| 高压扭转Cu试样微观组织的热稳定性分析 |
| 谢子令1;2; 武晓雷2; 谢季佳2; 洪友士2 |
1. 温州大学建筑与土木工程学院; 温州 325035
2. 中国科学院力学研究所非线性力学国家重点实验室; 北京 100190 |
|
| ANALYSIS OF THE THERMAL STABILITY OF COPPER SPECIMENS DEFORMED BY HIGH–PRESSURE TORSION |
| XIE Ziling 1;2; WU Xiaolei 2; XIE Jijia 2; HONG Youshi 2 |
1. College of Architecture and Civil Engineering; University of Wenzhou; Wenzhou 325035
2. State Key Laboratory of Nonlinear Mechanics; Institute of Mechanics; Chinese Academy of Sciences; Beijing 100190 |
引用本文:
谢子令 武晓雷 谢季佳 洪友士. 高压扭转Cu试样微观组织的热稳定性分析[J]. 金属学报, 2010, 46(4): 458-465.
,
,
,
.
ANALYSIS OF THE THERMAL STABILITY OF COPPER SPECIMENS DEFORMED BY HIGH–PRESSURE TORSION[J]. Acta Metall Sin, 2010, 46(4): 458-465.
| [1] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[2] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[3] Wang J T, Kang S B, Kim H W, Horita Z. J Mater Sci, 2002; 37: 5223
[4] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S. Acta Mater, 2006; 54: 655
[5] Wu X L, Tao N R, Wei Q M, Jiang P, Lu J, Lu K. Acta Mater, 2007; 55: 5768
[6] Xie Z L, Wu X L, Xie J J, Hong Y S. Acta Metall Sin, 2008; 44: 803
(谢子令, 武晓雷, 谢季佳, 洪友士. 金属学报, 2008; 44: 803)
[7] Zhang K, Weertman J R, Eastman J A. Appl Phys Lett, 2005; 87: 61921
[8] Liao X Z, Kilmametov A R, Valiev R Z, Gao H S, Li X D, Mukherjee A K, Bingert J F, Zhu Y T. Appl Phys Lett, 2006; 88: 21909
[9] Schafler E, Kerber M B. Mater Sci Eng, 2007; A462: 139
[10] Jiang H G, Zhu Y T, Butt D P, Alexandrov I V, Lowe T C. Mater Sci Eng, 2000; A290: 128
[11] Pan J S, Tong J M, Dian M B. Foundation of Material Science. Beijing: Tsinghua University Press, 1998: 512
(潘金生, 仝健民, 田民波. 材料科学基础. 北京: 清华大学出版社, 1998: 512)
[12] Wang Y M, Jiao T, Ma E. Mater Trans, 2003; 44: 1926
[13] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. New York: Pergamon, 2004:11
[14] Zhang Y, Tao N R, Lu K. Acta Mater, 2008; 56: 2429 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|