| 定向凝固DZ444镍基高温合金初生MC碳化物的分解行为 |
肖旋1, 曾超1,2, 侯介山2, 秦学智2, 郭建亭2, 周兰章2( ) |
1 沈阳理工大学材料科学与工程学院, 沈阳110159 2 中国科学院金属研究所, 沈阳110016 |
|
| THE DECOMPOSITION BEHAVIOR OF PRIMARY MC CARBIDE IN NICKEL BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ444 |
XIAO Xuan1, ZENG Chao1,2, HOU Jieshan2, QIN Xuezhi2, GUO Jianting2, ZHOU Lanzhang2( ) |
1 School of Materials Science and Engineering, Shenyang Ligong University, Shenyang 110159 2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
肖旋, 曾超, 侯介山, 秦学智, 郭建亭, 周兰章. 定向凝固DZ444镍基高温合金初生MC碳化物的分解行为[J]. 金属学报, 2014, 50(9): 1031-1038.
Xuan XIAO,
Chao ZENG,
Jieshan HOU,
Xuezhi QIN,
Jianting GUO,
Lanzhang ZHOU.
THE DECOMPOSITION BEHAVIOR OF PRIMARY MC CARBIDE IN NICKEL BASE DIRECTIONALLY SOLIDIFIED SUPERALLOY DZ444[J]. Acta Metall Sin, 2014, 50(9): 1031-1038.
| [1] |
Wang J, Zhou L Z, Sheng L Y, Guo J T. Mater Des, 2012; 39: 55
|
| [2] |
Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Mater Sci Eng, 2012; A543: 121
|
| [3] |
Guo J T. Materials Science and Engineering for Superalloys I. Beijing: Science Press, 2008: 4
|
| [3] |
(郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 4)
|
| [4] |
Collins H E, Quigg R J. Trans ASM, 1968; 61: 139
|
| [5] |
Wu Q Y, Song H, Swindeman R W, Shingledecker J P, Vasudevan V K. Metall Mater Trans, 2008; 39A: 2569
|
| [6] |
Zhao S Q, Xie X S, Gaylord S D, Shailesh P J. Mater Des, 2006; 27: 1120
|
| [7] |
Hou J S, Zhou L Z, Yuan C, Tang Z, Guo J T, Qin X Z, Liaw P K. Mater Sci Eng, 2013; A560: 25
|
| [8] |
Choi B G, Kim I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329
|
| [9] |
Huang X B, Kang Y, Zhou H H, Zhang Y, Hu Z Q. Mater Lett, 1998; 36: 210
|
| [10] |
Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361: 191
|
| [11] |
He L Z, Zheng Q, Sun X F, Hou G C, Guan H R, Hu Z Q. Mater Sci, 2005; 40: 2959
|
| [12] |
Qin X Z, Guo J T, Yuan C, Chen C L, Hou J S, Ye H Q. Mater Sci Eng, 2008; A485: 75
|
| [13] |
Hou J S, Guo J T, Yang G X, Zhou L Z, Qin X Z, Ye H Q. Mater Sci Eng, 2008; A498: 449
|
| [14] |
Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; 37: 237
|
| [15] |
Nazmy M, Staubli M. Scr Metall Mater, 1990; 24: 135
|
| [16] |
Wang J, Zhou L Z, Qin X Z, Sheng L Y, Hou J S, Guo J T. Mater Sci Eng, 2012; A553: 14
|
| [17] |
Lvov G, Levit V I, Kaufman M J. Metall Mater Trans, 2004; 35A: 1672
|
| [18] |
Sims C T, Stoloff N S, Hagel W C. Superalloys II. New York: John Wiley & Sons Inc., 1987: 122
|
| [19] |
Tawancy H M, Abbas N M, Al-Mana A I, Rhysjones T N. J Mater Sci, 1994; 29: 2445
|
| [20] |
Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Acta Metall Sin, 2010; 46: 216
|
| [20] |
(秦学智, 郭建亭, 袁 超, 侯介山, 周兰章, 叶恒强. 金属学报. 2010; 46: 216)
|
| [21] |
Qin X Z. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007
|
| [21] |
(秦学智. 中国科学院金属研究所博士学位论文, 沈阳, 2007)
|
| [22] |
Cyril W, Water B, Robert F M. J Metall Trans AIME, 1950; 188: 558
|
| [23] |
Fujiwara K, Horita Z. Acta Mater, 2002; 50: 1578
|
| [24] |
Minamino Y, Jung S B, Yamane T, Hirao K. Metall Trans, 1992; 23A: 2784
|
| [25] |
Karunaratne M S A, Carter P, Reed R C. Acta Metall, 2001; 49: 861
|
| [26] |
Watanable M, Horita Z, Smith D J, McCartney M R, Sano T, Nemoto M. Acta Metall, 1994; 42: 3381
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|