| 低碳钢在Ae3温度之上的形变诱导铁素体(一种马氏体)的相变研究 |
| 刘朝霞; 李殿中; 乔桂文 |
| 中国科学院金属研究所 |
|
| Investigation on deformation induced ferrite (a kind of martensite) transformation above Ae3 temperature in a low carbon steel |
| LIU Zhaoxia; LI Dianzhong; QIAO Guiwen |
| Institute of Metal Research; The Chinese Academy of Sciences |
引用本文:
刘朝霞; 李殿中; 乔桂文 . 低碳钢在Ae3温度之上的形变诱导铁素体(一种马氏体)的相变研究[J]. 金属学报, 2005, 41(11): 1127-1135 .
,
,
.
Investigation on deformation induced ferrite (a kind of martensite) transformation above Ae3 temperature in a low carbon steel[J]. Acta Metall Sin, 2005, 41(11): 1127-1135 .
[1] Priestner R, Hodgson P D. Mater Sci Technol, 1992; 8: 849 [2] Huang Y D, Yang W Y, Sun Z Q. J Mater Proc Technol, 2003; 134: 19 [3] Hodgson P D, Hickson M R, Gibbs R K. Scr Mater, 1999; 40: 1179 [4] Hurley P J, Hodgson P D, Muddle B C. Scr Mater, 1999; 40: 433 [5] Hurley P J, Hodgson P D. Mater Sci Technol, 2001; 17: 1360 [6] Hickson M R , Hodgson P D. Mater Sci Technol, 1999; 15: 85 [7] Yang P, Fu Y Y, Cui F E, Sun Z Q. Ada Metall Sin, 2001; 37: 900 (杨平,傅云义,崔凤娥,孙祖庆.金属学报,2001;37:900) [8] Qi J J, Yang W Y, Sun Z Q. Acta Metall Sin, 2002; 38: 629 (齐俊杰,杨王玥,孙祖庆.金属学报, 2002;38:629) [9] Hickson M R , Gibbs R K, Hodgson P D. ISIJ Int, 1999;39:1176 [10] Yada H, Matsumura Y. Trans Iron Steel Inst Jpn, 1987;27:492 [11] Matsumura Y, Yada H. Metall Soc Technol Paper, 1986;A86-28:1 [12] Yada H, Li C M, Yamagata H. ISIJ Int, 2000; 40: 200 [13] Mintz B, Lewis J, Jonas J J. Mater Sci Technol, 1997; 13:379 [14] Hurley P J, Hodgson P D. Mater Sci Eng, 2001; 302A:206 [15] Bleck W, Herzig C, Lorenz U. Mater Technol, 2001; 72:406 [16] Yang Z M, Wang R Z. ISIJ Int, 2003; 43: 761 [17] Tong M M, Ni J, Zhang Y T, Li D Z, Li Y Y. Scr Mater,2004; 50: 909 [18] Priestner R, Al-Horr Y M, Ibraheem A K. Mater Sci Technol, 2002; 18: 973 [19] Yang Z M, Zhao Y, Wang R Z, MA Y W, Che Y M. Acta Metall Sin, 2000; 36: 818 (杨忠民,赵燕,王瑞珍,马燕文,车彦民.金属学报,2000; 36:818) [20] Yang Z M, Zhao Y, Wang R Z, Ma Y W, Che Y M, Chen Q A. Acta Metall Sin, 2000; 36: 1061 (杨忠民,赵燕,王瑞珍,马燕文,车彦民,陈其安.金属学 报,2000;36:1061) [21] Liu Z X, Tong M M, Huang C J, Li D Z. Acta Metall Sin, 2004; 40: 930 (刘朝霞,佟铭明,黄成江,李殿中.金属学报,2004;40:930) [22] Li W J, Du L X, Zhang H M, Liu X H, Wang G D. J Iron Steel Res, 2000; 12: 36 (李维娟,杜林秀,张红梅,刘相华,王国栋.钢铁研究学报, 2000;12:36) [23] Amin R K, Pickering F B. Thermomechanical processing of microalloyed austenite , Warrendale, PA: TMS, 1982: 377 [24] Dube A, Aranson H I, Mehl R F. Rev Met, 1958; 55: 201 [25] Massalski T B. Acta Metall, 1958; 6: 243 [26] Xu Z Y. Heat Treatment, 2003; 18: 1 (徐祖耀.热处理,2003;18:1) |
|