| 5356铝合金TIG电弧增材制造组织与力学性能 |
孙佳孝1, 杨可1( ), 王秋雨1, 季珊林1, 包晔峰1, 潘杰2 |
1.河海大学 机电工程学院 常州 213022 2.中国科学院金属研究所 沈阳材料科学国家研究中心 沈阳 110016 |
|
| Microstructure and Mechanical Properties of 5356 Aluminum Alloy Fabricated by TIG Arc Additive Manufacturing |
SUN Jiaxiao1, YANG Ke1( ), WANG Qiuyu1, JI Shanlin1, BAO Yefeng1, PAN Jie2 |
1.College of Mechanical and Electronic Engineering, Hohai University, Changzhou 213022, China 2.Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
孙佳孝, 杨可, 王秋雨, 季珊林, 包晔峰, 潘杰. 5356铝合金TIG电弧增材制造组织与力学性能[J]. 金属学报, 2021, 57(5): 665-674.
Jiaxiao SUN,
Ke YANG,
Qiuyu WANG,
Shanlin JI,
Yefeng BAO,
Jie PAN.
Microstructure and Mechanical Properties of 5356 Aluminum Alloy Fabricated by TIG Arc Additive Manufacturing[J]. Acta Metall Sin, 2021, 57(5): 665-674.
| 1 |
Li Q, Wang F D, Wang G Q, et al. Wire and arc additive manufacturing of lightweight metal components in aeronautics and astronautics [J]. Aeronaut. Manuf. Technol., 2018, 61(3): 74
|
| 1 |
李 权, 王福德, 王国庆等. 航空航天轻质金属材料电弧熔丝增材制造技术 [J]. 航空制造技术, 2018, 61(3): 74
|
| 2 |
Wang T T, Zhang Y B, Xie Y L. Status and development prospects of the wire arc additive manufacture technology [J]. Elect. Weld. Mach., 2017, 47(8): 60
|
| 2 |
王庭庭, 张元彬, 谢岳良. 丝材电弧增材制造技术研究现状及展望 [J]. 电焊机, 2017, 47(8): 60
|
| 3 |
Nie D J, Luo M Q, Chen W S, et al. Review of research progress of aluminum alloys for transportation [J]. Nonferrous Met. Process., 2016, 45(5): 15
|
| 3 |
聂德键, 罗铭强, 陈文泗等. 交通运输用铝合金材料研究进展 [J]. 有色金属加工, 2016, 45(5): 15
|
| 4 |
Zhang X M, Deng Y L, Zhang Y. Development of high strength aluminum alloys and processing techniques for the materials [J]. Acta Metall. Sin., 2015, 51: 257
|
| 4 |
张新明, 邓运来, 张 勇. 高强铝合金的发展及其材料的制备加工技术 [J]. 金属学报, 2015, 51: 257
|
| 5 |
Zhou D W, Peng Y, Xu S H, et al. Microstructure and mechanical property of steel/Al alloy laser welding with Sn powder addition [J]. Acta Metall. Sin., 2013, 49: 959
|
| 5 |
周惦武, 彭 艳, 徐少华等. 添加Sn粉激光焊接钢/铝合金异种金属的显微组织与性能 [J]. 金属学报, 2013, 49: 959
|
| 6 |
Pan F, Cui L, Qian W, et al. Microstructures and mechanical properties of dual-beam laser keyhole welded joints of aluminum alloys to stainless steels [J]. Acta Metall. Sin., 2016, 52: 1388
|
| 6 |
潘 峰, 崔 丽, 钱 伟等. 铝合金/不锈钢双光束激光深熔焊接接头组织及力学性能 [J]. 金属学报, 2016, 52: 1388
|
| 7 |
Jin P, Sui R, Li F X, et al. Reactive wetting of TC4 titanium alloy by molten 6061 Al and 4043 Al alloys [J]. Acta Metall. Sin., 2017, 53: 479
|
| 7 |
靳 鹏, 隋 然, 李富祥等. 熔融6061/4043铝合金在TC4钛合金表面的反应润湿 [J]. 金属学报, 2017, 53: 479
|
| 8 |
Chen L, Zhao G Q, Gong J, et al. Hot deformation behaviors and processing maps of 2024 aluminum alloy in as-cast and homogenized states [J]. J. Mater. Eng. Perform., 2015, 24: 5002
|
| 9 |
Liu Z L, Cui H T, Ji S D, et al. Improving joint features and mechanical properties of pinless fiction stir welding of alcald 2A12-T4 aluminum alloy [J]. J. Mater. Sci. Technol., 2016, 32: 1372
|
| 10 |
Bai J Y, Fan C L, Yang Y C, et al. Microstructures of 2219-Al thin-walled parts produced by shaped metal deposition [J]. Trans. China Weld. Inst., 2016, 37(6): 124
|
| 10 |
柏久阳, 范成磊, 杨雨晨等. 2219铝合金TIG填丝堆焊成形薄壁试样组织特征 [J]. 焊接学报, 2016, 37(6): 124
|
| 11 |
Liu Y B, Sun Q J, Jiang Y L, et al. Rapid prototyping process based on cold metal transfer arc welding technology [J]. Trans. China Weld. Inst., 2014, 35(7): 1
|
| 11 |
刘一搏, 孙清洁, 姜云禄等. 基于冷金属过渡技术快速成形工艺 [J]. 焊接学报, 2014, 35(7): 1
|
| 12 |
Gu J l, Ding J L, Williams S W, et al. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys [J]. J. Mater. Process. Technol., 2016, 230: 26
|
| 13 |
Colegrove P A, Donoghue J, Martina F, et al. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components [J]. Scr. Mater., 2017, 135: 111
|
| 14 |
Wang H, Kovacevic R. Rapid prototyping based on variable polarity gas tungsten arc welding for a 5356 aluminium alloy [J]. Proc. Inst. Mech. Eng., 2001, 215B: 1519
|
| 15 |
Ouyang J H, Wang H, Kovacevic R. Rapid prototyping of 5356-aluminum alloy based on variable polarity gas tungsten arc welding: Process control and microstructure [J]. Mater. Manuf. Process., 2002, 17: 103
|
| 16 |
Sun C S, Zhang Z D, Liu L M. Microstructure and mechanical properties of 5356 aluminum alloy thin wall parts manufactured by laser induced MIG arc additive [J]. Weld. Technol., 2017, 46(5): 47
|
| 16 |
孙承帅, 张兆栋, 刘黎明. 激光诱导MIG电弧增材制造5356铝合金薄壁零件组织及力学性能 [J]. 焊接技术, 2017, 46(5): 47
|
| 17 |
Zhang C, Gao M, Zeng X Y. Workpiece vibration augmented wire arc additive manufacturing of high strength aluminum alloy [J]. J. Mater. Process. Technol., 2019, 271: 85
|
| 18 |
Long Q, Lu F H, Zhang Y L, et al. Present research status and new development of the welding technologies of Mg/Al dissimilar metals [J]. Light Met., 2018, (2): 47
|
| 18 |
龙 琼, 路坊海, 张玉兰等. Mg/Al异种金属焊接技术的研究现状及最新进展 [J]. 轻金属, 2018, (2): 47
|
| 19 |
Dai Q S, Ou S S, Deng Y L, et al. Microstructure evolution and grain size model of 5083 aluminum alloy during hot deformation [J]. Mater. Rev., 2017, 31(14): 143
|
| 19 |
戴青松, 欧世声, 邓运来等. 5083铝合金的热变形组织演变及晶粒度模型 [J]. 材料导报, 2017, 31(14): 143
|
| 20 |
Liang Y, Shen J Q, Hu S S, et al. Effect of TIG current on microstructural and mechanical properties of 6061-T6 aluminium alloy joints by TIG-CMT hybrid welding [J]. J. Mater. Process. Technol., 2018, 255: 161
|
| 21 |
Dubyna A, Mogucheva A, Kaibyshev R. Hall-Petch relationship in an Al-Mg-Sc alloy subjected to ECAP [J]. Adv. Mater. Res., 2014, 922: 120
|
| 22 |
Humphreys F J, Prangnell P B, Priestner R. Fine-grained alloys by thermomechanical processing [J]. Curr. Opin. Solid State Mater. Sci., 2001, 5: 15
|
| 23 |
Horgar A, Fostervoll H, Nyhus B, et al. Additive manufacturing using WAAM with AA5183 wire [J]. J. Mater. Process. Technol., 2018, 259: 68
|
| 24 |
Sha G, Marceau R K W, Gao X, et al. Nanostructure of aluminium alloy 2024: Segregation, clustering and precipitation processes [J]. Acta Mater., 2011, 59: 1659
|
| 25 |
Pang Y G, Wang Z T. Application of Al and Al alloys in high-tech and new weapons [J]. Light Alloy Fab. Technol., 2018, 46(6): 1
|
| 25 |
庞彦国, 王祝堂. 铝及铝合金在高新兵器中的应用 [J]. 轻合金加工技术, 2018, 46(6): 1
|
| 26 |
Gu J L, Wang X S, Bai J, et al. Deformation microstructures and strengthening mechanisms for the wire+arc additively manufactured Al-Mg4.5Mn alloy with inter-layer rolling [J]. Mater. Sci. Eng., 2018, A712: 292
|
| 27 |
Boeira A P, Ferreira I L, Garcia A. Alloy composition and metal/mold heat transfer efficiency affecting inverse segregation and porosity of as-cast Al-Cu alloys [J]. Mater. Des., 2009, 30: 2090
|
| 28 |
Gu J L, Ding J L, Williams S W, et al. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys [J]. J. Mater. Process. Technol., 2016, 230: 26
|
| 29 |
Cong B Q, Ding J L, Williams S. Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy [J]. Int. J. Adv. Manuf. Technol., 2015, 76: 1593
|
| 30 |
Bai J Y, Yang C L, Lin S B, et al. Mechanical properties of 2219-Al components produced by additive manufacturing with TIG [J]. Int. J. Adv. Manuf. Technol., 2016, 86: 479
|
| 31 |
Liu P W, Wang Z, Xiao Y H, et al. Insight into the mechanisms of columnar to equiaxed grain transition during metallic additive manufacturing [J]. Add. Manuf., 2019, 26: 22
|
| 32 |
Bermingham M J, StJohn D H, Krynen J, et al. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing [J]. Acta Mater., 2019, 168: 261
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|