| 时效对Ti-50.8Ni-0.1Zr形状记忆合金显微组织、拉伸性能和记忆行为的影响 |
叶俊杰, 贺志荣( ), 张坤刚, 杜雨青 |
| 陕西理工大学 材料科学与工程学院 汉中 723001 |
|
| Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy |
YE Junjie, HE Zhirong( ), ZHANG Kungang, DU Yuqing |
| School of Materials Science and Engineering, Shaanxi University of Technology, Hanzhong 723001, China |
引用本文:
叶俊杰, 贺志荣, 张坤刚, 杜雨青. 时效对Ti-50.8Ni-0.1Zr形状记忆合金显微组织、拉伸性能和记忆行为的影响[J]. 金属学报, 2021, 57(6): 717-724.
Junjie YE,
Zhirong HE,
Kungang ZHANG,
Yuqing DU.
Effect of Ageing on Microsturcture, Tensile Properties, and Shape Memory Behaviors of Ti-50.8Ni-0.1Zr Shape Memory Alloy[J]. Acta Metall Sin, 2021, 57(6): 717-724.
| 1 |
Jin M J, Song Y W, Wang X D, et al. Ultrahigh damping capacity achieved by modulating R phase in Ti49.2Ni50.8 shape memory alloy wires [J]. Scr. Mater., 2020, 183: 102
|
| 2 |
Zheng Y, Dong Y, Li Y H. Resilience and life-cycle performance of smart bridges with shape memory alloy (SMA)-cable-based bearings [J]. Constr. Build. Mater., 2018, 158: 389
|
| 3 |
Azadpour F, Maghsoudi A A. Experimental and analytical investigation of continuous RC beams strengthened by SMA strands under cyclic loading [J]. Constr. Build. Mater., 2020, 239: 117730
|
| 4 |
Jani J M, Leary M, Subic A, et al. A review of shape memory alloy research, applications and opportunities [J]. Mater. Des., 2014, 56: 1078
|
| 5 |
Soother D K, Daudpoto J, Chowdhry B S. Challenges for practical applications of shape memory alloy actuators [J]. Mater. Res. Express, 2020, 7: 073001
|
| 6 |
Sun L, Huang W M, Ding Z, et al. Stimulus-responsive shape memory materials: A review [J]. Mater. Des., 2012, 33: 577
|
| 7 |
Shariat B S, Meng Q L, Mahmud A S, et al. Functionally graded shape memory alloys: Design, fabrication and experimental evaluation [J]. Mater. Des., 2017, 124: 225
|
| 8 |
He Z R, Zhou J E, Miyazaki S. Relationship between transformation behaviors and Ni content in solution-aged Ti-Ni alloys [J]. Acta Metall. Sin., 2003, 39: 617
|
| 8 |
贺志荣, 周敬恩, 宫崎修一. 固溶时效态Ti-Ni合金相变行为与Ni含量的关系 [J]. 金属学报, 2003, 39: 617
|
| 9 |
He Z R, Wang F, Wang Y S, et al. Effects of V and Cr on transformation and deformation characteristics of Ti-Ni superelastic alloy [J]. Acta Metall. Sin., 2007, 43: 1293
|
| 9 |
贺志荣, 王 芳, 王永善等. V和Cr对Ti-Ni超弹性合金相变和形变特性的影响 [J]. 金属学报, 2007, 43: 1293
|
| 10 |
Bozzolo G, Noebe R D, Mosca H O. Site preference of ternary alloying additions to NiTi: Fe, Pt, Pd, Au, Al, Cu, Zr and Hf [J]. J. Alloys Compd., 2005, 389: 80
|
| 11 |
Yuan Z S, Lin D Z, Cui Y, et al. Research progress on the phase transformation behavior, microstructure and property of NiTi based high temperature shape memory alloys [J]. Rare Met. Mater. Eng., 2018, 47: 2269
|
| 11 |
袁志山, 吝德智, 崔 跃等. NiTi基高温记忆合金相变行为与组织性能研究进展 [J]. 稀有金属材料与工程, 2018, 47: 2269
|
| 12 |
He Z R, Wang F, Zhou J E. Effect of Ni content and heat treatment on phase transformation and deformation behavior of Ti-Ni shape memory alloys [J]. Heat Treat. Met, 2006, 31(9): 17
|
| 12 |
贺志荣, 王 芳, 周敬恩. Ni含量和热处理对Ti-Ni形状记忆合金相变和形变行为的影响 [J]. 金属热处理, 2006, 31(9): 17
|
| 13 |
Wang H Z. Microstructure and strain recovery characteristic of proton irradiated NiTi alloys [D]. Harbin: Harbin Institute of Technology, 2019
|
| 13 |
王海振. 质子辐照NiTi合金的微观组织结构与应变恢复特性 [D]. 哈尔滨: 哈尔滨工业大学, 2019
|
| 14 |
Frenzel J, George E P, Dlouhy A, et al. Influence of Ni on martensitic phase transformations in NiTi shape memory alloys [J]. Acta Mater., 2010, 58: 3444
|
| 15 |
Tong Y X, Liu J T, Chen F, et al. Effect of aging on martensitic transformation and superelasticity of TiNiCr shape memory alloy [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2598
|
| 16 |
He Z R, Wang F. Effect of heat treatment on transformation behavior of low-temperature superelasticity alloy Ti-50.8Ni-0.3Cr [J]. Acta Metall. Sin., 2010, 46: 329
|
| 16 |
贺志荣, 王 芳. 热处理对Ti-Ni-Cr低温超弹性合金相变行为的影响 [J]. 金属学报, 2010, 46: 329
|
| 17 |
Feng Z W, Qian D F, Gao B D, et al. Research on properties of TiNiZr shape memory alloys [J]. Chin. J. Rare Met., 2001, 25: 47
|
| 17 |
冯昭伟, 千东范, 高宝东等. TiNiZr形状记忆合金的性能研究 [J]. 稀有金属, 2001, 25: 47
|
| 18 |
Feng Z W, Cui Y, Shang Z Y, et al. Development of NiTiZr high temperature shape memory alloys [J]. Mater. Rev., 2016, 30: 616
|
| 18 |
冯昭伟, 崔 跃, 尚再艳等. 镍钛锆高温形状记忆合金的研究进展 [J]. 材料导报, 2016, 30: 616
|
| 19 |
Yi X Y, Wang H Z, Sun B, et al. The crystallization process, microstructure, martensitic transformation and mechanical properties of Ti-Ni-Zr alloy ribbons [J]. J. Alloys Compd., 2019, 778: 542
|
| 20 |
Li Q Q, Ma Y H, Li Y. Microstructure, phase transformation and shape memory properties of Ni-Ti-Zr alloys [J]. Foundry, 2019, 68: 1204
|
| 20 |
李启泉, 马悦辉, 李 岩. Ni-Ti-Zr合金组织、相变与形状记忆性能 [J]. 铸造, 2019, 68: 1204
|
| 21 |
Malykhin S V, Kondratenko V V, АKopylets I, et al. Structure and phase formation features of Ti-Zr-Ni quasicrystalline films under heating [J]. J. Nano-Electron. Phys., 2019, 11: 03009
|
| 22 |
Atli K C. The effect of tensile deformation on the damping capacity of NiTi shape memory alloy [J]. J. Alloys Compd., 2016, 679: 260
|
| 23 |
Yi X Y, Gao W H, Wang H Z, et al. Dependence of aging parameters on precipitation behavior, martensitic transformation and mechanical properties of the aged Ni-Ti alloy under super high pressure [J]. Mater. Sci. Eng., 2018, A736: 354
|
| 24 |
Holec D, Bojda O, Dlouhý A. Ni4Ti3 precipitate structures in Ni-rich NiTi shape memory alloys [J]. Mater. Sci. Eng., 2006, A481-482: 462
|
| 25 |
Santamarta R, Arróyave R, Pons J, et al. TEM study of structural and microstructural characteristics of a precipitate phase in Ni-rich Ni-Ti-Hf and Ni-Ti-Zr shape memory alloys [J]. Acta Mater., 2013, 61: 6191
|
| 26 |
Wang Q, He Z R, Shao D W. Effects of Solution annealing and aging on tensile property and microstructure of Ti-Ni-Cr shape memory alloy [J]. Rare Met. Mater. Eng., 2012, 41: 1191
|
| 26 |
王 启, 贺志荣, 邵大伟. 固溶-时效处理对Ti-Ni-Cr形状记忆合金拉伸性能和显微组织的影响 [J]. 稀有金属材料与工程, 2012, 41: 1191
|
| 27 |
Sandu A M, Tsuchiya K, Tabuchi M, et al. Microstructural evolution during isothermal aging in Ni-Rich Ti-Zr-Ni shape memory alloys [J]. Mater. Trans., 2007, 48: 432
|
| 28 |
Sandu A, Tsuchiya K, Yamamoto S, et al. Effect of aging on microstructure and martensitic transformation in Ti-Zr-Ni shape memory alloys [J]. Mater. Sci. Forum, 2007, 539-543: 3163
|
| 29 |
Chang B C, Shaw J A, Iadicola M A. Thermodynamics of shape memory alloy wire: Modeling, experiments, and application [J]. Continuum Mech. Thermodyn., 2006, 18: 83
|
| 30 |
Chumlyakov Y I, Kireeva I V, Karaman I, et al. Orientational dependence of shape memory effects and superelasticity in CoNiGa, NiMnGa, CoNiAl, FeNiCoTi, and TiNi single crystals [J]. Russ. Phys. J., 2004, 47: 893
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|