| 冷拉拔珠光体钢丝的力学性能各向异性研究 |
季培蓓, 周立初, 周雪峰, 方峰( ), 蒋建清 |
| 东南大学材料与科学工程学院 南京 211189 |
|
| Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire |
Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG( ), Jianqing JIANG |
| School of Materials Science and Engineering, Southeast University, Nanjing 211189, China |
引用本文:
季培蓓, 周立初, 周雪峰, 方峰, 蒋建清. 冷拉拔珠光体钢丝的力学性能各向异性研究[J]. 金属学报, 2018, 54(4): 494-500.
Peibei JI,
Lichu ZHOU,
Xuefeng ZHOU,
Feng FANG,
Jianqing JIANG.
Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. Acta Metall Sin, 2018, 54(4): 494-500.
| [1] | Zelin M.Microstructure evolution in pearlitic steels during wire drawing[J]. Acta Mater., 2002, 50: 4431 | | [2] | Li Y J, Choi P, Goto S, et al.Evolution of strength and microstructure during annealing of heavily cold-drawn 6.3 GPa hypereutectoid pearlitic steel wire[J]. Acta Mater., 2012, 60: 4005 | | [3] | Read H G, Reynolds Jr W T, Hono K, et al. APFIM and TEM studies of drawn pearlitic wire[J]. Scr. Mater., 1997, 37: 1221 | | [4] | Zhang X D, Godfrey A, Huang X X, et al.Microstructure and strengthening mechanisms in cold-drawn pearlitic steel wire[J]. Acta Mater., 2011, 59: 3422 | | [5] | Embury J D, Fisher R M.The structure and properties of drawn pearlite[J]. Acta Metall., 1966, 14: 147 | | [6] | Buono V T L, Gonzalez B M, Lima T M, et al. Measurement of fine pearlite interlamellar spacing by atomic force microscopy[J]. J. Mater. Sci., 1997, 32: 1005 | | [7] | Zhou L C, Hu X J, Ma C, et al.Effect of pearlitic lamella orientation on deformation of pearlite steel wire during cold drawing[J]. Acta Metall. Sin., 2015, 51: 897(周立初, 胡显军, 马驰等. 珠光体层片取向对冷拔珠光体钢丝形变的影响[J]. 金属学报, 2015, 51: 897) | | [8] | Fang F, Zhao Y F, Liu P P, et al.Deformation of cementite in cold drawn pearlitic steel wire[J]. Mater. Sci. Eng., 2014, A608: 11 | | [9] | Lamontagne A, Massardier V, Kléber X, et al.Comparative study and quantification of cementite decomposition in heavily drawn pearlitic steel wires[J]. Mater. Sci. Eng., 2015, A644: 105 | | [10] | Li Y J, Choi P, Borchers C, et al.Atom probe tomography characterization of heavily cold drawn pearlitic steel wire[J]. Ultramicroscopy, 2011, 111: 628 | | [11] | Li Y J, Choi P, Borchers C, et al.Atomic-scale mechanisms of deformation-induced cementite decomposition in pearlite[J]. Acta Mater., 2011, 59: 3965 | | [12] | Zhou L C, Fang F, Zhou X F, et al.Cementite nano-crystallization in cold drawn pearlitic wires instigated by low temperature annealing[J]. Scr. Mater., 2016, 120: 5 | | [13] | Li Y J, Raabe D, Herbig M, et al.Segregation stabilizes nanocrystalline bulk steel with near theoretical strength[J]. Phys. Rev. Lett., 2014, 113: 106104 | | [14] | Fang F, Zhou L C, Hu X J, et al.Microstructure and mechanical properties of cold-drawn pearlitic wires affect by inherited texture[J]. Mater. Des., 2015, 79: 60 | | [15] | Zhang X D, Godfrey A, Hansen N, et al.Hierarchical structures in cold-drawn pearlitic steel wire[J]. Acta Mater., 2013, 61: 4898 | | [16] | Zhao T Z, Song H W, Zhang G L, et al.The texture evolution at the center of pearlitic steel wire during drawing and its influence on the mechanical properties[J]. Acta Metall. Sin., 2014, 50: 667(赵天章, 宋鸿武, 张光亮等. 拉拔过程中珠光体钢丝心部的织构演化规律及其对力学性能的影响[J]. 金属学报, 2014, 50: 667) | | [17] | Zhang X D, Godfrey A, Liu W, et al.Evolutions of microstructure and ferritic micro-orientation and texture in a pearlitic steel wire during cold drawing[J]. Acta Metall. Sin., 2010, 46: 141(张晓丹, Godfrey A, 刘伟等. 珠光体钢丝冷拉拔过程中微观组织及铁素体微区取向与织构演变[J]. 金属学报, 2010, 46: 141) | | [18] | Kapp M W, Hohenwarter A, Wurster S, et al.Anisotropic deformation characteristics of an ultrafine-and nanolamellar pearlitic steel[J]. Acta Mater., 2016, 106: 239 | | [19] | Kammerhofer C, Hohenwarter A, Scheriau S, et al.Influence of morphology and structural size on the fracture behavior of a nanostructured pearlitic steel[J]. Mater. Sci. Eng., 2013, A585: 190 | | [20] | Hohenwarter A, Taylor A, Stock R, et al.Effect of large shear deformations on the fracture behavior of a fully pearlitic steel[J]. Metall. Mater. Trans., 2011, 42A: 1609 | | [21] | He Y, Xiang S, Shi W, et al.Effect of microstructure evolution on anisotropic fracture behaviors of cold drawing pearlitic steels[J]. Mater. Sci. Eng., 2017, A683: 153 | | [22] | Toribio J, Ayaso F J.Anisotropic fracture behaviour of cold drawn steel: A materials science approach[J]. Mater. Sci. Eng., 2003, A343: 265 | | [23] | Suzuki T, Tomota Y, Isaka M, et al.Strength anisotropy and residual stress in drawn pearlite steel wire[J]. ISIJ Int., 2004, 44: 1426 | | [24] | Zhang X D, Hansen N, Godfrey A, et al.Dislocation-based plasticity and strengthening mechanisms in sub-20 nm lamellar structures in pearlitic steel wire[J]. Acta Mater., 2016, 114: 176 | | [25] | Ju H L, Li B H, Wu Z F, et al.Perpendicular magnetic anisotropy in Co/Ni multilayers studied by anomalous Hall effect[J]. Acta Phys. Sin., 2015, 64: 097501(俱海浪, 李宝河, 吴志芳等. Co/Ni多层膜垂直磁各向异性的研究[J]. 物理学报, 2015, 64: 097501) | | [26] | Chen Z Y, Cai H N, Wang F C, et al.Investigation on anisotropy of dynamic compressive mechanical properties of cold-rolled Cu sheet[J]. Acta Metall. Sin., 2009, 45: 143(陈志永, 才鸿年, 王富耻等. 冷轧Cu板动态压缩力学性能各向异性的研究[J]. 金属学报, 2009, 45: 143) | | [27] | Xu Y B, Liu M Z.An in situ study of crack nucleation and propagation in pearlite during deformation[J]. Acta Metall. Sin., 1982, 18: 58(徐永波, 刘民治. 珠光体组织的形变、裂纹形核与扩展微观过程的动态研究[J]. 金属学报, 1982, 18: 58) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|