| 双相不锈钢中奥氏体相内裂纹扩展路径的透射电镜原位观察 |
| 姚可夫;唐迺泳;陈南平 |
| 北京科技大学材料科学与工程系;博士后北京(100083);清华大学;清华大学 |
|
| IN SITU OBSERVATION ON CRACK PROPAGATING PATH IN AUSTENITE OF A DUPLEX STAINLESS STEEL |
| YAO Kefu University of Science and Technology Beijing; TANG Naiyong; CHEN Nanping Tsinghua University; Beijing |
引用本文:
姚可夫;唐迺泳;陈南平. 双相不锈钢中奥氏体相内裂纹扩展路径的透射电镜原位观察[J]. 金属学报, 1991, 27(2): 20-26.
,
,
.
IN SITU OBSERVATION ON CRACK PROPAGATING PATH IN AUSTENITE OF A DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 1991, 27(2): 20-26.
| 1 Kobayashi S. Ohr S M. Philos Mag, 1980; A42: 763
2 Kobayashi S, Ohr S M. Scr Metall, 1981; 15: 343
3 Kobayashi S, Ohr S M. J Mater Sci, 1984; 19: 2273
4 Ohr S M. Mater Sci Eng, 1985; 72: 1
5 张以增,戴蜀娟,邹鸿承,苗丕峰.理化检验(物理分册),1985;22(5) :19
6 姚可夫,唐迺泳,陈南平.金属学报,1989; 25:A213
7 姚可夫,清华大学博士学位论文,1989
8 姚可夫,唐迺泳,陈南平.第五届全国断裂力学会议论文集,桂林,1988:1564
9 Lin I-H, Thomson R. Acta Metall, 1986; 34: 187 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|