| 高锰TRIP/TWIP钢压缩过程晶体学行为的EBSD分析 I. 相变特点、孪生及奥氏体取向的影响 |
| 杨平; 鲁法云; 孟 利; 崔凤娥 |
| 北京科技大学材料学院; 北京 100083 |
|
εCRYSTALLOGRAPHIC BEHAVIORS OF COMPRESSED HIGH MANGANESE TRIP/TWIP STEELS ANALYZED BY EBSD TECHNIQUES
I. Transformation Characteristics, Twinning and the Influence of Austenitic Orientations |
| YANG Ping; LU Fayun; MENG Li; CUI Feng’e |
| School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
杨平 鲁法云 孟 利 崔凤娥. 高锰TRIP/TWIP钢压缩过程晶体学行为的EBSD分析 I. 相变特点、孪生及奥氏体取向的影响[J]. 金属学报, 2010, 46(6): 657-665.
.
εCRYSTALLOGRAPHIC BEHAVIORS OF COMPRESSED HIGH MANGANESE TRIP/TWIP STEELS ANALYZED BY EBSD TECHNIQUES
I. Transformation Characteristics, Twinning and the Influence of Austenitic Orientations[J]. Acta Metall Sin, 2010, 46(6): 657-665.
| [1] Frommeyer G, Br¨ux U, Neumann P. ISIJ Int, 2003; 43: 438
[2] Huang B X, Wang X D, Rong Y H, Wang L, Jin L. Mater Sci Eng, 2006; A438–440: 306
[3] Gr¨assel O, Kr¨uger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391
[4] Srivastava A K, Bhattacharjee D, Jha G, Gope N, Singh S B. Mater Sci Eng, 2007, A445–446: 549
[5] Jacques P J, Furne’mont Q, Lani F, Pardoen T, Delannay F. Acta Mater, 2007; 55: 3681
[6] Bracke L, Kestens L, Penning J. Scr Mater, 2007; 57: 385
[7] Idrissi H, Ryelandt L, Veron M, Schryvers D, Jacques P J. Scr Mater, 2009; 60: 941
[8] Tsakiris V, Edmonds D V. Mater Sci Eng, 1999; A273–275: 430
[9] Kirindi T, Dikici M. J Alloys Compd, 2006; 407: 157
[10] Kireeva I V, Chumlyakov Y I. Mater Sci Eng, 2008; A481–482: 737
[11] Meng L, Yang P, Xie Q, Ding H, Tang Z. Scr Mater, 2007; 56: 931
[12] Gey N, Petit B, Humbert M. Metall Mater Trans, 2005; 36A: 3291
[13] Kitahara H, Ueji R, Tsuji N, Minamino Y. Acta Mater, 2006; 54: 1279
[14] Kitahara H, Uejib R, Uedac M, Tsujia N, Minamino Y. Mater Charact, 2005; 54: 378
[15] Lu F Y. Master Dissertation, Univeristy of Science and Technology Beijing, 2009
(鲁法云. 北京科技大学硕士学位论文, 2009)
[16] Bracke L, Meert G, Penning J, Cooman B C De. Metall Mater Trans, 2006; 37A: 307 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|