| 一种Fe-Cr-Ni-Mo高强钢焊接热影响区的显微组织与冲击韧性研究 |
文明月1,2, 董文超1, 庞辉勇3, 陆善平1( ) |
1 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室 沈阳 110016 2 中国科学技术大学材料科学与工程学院 沈阳 110016 3 舞阳钢铁有限责任公司 平顶山 462500 |
|
| Microstructure and Impact Toughness of Welding Heat-Affected Zones of a Fe-Cr-Ni-Mo High Strength Steel |
Mingyue WEN1,2, Wenchao DONG1, Huiyong PANG3, Shanping LU1( ) |
1 Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China,Shenyang 110016, China 3 Wuyang Iron and Steel Co. Ltd., Pingdingshan 462500, China |
引用本文:
文明月, 董文超, 庞辉勇, 陆善平. 一种Fe-Cr-Ni-Mo高强钢焊接热影响区的显微组织与冲击韧性研究[J]. 金属学报, 2018, 54(4): 501-511.
Mingyue WEN,
Wenchao DONG,
Huiyong PANG,
Shanping LU.
Microstructure and Impact Toughness of Welding Heat-Affected Zones of a Fe-Cr-Ni-Mo High Strength Steel[J]. Acta Metall Sin, 2018, 54(4): 501-511.
| [1] | Wang C J, Liang J X, Liu Z B, et al.Effect of metastable austenite on mechanical property and mechanism in cryogenic steel applied in oceaneering[J]. Acta Metall. Sin., 2016, 52: 385(王长军, 梁剑雄, 刘振宝等. 亚稳奥氏体对低温海工用钢力学性能的影响与机理[J]. 金属学报, 2016, 52: 385) | | [2] | Di G B, Liu Z Y, Ma Q S, et al.Low temperature toughness and Z-direction performance of self-elevating platform plate[J]. J. Iron. Steel Res., 2010, 22(7): 51(狄国标, 刘振宇, 麻庆申等. 自升式平台用厚板的低温韧性与Z向性能[J]. 钢铁研究学报, 2010, 22(7): 51) | | [3] | Zhou Y L, Jia T, Zhang X J, et al.Microstructure and toughness of the CGHAZ of an offshore platform steel[J]. J. Mater. Process. Technol., 2015, 219: 314 | | [4] | Li C W, Wang Y, Han T, et al.Microstructure and toughness of coarse grain heat-affected zone of domestic X70 pipeline steel during in-service welding[J]. J. Mater. Sci., 2011, 46: 727 | | [5] | Spanos G, Fonda R W, Vandermeer R A, et al.Microstructural changes in HSLA-100 steel thermally cycled to simulate the heat-affected zone during welding[J]. Metall. Mater. Trans., 1995, 26A: 3277 | | [6] | Kumar S, Shahi A S.Studies on metallurgical and impact toughness behavior of variably sensitized weld metal and heat affected zone of AISI 304L welds[J]. Mater. Des., 2016, 89: 399 | | [7] | Hutchinson B, Komenda J, Rohrer G S, et al.Heat affected zone microstructures and their influence on toughness in two microallyed HSLA steels[J]. Acta Mater., 2015, 97: 380 | | [8] | Jang J I, Ju J B, Lee B W, et al.Effects of microstructural change on fracture characteristics in coarse-grained heat-affected zones of QLT-processes 9% Ni steel[J]. Mater. Sci. Eng., 2003, A340: 68 | | [9] | Lee S G, Lee D H, Sohn S S, et al.Effects of Ni and Mn addition on critical crack tip opening displacement (CTOD) of weld-simulated heat-affected zones of three high-strength low-alloy (HSLA) steels[J]. Mater. Sci. Eng., 2017, A697: 55 | | [10] | Li Y J, Zou Z D, Chen Z N, et al.Effects of the weld thermal cycle on microstructure and properties of the heat-affected zone of HQ130 steel[J]. Acta Metall. Sin., 1996, 32: 532(李亚江, 邹增大, 陈祝年等. 焊接热循环对HQ130钢热影响区组织及性能的影响[J]. 金属学报, 1996, 32: 532) | | [11] | Li Y J, Zou Z D, Wu H Q, et al.Microstructure and performance in the inter-critical region of heat-affected zone of HQ130 steel[J]. Trans. China Weld. Inst., 2001, 22(2): 54(李亚江, 邹增大, 吴会强等. HQ130钢热影响区的ICHAZ区组织性能[J]. 焊接学报, 2001, 22(2): 54) | | [12] | Wen T.Study on high-strength and high-toughness Fe-Cr-Ni-Mo based steel for gas cylinder application [D]. Beijing: University of Chinese Academy of Sciences, 2014(温涛. 气瓶用高强高韧Fe-Cr-Ni-Mo系合金钢的研究 [D]. 北京: 中国科学院大学, 2014) | | [13] | Mathur K K, Needleman A, Tvergaard V.Three dimensional analysis of dynamic ductile crack growth in a thin plate[J]. J. Mech. Phys. Solids, 1996, 44: 439 | | [14] | Nazari A.Simulation Charpy impact energy of functionally graded steels by modified stress-strain curve through mechanism-based strain gradient plasticity theory[J]. Comput. Mater. Sci., 2012, 51: 225 | | [15] | Curry D A.The relationship between fracture toughness and Charpy impact transition temperatures in mild steel[J]. Mater. Sci. Eng., 1980, A44: 285 | | [16] | Kim H, Park J, Kang M, et al.Interpretation of Charpy impact energy characteristics by microstructural evolution of dynamically compressed specimens in three tempered martensitic steels[J]. Mater. Sci. Eng., 2016, A649: 57 | | [17] | Das A, Viehrig H W, Bergner F, et al.Effect of microstructural anisotropy on fracture toughness of hot rolled 13Cr ODS steel—The role of primary and secondary cracking[J]. J. Nucl. Mater., 2017, 491: 83 | | [18] | Kim D K, Kim E Y, Han J, et al.Effect of microstructural factors on void formation by ferrite/martensite interface decohesion in DP980 steel under uniaxial tension[J]. Int. J. Plast., 2017, 94: 3 | | [19] | Sun X, Choi K S, Liu W N, et al.Predicting failure modes and ductility of dual phase steels using plastic strain localization[J]. Int. J. Plast., 2009, 25: 1888 | | [20] | Rice J R, Tracey D M.On the ductile enlargement of voids in triaxial stress fields[J]. J. Mech. Phys. Solids, 1969, 17: 201 | | [21] | Cox T B, Low J R.An investigation of the plastic fracture of AISI 4340 and 18 Nickel-200 grade maraging steels[J]. Metall. Trans., 1974, 5: 1457 | | [22] | Tvergaard V. Study of localization in a void-sheet under stress states near pure shear [J]. Int. J. Solids Struct., 2015, 75-76: 134 | | [23] | Eizadjou M, Manesh H D, Janghorban K.Microstructure and mechanical properties of ultra-fine grains (UFGs) aluminum strips produced by ARB process[J]. J. Alloys Compd., 2009, 474: 406 | | [24] | Valiev R Z, Murashkin M Y, Semenova I P.Grain boundaries and mechanical properties of ultrafine-grained metals[J]. Metall. Mater. Trans., 2010, 41A: 816 | | [25] | Wen T, Hu X F, Song Y Y, et al.Effect of tempering temperature on carbide and mechanical properties in a Fe-Cr-Ni-Mo high-strength steel[J]. Acta Metall. Sin., 2014, 50: 447(温涛, 胡小锋, 宋元元等. 回火温度对一种Fe-Cr-Ni-Mo高强钢碳化物及其力学性能的影响[J]. 金属学报, 2014, 50: 447) | | [26] | Cao R, Feng W, Peng Y, et al.Investigation of abnormal high impact toughness in simulated welding CGHAZ of a 8%Ni 980 MPa high strength steel[J]. Mater. Sci. Eng., 2010, A528: 631 |
|
|