金属学报  2019, Vol. 55 Issue (12): 1487-1494    DOI: 10.11900/0412.1961.2019.00147
  研究论文 本期目录 | 过刊浏览 |
Ce微合金化H13钢中一次碳化物的析出机理及热稳定性研究
黄宇,成国光(),李世健,代卫星
北京科技大学钢铁冶金新技术国家重点实验室 北京 100083
Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel
HUANG Yu,CHENG Guoguang(),LI Shijian,DAI Weixing
State Key laboratory of Advanced Metallurgy, University of Science and Technology Beijing, Beijing 100083, China
引用本文:

黄宇, 成国光, 李世健, 代卫星. Ce微合金化H13钢中一次碳化物的析出机理及热稳定性研究[J]. 金属学报, 2019, 55(12): 1487-1494.
HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. Acta Metall Sin, 2019, 55(12): 1487-1494.

全文: PDF(19895 KB)   HTML
摘要: 

系统研究了Ce微合金化H13热作模具钢中一次碳化物的析出机理及热稳定性。首先通过SEM以及夹杂物自动分析系统观察Ce微合金化H13钢中夹杂物的二维形貌、类型、数量及尺寸;进一步利用非水溶液电解法观察Ce微合金化H13钢中一次碳化物的三维形貌;随后在不同的加热温度下保温1 h研究一次碳化物的热稳定性;最后利用Factsage 7.2热力学软件计算一次碳化物的析出机理以及热稳定性。结果表明:Ce能够有效地与钢液中的O、S、P、As元素反应生成对应的夹杂物;一次碳化物的二维形貌为长条状而三维形貌为片状,两者之间差别较大;富Ti、V碳化物首先析出,随后作为富V碳化物的形核核心促进其析出,一次碳化物的三维尺寸达到50 μm;富Ti、V碳化物的热稳定性明显高于富V碳化物,当加热温度达到1250 ℃时,富Ti、V碳化物刚开始溶解但依然存在,而富V碳化物已经完全溶解;经过加热处理后,一次碳化物的三维平均尺寸降低到10 μm左右;Factsage 7.2的理论计算结果与实际观察结果基本一致。较高的加热温度可以一定程度上降低Ce微合金化H13钢中一次碳化物的危害,但不能完全去除。

关键词 : H13钢,  稀土,  一次碳化物,  热稳定性,  析出机理    
Abstract:

Ce microalloyed H13 hot die steel is widely used in manufacturing hot extrusion and die casting mold of magnesium-aluminium alloy because of its excellent combination of hot strength and impact toughness. The C content in Ce microalloyed H13 steel is approximately 4% (mass fraction), and the alloy elements content such as Cr, Mo, V et al are about 8%. Therefore, it is easy for primary carbide to precipitate during the solidification of the molten steel due to the segregation of alloy elements. Most researchers study the precipitation mechanism of primary carbide in the two-dimensional perspective. A few people are involved in the three-dimensional morphology of the primary carbide, especially the thermal stability of the primary carbide in the three-dimensional perspective in the Ce microalloyed H13 steel. Therefore, the precipitation mechanism and thermal stability of the primary carbide were systematically studied in this work. First, the SEM and inclusion automatic analysis system were used to analyze the morphology, number density and size of the inclusions in Ce microalloyed H13 steel. The three-dimensional morphology of the primary carbide in sample was observed after electrolyzed in a non-aqueous solution. The voltage was 20 V, the electrolysis time was about 3 min and the electrolyte was composed of 1% tetramethylammonium chloride, 10% acetylacetone, and 89% methanol (volume fraction). Three samples were heated to 1150, 1200 and 1250 ℃ for 1 h to investigate the thermal stability of the primary carbide. Finally, Factsage 7.2 software was used to calculate the precipitation mechanism and thermal stability of the primary carbide. Elemental Ce can effectively react with O, S, P and As elements to form the corresponding Ce-O, Ce-S and Ce-P-As inclusions. There is a huge difference between the two-dimensional and three-dimensional morphologies of the primary carbide, the two-dimensional morphology is strip and the three-dimensional morphology is irregular flake. Ti-V-rich carbide precipitates first, and then acts as the nucleation core of V-rich carbide. When the heating temperature reaches 1250 ℃, the V-rich carbide has completely dissolved, and the Ti-V-rich carbide begins to dissolve. The three-dimensional morphology of the wrapped Ti-V-rich carbide is completely exposed after the V-rich carbide disappears completely. The Ce-O inclusion is formed before solidification, and the primary carbide precipitates at the end of the solidification of molten steel. As the Ce content in molten steel increases, the stability diagram of Ce2O2S and Ce-S increases gradually. The precipitation temperature of Ti-V-rich carbide is approximately 1360 ℃, and the V-rich carbide starts to precipitate at about 1200 ℃. The calculated results are keeping well with the experimental observations. The damage of primary carbide in Ce microalloyed H13 steel can be partly reduced by higher heating temperature, but cannot be completely removed.

Key words: H13 steel    rare earth    primary carbide    thermal stability    precipitation mechanism
收稿日期: 2019-05-06     
ZTFLH:  TF769.9  
基金资助:国家自然科学基金项目(No.51874034)
作者简介: 黄 宇,男,1992年生,博士
图1  Ce微合金化H13钢中主要夹杂物形貌的SEM像
Primary carbide1~3 μm3~5 μm5~10 μm>10 μmTotal
V-rich3.241.202.321.608.36
Ti-V-rich0.680.080.0400.80
表1  一次碳化物的数量密度 (mm-2)
图 2  富V碳化物的元素组成
图3  富V碳化物的纵横比
图4  一次碳化物的三维形貌
图5  图4a三维一次碳化物的EDS面扫描图
图6  三维一次碳化物的热稳定性
图7  1150、1200和1250 ℃热处理1 h后三维一次碳化物的数量密度和尺寸
图8  热处理后三维一次碳化物的EDS面扫描图
图9  Ce微合金化H13钢的平衡凝固过程
图10  1600 ℃下Fe-C-Cr-Mo-Ce-O-S体系中Ce-O-S的稳定相图
图11  一次碳化物的析出过程
[1] Chang S H, Tang T P, Huang K T. Improvement of aluminum erosion behavior and corrosion resistance of AISI H13 tool steel by oxidation treatment [J]. ISIJ Int., 2010, 50: 569
[2] Maugis P, Gouné M. Kinetics of vanadium carbonitride precipitation in steel: A computer model [J]. Acta Mater., 2005, 53: 3359
[3] Mao M T, Guo H J, Wang F, et al. Effect of cooling rate on the solidification microstructure and characteristics of primary carbides in H13 steel [J]. ISIJ Int., 2019, 59: 848
[4] Ali D, Ali Boutorabi S M, Kheirandish S. Effect of titanium carbide concentration on the morphology of MC carbides in pulsed laser surface alloyed AISI H13 tool steel [J]. Opt. Laser Technol., 2019, 112: 236
[5] Xie Y, Cheng G G, Meng X L, et al. Precipitation behavior of primary precipitates in Ti-microalloyed H13 tool steel [J]. ISIJ Int., 2016, 56: 1996
[6] Jiang Q C, Sui H L, Guan Q F. Thermal fatigue behavior of new type high-Cr cast hot work die steel [J]. ISIJ Int., 2004, 44: 1103
[7] Tang W J, Wu X C. Effect of carbides in 4Cr5MoSiVl steel on thermal fatigue behavior [J]. Heat Treat., 2003, 18: 32
[7] (唐文军, 吴晓春. 4Cr5MoSiV1钢中碳化物对热疲劳性能影响 [J]. 热处理, 2003, 18: 32)
[8] Wang L M, Lin Q, Ji J W, et al. New study concerning development of application of rare earth metals in steels [J]. J. Alloys Compd., 2006, 408-412: 384
[9] Waudby P E. Rare earth additions to steel [J]. Int. Met. Rev., 1978, 23: 74
[10] Yang X H, Wu P F, Wu C C, et al. Behavior of rare earth on modifying inclusion in special steel [J]. J. Chin. Rare Earth Soc., 2010, 28: 612
[10] (杨晓红, 吴鹏飞, 吴铖川等. 特殊钢中稀土变质夹杂物行为研究 [J]. 中国稀土学报, 2010, 28: 612)
[11] Wang L J, Liu Y Q, Wang Q, et al. Evolution mechanisms of MgO·Al2O3 inclusions by cerium in spring steel used in fasteners of high-speed railway [J]. ISIJ Int., 2015, 55: 970
[12] Huang Y, Cheng G G, Xie Y. Modification mechanism of cerium on the inclusions in drill steel [J]. Acta Metall. Sin., 2018, 54: 1253
[12] (黄 宇, 成国光, 谢 有. 稀土Ce对钎具钢中夹杂物的改质机理研究 [J]. 金属学报, 2018, 54: 1253)
[13] Huang Y, Cheng G G, Li S J, et al. Effect of cerium on the behavior of inclusions in H13 steel [J]. Steel Res. Int., 2018, 89: 1800371
[14] Liu H L, Liu C J, Jiang M F. Effect of rare earths on impact toughness of a low-carbon steel [J]. Mater. Des., 2012, 33: 306
[15] Liu X, Yang J C, Yang L, et al. Effect of Ce on inclusions and impact property of 2Cr13 stainless steel [J]. J. Iron Steel Res. Int., 2010, 17: 59
[16] Adabavazeh Z, Hwang W S, Su Y H. Effect of adding cerium on microstructure and morphology of Ce-based inclusions formed in low-carbon steel [J]. Sci. Rep., 2017, 7: 46503
[17] Yan N, Yu S F, Chen Y. In situ observation of austenite grain growth and transformation temperature in coarse grain heat affected zone of Ce-alloyed weld metal [J]. J. Rare Earths, 2017, 35: 203
[18] Yue L J, Han J S, Wang L M. Study on nonmetallic inclusions and pitting corrosion resistance of RE weathering steel [J]. Chin. Rare Earth, 2013, 34(3): 13
[18] (岳丽杰, 韩金生, 王龙妹. 稀土耐候钢中的夹杂物及耐点蚀性能研究 [J]. 稀土, 2013, 34(3): 13)
[19] Yue L J, Wang L L, Wang L M. Influence of rare earth element on the mechanical properties of clean weathering steel [J]. Chin. Rare Earth, 2014, 35(6): 20
[19] (岳丽杰, 汪磊丽, 王龙妹. 微量稀土对洁净耐候钢力学性能的影响 [J]. 稀土, 2014, 35(6): 20)
[20] Wen Z, Yi D Q, Wang B, et al. Effect of rare earths on the recrystallization behavior of T91 heat-resistant steel [J]. J. Univ. Sci. Technol. Beijing, 2013, 35: 1000
[20] (文 智, 易丹青, 王 斌等. 稀土对T91耐热钢动态再结晶行为影响 [J]. 北京科技大学学报, 2013, 35: 1000)
[21] Fu X Y, Yang J C, Jiang X Z, et al. Effects of Ce on the inclusions and impact toughness of T91 heat-resistant steel [J]. Chin. Rare Earth, 2015, 36(5): 60
[21] (富晓阳, 杨吉春, 蒋学智等. Ce对T91耐热钢夹杂物的变质及冲击韧性的影响 [J]. 稀土, 2015, 36(5): 60)
[22] Wang M J, Li Y M, Wang Z X, et al. Effect of rare earth elements on the thermal cracking resistance of high speed steel rolls [J]. J. Rare Earth, 2011, 29: 489
[23] Liu H H, Fu P X, Liu H W, et al. Carbides evolution and tensile property of 4Cr5MoSiV1 die steel with rare earth addition [J]. Metals, 2017, 7: 436
[24] Ali Hamidzadeh M, Meratian M, Saatchi A. Effect of cerium and lanthanum on the microstructure and mechanical properties of AISI D2 tool steel [J]. Mater. Sci. Eng., 2013, A571: 193
[25] Xie Y, Cheng G G, Chen L, et al. Generating mechanism of large heterogeneous carbonitrides with multiple layers in H13+Nb Bar [J]. Steel Res. Int., 2017, 88: 1600119
[26] Xie Y, Cheng G G, Chen L, et al. Characteristics and generating mechanism of large precipitates in Nb-Ti-microalloyed H13 tool steel [J]. ISIJ Int., 2016, 56: 995
[27] Huang Y, Cheng G G, Li S J, et al. Precipitation behavior of large primary carbides in cast H13 steel [J]. Steel Res. Int., 2019, 90: 1900035
[1] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[2] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[3] 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁. 以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升[J]. 金属学报, 2023, 59(4): 523-536.
[4] 杨天野, 崔丽, 贺定勇, 黄晖. 选区激光熔化AlSi10Mg-Er-Zr合金微观组织及力学性能强化[J]. 金属学报, 2022, 58(9): 1108-1117.
[5] 李民, 李昊泽, 王继杰, 马颖澈, 刘奎. 稀土Ce对薄带连铸无取向6.5%Si钢组织、高温拉伸性能和断裂模式的影响[J]. 金属学报, 2022, 58(5): 637-648.
[6] 刘洁, 徐乐, 史超, 杨少朋, 何肖飞, 王毛球, 时捷. 稀土Ce对非调质钢中硫化物特征及微观组织的影响[J]. 金属学报, 2022, 58(3): 365-374.
[7] 聂金凤, 伍玉立, 谢可伟, 刘相法. Al-AlN异构纳米复合材料的组织构型与热稳定性[J]. 金属学报, 2022, 58(11): 1497-1508.
[8] 刘仲武, 何家毅. 钕铁硼永磁晶界扩散技术和理论发展的几个问题[J]. 金属学报, 2021, 57(9): 1155-1170.
[9] 王一涵, 原园, 喻嘉彬, 吴宏辉, 吴渊, 蒋虽合, 刘雄军, 王辉, 吕昭平. 纳米晶合金热稳定性的熵调控设计[J]. 金属学报, 2021, 57(4): 403-412.
[10] 王晓波, 王墉哲, 程旭东, 蒋蓉. 大气条件下AlCrON基光谱选择性吸收涂层的热稳定性[J]. 金属学报, 2021, 57(3): 327-339.
[11] 陆斌, 陈芙蓉, 智建国, 耿如明. 应用稀土氧化物冶金技术改善高强钢焊接性能[J]. 金属学报, 2020, 56(9): 1206-1216.
[12] 彭艳艳, 余黎明, 刘永长, 马宗青, 刘晨曦, 李冲, 李会军. 650 ℃时效对9Cr-ODS钢显微组织和性能的影响[J]. 金属学报, 2020, 56(8): 1075-1083.
[13] 朱健, 张志豪, 谢建新. 基于原位TEM拉伸的稀土H13钢塑性形变行为和断裂机制[J]. 金属学报, 2020, 56(12): 1592-1604.
[14] 何贤美, 童六牛, 高成, 王毅超. Nd含量对磁控溅射Si(111)/Cr/Nd-Co/Cr薄膜结构与磁性的影响[J]. 金属学报, 2019, 55(10): 1349-1358.
[15] 黄宇, 成国光, 谢有. 稀土Ce对钎具钢中夹杂物的改质机理研究[J]. 金属学报, 2018, 54(9): 1253-1261.