Qian Z L, Xiong W H. Mater Rev, 1996; (5): 8 (钱中良,熊惟皓.材料导报,1996;(5):8) [5] Guan D H, Yu B H, Bi J. Powder Metall Technol, 1998; 16(1): 36 (关德慧,于宝海,毕敬.粉末冶金技术,1998;16(1):36) [6] Zhang S. Key Eng Mater, 1998; 521: 138 [7] Zhu L J, Tang M, Yu B H, Liu Y, Tian Y W. J Mater Eng, 2001; 10: 6 (朱丽娟,唐猛,于宝海,刘越,田彦文.材料工程,2001; 10:6) [8] Liu Y, Yu B H, Guan D H, Wang Z B, Bi J. J Mater Sci Lett, 2001; 20: 619 [9] Iyori. US Pat No.4,983,212, 1991 [10] Zhang W, Jiang Y. flare Met Cem Carbide, 1997; 55: 129 (张伟,蒋勇.稀有金属与硬质合金, 1997;55:129) [11] Liu N, Xu Y D, Li H, Li G H, Zhang L D. J Euro Ceramic Soc, 2002; 22: 2409 [12] Jung J, Kang S. Powder Metall, 2002; 45: 83 [13] Wang Q Z, Liu Y, Chen Z L, Bi J. Chin J Mater Res, 2005; 19: 354 (王全兆,刘越,陈志亮,毕敬.材料研究学报,2005;19: 354) [14] Li C H, Yu L X, Xiong W H. Acta Mater Compos Sin, 2003; 20: 1 (李晨辉,余立新,熊惟皓.复合材料学报,2003;20:1) [15] Jung I J, Kang S. J Mater Sci, 2000; 35: 87 |
|