| 汽车用齿轮钢16MnCrS5热处理变形机理 |
屈小波1( ), 安金敏1, 王林2, 李喜2( ) |
1 江苏永钢集团有限公司 苏州 215628 2 上海交通大学 材料科学与工程学院 上海 200240 |
|
| Quenching Deformation of the 16MnCrS5 Gear Steel for Automobile |
QU Xiaobo1( ), AN Jinmin1, WANG Lin2, LI Xi2( ) |
1 Jiangsu Yonggang Group Co. Ltd., Suzhou 215628, China 2 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China |
引用本文:
屈小波, 安金敏, 王林, 李喜. 汽车用齿轮钢16MnCrS5热处理变形机理[J]. 金属学报, 2025, 61(4): 597-607.
Xiaobo QU,
Jinmin AN,
Lin WANG,
Xi LI.
Quenching Deformation of the 16MnCrS5 Gear Steel for Automobile[J]. Acta Metall Sin, 2025, 61(4): 597-607.
| 1 |
Lin C, Zhao M J, Pan H, et al. Blending gear shift strategy design and comparison study for a battery electric city bus with AMT [J]. Energy, 2019, 185: 1
|
| 2 |
Arunachalam R, Krishnan P K, Muraliraja R. A review on the production of metal matrix composites through stir casting—Furnace design, properties, challenges, and research opportunities [J]. J. Manuf. Processes, 2019, 42: 213
|
| 3 |
Gupta K, Jain N K, Laubscher R F. Spark erosion machining of miniature gears: A critical review [J]. Int. J. Adv. Manuf. Technol., 2015, 80: 1863
|
| 4 |
Xiao N, Hui W J, Zhang Y J, et al. Hydrogen embrittlement behavior of a vacuum-carburized gear steel [J]. Acta Metall. Sin., 2021, 57: 977
doi: 10.11900/0412.1961.2020.00363
|
| 4 |
肖 娜, 惠卫军, 张永健 等. 真空渗碳处理齿轮钢的氢脆敏感性 [J]. 金属学报, 2021, 57: 977
|
| 5 |
Inoue A, Takeuchi A. Recent development and application products of bulk glassy alloys [J]. Acta Mater., 2011, 59: 2243
|
| 6 |
Fang X R, Liu L, Xu H H, et al. Effect of pre-heat treatment before carburizing on distortion of gear shaft made of 17CrNiMo6 steel [J]. Heat Treat. Met., 2022, 47(3): 113
doi: 10.13251/j.issn.0254-6051.2022.03.022
|
| 6 |
方秀荣, 刘 留, 徐慧慧 等. 渗碳前预热处理对17CrNiMo6钢制齿轮轴畸变的影响 [J]. 金属热处理, 2022, 47(3): 113
doi: 10.13251/j.issn.0254-6051.2022.03.022
|
| 7 |
Zhang G Q. Microstructure and distortion of niobium-containing 18CrNiMo7-6 gear steel after high-temperature carburization [D]. Beijing: Central Iron & Steel Research Institute, 2021
|
| 7 |
张国强. 含铌18CrNiMo7-6齿轮钢高温渗碳组织和变形研究 [D]. 北京: 钢铁研究总院, 2021
|
| 8 |
Cao Y G. Study on hardenability, heat treatment distortion and fatigue property of carburized gear steels [D]. Beijing: Central Iron & Steel Research Institute, 2017
|
| 8 |
曹燕光. 渗碳齿轮钢淬透性及其热处理变形和疲劳性能研究 [D]. 北京: 钢铁研究总院, 2017
|
| 9 |
Liu J M. Research on abnormal deformation of automobile gear during carburizing and quenching heat treatment [J]. Met. Work., 2005, (11): 40
|
| 9 |
刘建明. 汽车齿轮渗碳淬火热处理异常变形的研究 [J]. 机械工人, 2005, (11): 40
|
| 10 |
An J M, Qin M, Ding Y. Effect of austenite grain size on heat treatment distortion automotive gear steels [J]. Heat Treat., 2013, 28(3): 48
|
| 10 |
安金敏, 覃 明, 丁 毅. 奥氏体晶粒度对汽车齿轮钢热处理畸变的影响 [J]. 热处理, 2013, 28(3): 48
|
| 11 |
Wang J, Dang S E, Fan Z J, et al. Microstructure homogenization of 17CrNiMo6 gear steel [J]. Heat Treat. Met., 2022, 47(11): 126
doi: 10.13251/j.issn.0254-6051.2022.11.022
|
| 11 |
王 杰, 党淑娥, 范子靖 等. 17CrNiMo6齿轮钢的组织均匀化 [J]. 金属热处理, 2022, 47(11): 126
|
| 12 |
Lai H Z. Research on forming mechanism of banded structure in 60Si2Mn spring flat steel and its influence on mechanical properties [D]. Ganzhou: Jiangxi University of Science and Technology, 2014
|
| 12 |
赖泓州. 60Si2Mn弹簧扁钢带状组织形成机理及对性能的影响研究 [D]. 赣州: 江西理工大学, 2014
|
| 13 |
Hua G P, Chao G Q, Shi J X. Formation and elimination of banded structure of 20CrNi2Mo steel [J]. Loco. Rolling Stock Technol., 2003, (5): 7
|
| 13 |
华公平, 晁国强, 侍继香. 20CrNi2Mo钢带状组织的形成与消除 [J]. 机车车辆工艺, 2003, (5): 7
|
| 14 |
Wang Z Y, Xing Z G, Wang H D, et al. The relationship between inclusions characteristic parameters and bending fatigue performance of 20Cr2Ni4A gear steel [J]. Int. J. Fatigue, 2022, 155: 106594
|
| 15 |
Wang B X, Liu X H, Wang G D. Dynamic recrystallisation behaviour and microstructural evolution in a Mn-Cr gear steel [J]. Mater. Sci. Technol., 2005, 21: 798
|
| 16 |
Huang J B. Research on the hardenability and phase transformation behavior of heavy transmission gear steel [D]. Beijing: Beijing Jiaotong University, 2017
|
| 16 |
黄金宝. 重载传动齿轮钢淬透性及相变变形规律的研究 [D]. 北京: 北京交通大学, 2017
|
| 17 |
Yang C, An J M, Huan Z Z. Numerical simulation of banded microstructure on quenching distortion in gear steel based on Deform [J]. Bao-Steel Technol., 2016, (3): 16
|
| 17 |
杨 超, 安金敏, 黄宗泽. 基于Deform的带状组织对齿轮钢淬火变形影响数值模拟 [J]. 宝钢技术, 2016, (3): 16
|
| 18 |
Seo H, Lee D G, Park J, et al. Quench hardening effect of gray iron brake discs on particulate matter emission [J]. Wear, 2023, 523: 204781
|
| 19 |
Zhang W H. A study on fabrication, heat-treatments and mechanical properties of V-Nb microalloyed gear steel [D]. Wuhan: Wuhan University of Science and Technology, 2007
|
| 19 |
张文汉. V-Nb微合金化齿轮钢及其热处理工艺和力学性能的研究 [D]. 武汉: 武汉科技大学, 2007
|
| 20 |
An X X, Tian Y, Wang H J, et al. Suppression of austenite grain coarsening by using Nb-Ti microalloying in high temperature carburizing of a gear steel [J]. Adv. Eng. Mater., 2019, 21: 1900132
|
| 21 |
O'Brien E C H C, Yeddu H K. Multi-length scale modeling of carburization, martensitic microstructure evolution and fatigue properties of steel gears [J]. J. Mater. Sci. Technol., 2020, 49: 157
doi: 10.1016/j.jmst.2019.10.044
|
| 22 |
Wang B, He Y P, Liu Y, et al. Mechanism of the microstructural evolution of 18Cr2Ni4WA steel during vacuum low-pressure carburizing heat treatment and its effect on case hardness [J]. Materials, 2020, 13: 2352
|
| 23 |
Wang Y B. A study on hardenability and band structure of 20CrMoH gear steel [D]. Kunmin: Kunming University of Science and Technology, 2010
|
| 23 |
王彦彬. 20CrMoH齿轮钢的淬透性及带状组织研究 [D]. 昆明: 昆明理工大学, 2010
|
| 24 |
Hu S B. A simple conversion formule of HV and HRC mutual [J]. J. Hubei Univ. Auto. Technol., 1992, (2): 64
|
| 24 |
胡树兵. 一种简单的洛氏C硬度与维氏硬度相互换算数学公式 [J]. 湖北汽车工业学院学报, 1992, (2): 64
|
| 25 |
Koistine D F, Marburger R E. A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels [J]. Acta Metall., 1959, 7: 59
|
| 26 |
Denis S, Gautier E, Simon A, et al. Stress-phase-transformation interactions—Basic principles, modelling, and calculation of internal stresses [J]. Mater. Sci. Technol., 1985, 1: 805
|
| 27 |
Li H B, Zheng M Y, Tian W, et al. Flow stress constitutive equation of M50NiL gear steel based on Johnson-Cook model [J]. Mater. Mech. Eng., 2016, 40(11): 31
|
| 27 |
李红斌, 郑明月, 田 伟 等. 基于Johnson-Cook模型构建M50NiL齿轮钢的流变应力本构方程 [J]. 机械工程材料, 2016, 40(11): 31
|
| 28 |
Rego R, Löpenhaus C, Gomes J, et al. Residual stress interaction on gear manufacturing [J]. J. Mater. Process. Technol., 2018, 252: 249
|
| 29 |
Chen W, He X F, Yu W C, et al. Nano- and microhardness distribution in the carburized case of Nb-microalloyed gear steel [J]. J. Mater. Eng. Perform., 2020, 29: 4626
doi: 10.1007/s11665-020-04992-7
|
| 30 |
Du Y F. Effects of heat treatment and hot processing on banded structure characteristics and mechanical properties of PCrNi3MoV steel [D]. Taiyuan: North University of China, 2021
|
| 30 |
杜云飞. 热处理和热加工对PCrNi3MoV钢带状组织及力学性能的影响研究 [D]. 太原: 中北大学, 2021
|
| 31 |
Zhang Y T. Studies on mechanism and control of die quenching deformation for spiral bevel gear [D]. Chongqing: Chongqing University, 2017
|
| 31 |
张映桃. 螺旋锥齿轮模压淬火变形机理及控制研究 [D]. 重庆: 重庆大学, 2017
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|