纳入残余应力时不同拘束下DMWJ的断裂行为
吴进1, 杨杰1(), 陈浩峰2
1.上海理工大学 能源与动力工程学院 上海 200093
2.Department of Mechanical & Aerospace Engineering, University of Strathclyde, Glasgow, G1 1XJ, UK
Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress
WU Jin1, YANG Jie1(), CHEN Haofeng2
1.School of Energy and Power Engineering, University of Shanghai for Science and Technology, Shanghai 200093, China
2.Department of Mechanical & Aerospace Engineering, University of Strathclyde, Glasgow, G1 1XJ, UK
引用本文:

吴进, 杨杰, 陈浩峰. 纳入残余应力时不同拘束下DMWJ的断裂行为[J]. 金属学报, 2022, 58(7): 956-964.
Jin WU, Jie YANG, Haofeng CHEN. Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress[J]. Acta Metall Sin, 2022, 58(7): 956-964.

全文: PDF(2078 KB)   HTML
摘要: 

以核电安全端异种金属焊接接头(DMWJ)为研究对象,选用含中心裂纹三点弯曲(SENB)试样,分别在试样左右两面、上下两面、前后两面、左右上下前后六面施加不同载荷以在裂尖产生不同的应力,通过restart方法,将该应力作为残余应力引入SENB试样,系统研究考虑残余应力时不同拘束下DMWJ的断裂行为及残余应力与拘束效应的交互作用。结果表明:残余应力的变化对不同拘束下DMWJ的断裂行为有很大的影响。与低拘束试样相比,高拘束试样的J-R曲线对残余应力的变化更加敏感,这主要与裂尖的Mises应力和三向应力有关。残余应力对不同拘束下DMWJ J-R曲线的影响也与残余应力的方向相关。

关键词 : 残余应力,  拘束效应,  异种金属焊接接头,  断裂行为,  抗断裂设计    
Abstract:

In nuclear power pressure vessels, dissimilar metal welded joints (DMWJs) are the weak link owing to their highly heterogeneous microstructure, mechanical, thermal, and fracture properties; and some defects that occur at different positions within the DMWJs. To ensure the safety of nuclear power pressure vessels, it is important to examine the fracture behavior of DMWJ in detail. In addition to residual stress, constraint is an important factor affecting the fracture behavior of DMWJ. To understand this behavior, both constraint and residual stress must be considered. In this work, taking nuclear safety and DMWJ as the research objects, three-point bending (SENB) specimens with a central crack were selected. Different loads were applied to different sides of the specimen to produce different stresses at the crack tip, such as left and right, up and down, front and back, and both six sides, and the stresses were introduced into the SENB specimen as the residual stress by restart method. The fracture behavior of DMWJ was then systematically studied under various constraints considering residual stresses and the interaction between residual stress and constraint. The results showed that the change in residual stress significantly influenced the fracture behavior of DMWJ under different constraints. In contrast to the DMWJ with low constraint, the J-R curve of the DMWJ with high constraint was more sensitive to the change in residual stress. The main cause was the Mises stress at the crack tip and the triaxial stress. The direction of residual stress also influenced the J-R curve.

Key words: residual stress    constraint effect    dissimilar metal welded joint    fracture behavior    anti-fracture design
收稿日期: 2021-06-18     
ZTFLH:  TH114  
基金资助:国家自然科学基金项目(51975378)
作者简介: 吴 进,男,1997年生,硕士生
图 1  52M镍基合金异种金属焊接接头
图2  A508/52Mb界面附近子区域的细分示意图
图3  SENB试样的取样与尺寸示意图
图4  有限元数值计算的2个步骤
图5  左右两面加载时不同拘束SENB试样的J-R曲线
图6  不同载荷所引起的不同拘束试样裂尖的Mises应力
Loading directiona / W = 0.2a / W = 0.7
S11S22S33S11S22S33
Left and right sides-250.336-101.749-139.374-648.487-413.334-415.037
Up and down sides51.29422.198-16.06574.55832.180-20.025
Front and back sides14.327-43.5098.3066.344-46.6793.897
Six sides-297.622-170.190-212.761-715.665-365.400-481.419
表1  不同面加载50 MPa时的裂尖三向应力 (MPa)
图7  预加载荷为1 MPa时不同拘束试样的裂尖应力场
图8  上下两面加载时a / W = 0.2和0.7拘束SENB试样的J-R曲线
图9  不同载荷所引起的不同拘束试样裂尖的Mises应力
图10  前后两面加载时a / W = 0.2和0.7拘束SENB试样的J-R曲线
图11  六面加载时a / W = 0.2和0.7拘束SENB试样的J-R曲线
1 Li C L, Zhang M Q. Overview of reactor pressure vessel steel in PWR nuclear power plants [J]. Mater. Rep., 2008, 22(9): 65
1 李承亮, 张明乾. 压水堆核电站反应堆压力容器材料概述 [J]. 材料导报, 2008, 22(9): 65
2 Li G F, Li G J, Fang K W, et al. Stress corrosion cracking behavior of dissimilar metal weld A508/52M/316L in high temperature water environment [J]. Acta Metall. Sin., 2011, 47: 797
2 李光福, 李冠军, 方可伟 等. 异材焊接件A508/52M/316L在高温水环境中的应力腐蚀破裂 [J]. 金属学报, 2011, 47: 797
3 Østby E, Thaulow C, Zhang Z L. Numerical simulations of specimen size and mismatch effects in ductile crack growth—Part I: Tearing resistance and crack growth paths [J]. Eng. Fract. Mech., 2007, 74: 1770
doi: 10.1016/j.engfracmech.2006.09.013
4 Østby E, Thaulow C, Zhang Z L. Numerical simulations of specimen size and mismatch effects in ductile crack growth—Part II: Near-tip stress fields [J]. Eng. Fract. Mech., 2007, 74: 1793
doi: 10.1016/j.engfracmech.2006.09.014
5 Yang F Q, Xue H, Zhao L Y, et al. Effects of welded mechanical heterogeneity on interface crack propagation in dissimilar weld joints [J]. Adv. Mater. Sci. Eng., 2019, 2019: 6593982
6 Jang C, Lee J, Kim J S, et al. Mechanical property variation within Inconel 82/182 dissimilar metal weld between low alloy steel and 316 stainless steel [J]. Int. J. Press. Vessels. Pip., 2008, 85: 635
doi: 10.1016/j.ijpvp.2007.08.004
7 Yang J, Wang G Z, Xuan F Z, et al. An experimental investigation of in-plane constraint effect on local fracture resistance of a dissimilar metal welded joint [J]. Mater. Des., 2014, 53: 611
doi: 10.1016/j.matdes.2013.07.058
8 Yang J, Wang G Z, Xuan F Z, et al. Out-of-plane constraint effect on local fracture resistance of a dissimilar metal welded joint [J]. Mater. Des., 2014, 55: 542
doi: 10.1016/j.matdes.2013.10.034
9 Yang J, Wang L. Fracture mechanism of cracks in the weakest location of dissimilar metal welded joint under the interaction effect of in-plane and out-of-plane constraints [J]. Eng. Fract. Mech., 2018, 192: 12
doi: 10.1016/j.engfracmech.2018.02.008
10 Zha Y Y, Wang G Z, Xuan F Z, et al. Unified correlation of geometry and material constraints with fracture toughness of welded joint with high mismatch [J]. Press. Vessels. Technol., 2017, 34(3): 17
10 查媛媛, 王国珍, 轩福贞 等. 几何和材料拘束与高匹配焊接接头断裂韧性的统一关联 [J]. 压力容器, 2017, 34(3): 17
11 Zhu Z Q, Jing H Y, Ge J G, et al. Effects of strength mis-matching on the fracture behavior of nuclear pressure steel A508-III welded joint [J]. Mater. Sci. Eng., 2005, A390: 113
12 Younise B, Rakin M, Gubeljak N, et al. Effect of material heterogeneity and constraint conditions on ductile fracture resistance of welded joint zones-Micromechanical assessment [J]. Eng. Fail. Anal., 2017, 82: 435
doi: 10.1016/j.engfailanal.2017.08.006
13 Xue H, Ogawa K, Shoji T. Effect of welded mechanical heterogeneity on local stress and strain ahead of stationary and growing crack tips [J]. Nucl. Eng. Des., 2009, 239: 628
doi: 10.1016/j.nucengdes.2008.12.024
14 Mathar J. Determination of inherent stresses by measuring deformations of drilled holes [R]. Washington: NACA Technical Memorandum, 1933
15 Mahmoudi A H, Truman C E, Smith D J. Using local out-of-plane compression (LOPC) to study the effects of resxvidual stress on apparent fracture toughness [J]. Eng. Fract. Mech., 2007, 75: 1516
doi: 10.1016/j.engfracmech.2007.06.014
16 Chen L Y, Wang G Z, Tan J P, et al. Effects of residual stress on creep damage and crack initiation in notched CT specimens of a Cr-Mo-V steel [J]. Eng. Fract. Mech., 2013, 97: 80
doi: 10.1016/j.engfracmech.2012.10.020
17 Song X M, Wang G Z, Xuan F Z, et al. Investigation of residual stress effects on creep crack initiation and growth using local out-of-plane compression [J]. Eng. Fract. Mech., 2015, 149: 45
doi: 10.1016/j.engfracmech.2015.10.002
18 Song X M, Wang G Z, Tu S T, et al. Effects of residual stress on creep crack initiation and growth of Cr-Mo-V steel in cracked C(T) specimen [J]. Procedia Eng., 2015, 130: 1770
doi: 10.1016/j.proeng.2015.12.328
19 Song X M. Effect of residual stress on creep crack initiation and growth for specimens with different geometric and material constraints [D]. Shanghai: East China University of Science and Technology, 2016
19 宋晓梅. 残余应力对不同几何和材料拘束试样蠕变裂纹起裂和扩展行为的影响 [D]. 上海: 华东理工大学, 2016
20 Qian G A, Niffenegger M. Investigation of constraint and warm prestressing effects by means of a local approach to fracture [J]. Eng. Fract. Mech., 2015, 136: 26
doi: 10.1016/j.engfracmech.2015.01.031
21 Liu J, Zhang Z L, Nyhus B. Residual stress induced crack tip constraint [J]. Eng. Fract. Mech., 2008, 75: 4151
doi: 10.1016/j.engfracmech.2008.03.010
22 Wang H T, Wang G Z, Xuan F Z, et al. Local mechanical properties and microstructures of Alloy 52M dissimilar metal welded joint between A508 ferritic steel and 316L stainless steel [J]. Adv. Mater. Res., 2012, 509: 103
23 Wang H T, Wang G Z, Xuan F Z, et al. Local mechanical properties of a dissimilar metal welded joint in nuclear powersystems [J]. Mater. Sci. Eng., 2013, A568: 108
24 Yang J, Wang L. Effect and optimal design of the material constraint in the DMWJ of nuclear power plants [J]. Acta Metall. Sin., 2020, 56: 840
24 杨 杰, 王 雷. 核电站DMWJ中材料拘束的影响与优化 [J]. 金属学报, 2020, 56: 840
25 Yang J. Micromechanical analysis of in-plane constraint effect on local fracture behavior of cracks in the weakest locations of dissimilar metal welded joint [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 840
doi: 10.1007/s40195-017-0599-y
[1] 杜金辉, 毕中南, 曲敬龙. 三联冶炼GH4169合金研究进展[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] 毕中南, 秦海龙, 刘沛, 史松宜, 谢锦丽, 张继. 高温合金锻件残余应力量化表征及控制技术研究进展[J]. 金属学报, 2023, 59(9): 1144-1158.
[3] 李时磊, 李阳, 王友康, 王胜杰, 何伦华, 孙光爱, 肖体乔, 王沿东. 基于中子与同步辐射技术的工程材料/部件多尺度残余应力评价[J]. 金属学报, 2023, 59(8): 1001-1014.
[4] 张开元, 董文超, 赵栋, 李世键, 陆善平. 固态相变对Fe-Co-Ni超高强度钢长臂梁构件焊接-淬火过程应力和变形的影响[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] 王重阳, 韩世伟, 谢峰, 胡龙, 邓德安. 固态相变和软化效应对超高强钢焊接残余应力的影响[J]. 金属学报, 2023, 59(12): 1613-1623.
[6] 卢海飞, 吕继铭, 罗开玉, 鲁金忠. 激光热力交互增材制造Ti6Al4V合金的组织及力学性能[J]. 金属学报, 2023, 59(1): 125-135.
[7] 张新房, 向思奇, 易坤, 郭敬东. 脉冲电流调控金属固体中的残余应力[J]. 金属学报, 2022, 58(5): 581-598.
[8] 苏凯新, 张继旺, 张艳斌, 闫涛, 李行, 纪东东. 微弧氧化6082-T6铝合金的高周疲劳性能及残余应力松弛机理[J]. 金属学报, 2022, 58(3): 334-344.
[9] 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊. 从局域应力/应变视角理解异构金属材料的强韧化行为[J]. 金属学报, 2022, 58(11): 1427-1440.
[10] 骆文泽, 胡龙, 邓德安. SUS316不锈钢马鞍形管-管接头的残余应力数值模拟及高效计算方法开发[J]. 金属学报, 2022, 58(10): 1334-1348.
[11] 李索, 陈维奇, 胡龙, 邓德安. 加工硬化和退火软化效应对316不锈钢厚壁管-管对接接头残余应力计算精度的影响[J]. 金属学报, 2021, 57(12): 1653-1666.
[12] 杨杰, 王雷. 核电站DMWJ中材料拘束的影响与优化[J]. 金属学报, 2020, 56(6): 840-848.
[13] 李克俭, 张宇, 蔡志鹏. 异种金属焊接接头在热-力耦合作用下的断裂位置转移机理[J]. 金属学报, 2020, 56(11): 1463-1473.
[14] 姜霖, 张亮, 刘志权. Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响[J]. 金属学报, 2020, 56(10): 1433-1440.
[15] 毕中南,秦海龙,董志国,王相平,王鸣,刘永泉,杜金辉,张继. 高温合金盘锻件制备过程残余应力的演化规律及机制[J]. 金属学报, 2019, 55(9): 1160-1174.