| 块体非晶合金的3D打印成形研究进展 |
李宁( ), 黄信 |
| 华中科技大学 材料科学与工程学院 武汉 430074 |
|
| Recent Advances on 3D Printed Bulk Metallic Glasses |
LI Ning( ), HUANG Xin |
| School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China |
引用本文:
李宁, 黄信. 块体非晶合金的3D打印成形研究进展[J]. 金属学报, 2021, 57(4): 529-541.
Ning LI,
Xin HUANG.
Recent Advances on 3D Printed Bulk Metallic Glasses[J]. Acta Metall Sin, 2021, 57(4): 529-541.
| 1 |
Klement W, Willens R H, Duwez P. Non-crystalline structure in solidified gold-silicon alloys [J]. Nature, 1960, 187: 869
|
| 2 |
Nieh T G, Wadsworth J. Homogeneous deformation of bulk metallic glasses [J]. Scr. Mater., 2006, 54: 387
|
| 3 |
Tian L, Cheng Y Q, Shan Z W, et al. Approaching the ideal elastic limit of metallic glasses [J]. Nat. Commun., 2012, 3: 609
|
| 4 |
Wang J F, Li R, Hua N B, et al. Co-based ternary bulk metallic glasses with ultrahigh strength and plasticity [J]. J. Mater. Res., 2011, 26: 2072
|
| 5 |
Cao L F. Research on the preparation of Fe84(NbV)7B9 nanocrystalline soft magnetic materials and related fundamental theory [D]. Changsha: Central South University, 2006
|
| 5 |
曹玲飞. Fe84(NbV)7B9纳米晶软磁材料的制备及其相关基础问题的研究 [D]. 长沙: 中南大学, 2006
|
| 6 |
Pan J, Zhang M, Chen Q, et al. Study of anticorrosion ability of Fe43.7Co7.3Cr14.7Mo12.6C15.5B4.3Y1.9 bulk metallic glass in strong acid solutions [J]. Rare Met. Mater Eng., 2008, 37(suppl.4): 805
|
| 6 |
潘 杰, 张 猛, 谌 祺等. FeCoCrMoCBY块体非晶合金在强酸介质中的耐蚀性能 [J]. 稀有金属材料与工程, 2008, 37(): 805
|
| 7 |
Suryanarayana C, Inoue A. Bulk Metallic Glass [M]. Boca Raton: CRC Press, 2011: 1
|
| 8 |
Schroers J. Processing of bulk metallic glass [J]. Adv. Mater., 2010, 22: 1566
|
| 9 |
Schroers J, Paton N. Amorphous metal alloys form like plastics [J]. Adv. Mater. Process., 2006, 164: 61
|
| 10 |
Saotome Y, Miwa S, Zhang T, et al. The micro-formability of Zr-based amorphous alloys in the supercooled liquid state and their application to micro-dies [J]. J. Mater. Process. Technol., 2001, 113: 64
|
| 11 |
Gu D D, Hagedorn Y C, Meiners W, et al. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium [J]. Acta Mater., 2012, 60: 3849
|
| 12 |
Pauly S, Löber L, Petters R, et al. Processing metallic glasses by selective laser melting [J]. Mater. Today, 2013, 16: 37
|
| 13 |
Katakam S, Hwang J Y, Paital S, et al. In situ laser synthesis of Fe-based amorphous matrix composite coating on structural steel [J]. Metall. Mater. Trans., 2012, 43A: 4957
|
| 14 |
Zheng B, Zhou Y, Smugeresky J E, et al. Processing and behavior of Fe-based metallic glass components via laser-engineered net shaping [J]. Metall. Mater. Trans., 2009, 40A: 1235
|
| 15 |
Laser engineered net shaping, LENS [EB/OL].
|
| 16 |
Gibson M A, Mykulowycz N M, Shim J, et al. 3D printing metals like thermoplastics: Fused filament fabrication of metallic glasses [J]. Mater. Today, 2018, 21: 697
|
| 17 |
Zhang C, Wang W, Li Y C, et al. 3D printing of Fe-based bulk metallic glasses and composites with large dimensions and enhanced toughness by thermal spraying [J]. J. Mater. Chem., 2018, 6A: 6800
|
| 18 |
Gorodesky N, Sedghani‐Cohen S, Altman M, et al. Concurrent formation of metallic glass during laser forward transfer 3D printing [J]. Adv. Funct. Mater., 2020, 30: 2001260
|
| 19 |
Visser C W, Pohl R, Sun C, et al. Toward 3D printing of pure metals by laser-induced forward transfer [J]. Adv. Mater., 2015, 27: 4087
|
| 20 |
Duoss E. Direct ink writing of bulk metallic glasses [R/OL]. , 2017
|
| 21 |
Li X P, Kang C W, Huang H, et al. Selective laser melting of an Al86Ni6Y4.5Co2La1.5 metallic glass: Processing, microstructure evolution and mechanical properties [J]. Mater. Sci. Eng., 2014, A606: 370
|
| 22 |
Ouyang D, Li N, Xing W, et al. 3D printing of crack-free high strength Zr-based bulk metallic glass composite by selective laser melting [J]. Intermetallics, 2017, 90: 128
|
| 23 |
Deng L, Wang S H, Wang P, et al. Selective laser melting of a Ti-based bulk metallic glass [J]. Mater. Lett., 2018, 212: 346
|
| 24 |
Ouyang D, Xing W, Li N, et al. Structural evolutions in 3D-printed Fe-based metallic glass fabricated by selective laser melting [J]. Addit. Manuf., 2018, 23: 246
|
| 25 |
Bordeenithikasem P, Stolpe M, Elsen A, et al. Glass forming ability, flexural strength, and wear properties of additively manufactured Zr-based bulk metallic glasses produced through laser powder bed fusion [J]. Addit. Manuf., 2018, 21: 312
|
| 26 |
Li N, Zhang J J, Xing W, et al. 3D printing of Fe-based bulk metallic glass composites with combined high strength and fracture toughness [J]. Mater. Des., 2018, 143: 285
|
| 27 |
Mahbooba Z, Thorsson L, Unosson M, et al. Additive manufacturing of an iron-based bulk metallic glass larger than the critical casting thickness [J]. Appl. Mater. Today, 2018, 11: 264
|
| 28 |
Hofmann D C, Bordeenithikasem P, Pate A, et al. Developing processing parameters and characterizing microstructure and properties of an additively manufactured FeCrMoBC metallic glass forming alloy [J]. Adv. Eng. Mater., 2018, 20: 1800433
|
| 29 |
Jung H Y, Choi S J, Prashanth K G, et al. Fabrication of Fe-based bulk metallic glass by selective laser melting: A parameter study [J]. Mater. Des., 2015, 86: 703
|
| 30 |
Wang L, Wang H, Liu Y K, et al. Selective laser melting helps fabricate record-large bulk metallic glass: Experiments, simulation and demonstrative part [J]. J. Alloys Compd., 2019, 808: 151731
|
| 31 |
Zhang C, Li X M, Liu S Q, et al. 3D printing of Zr-based bulk metallic glasses and components for potential biomedical applications [J]. J. Alloys Compd., 2019, 790: 963
|
| 32 |
Xing W, Ouyang D, Chen Z, et al. Effect of energy density on defect evolution in 3D printed Zr-based metallic glasses by selective laser melting [J]. Sci. China Phys. Mech. Astron., 2019, 63: 226111
|
| 33 |
Li X P, Roberts M P, O'Keeffe S, et al. Selective laser melting of Zr-based bulk metallic glasses: Processing, microstructure and mechanical properties [J]. Mater. Des., 2016, 112: 217
|
| 34 |
Shen Y Y, Li Y Q, Chen C, et al. 3D printing of large, complex metallic glass structures [J]. Mater. Des., 2017, 117: 213
|
| 35 |
Sun H, Flores K M. Laser deposition of a Cu-based metallic glass powder on a Zr-based glass substrate [J]. J. Mater. Res., 2011, 23: 2692
|
| 36 |
ŁŻrodowski, Wysocki B, Wróblewski R, et al. New approach to amorphization of alloys with low glass forming ability via selective laser melting [J]. J. Alloys Compd., 2019, 771: 769
|
| 37 |
Yang C, Zhang C, Xing W, et al. 3D printing of Zr-based bulk metallic glasses with complex geometries and enhanced catalytic properties [J]. Intermetallics, 2018, 94: 22
|
| 38 |
Luo Y, Xing L L, Jiang Y D, et al. Additive manufactured large Zr-based bulk metallic glass composites with desired deformation ability and corrosion resistance [J]. Materials (Basel), 2020, 13: 597
|
| 39 |
Pacheco V, Karlsson D, Marattukalam J J, et al. Thermal stability and crystallization of a Zr-based metallic glass produced by suction casting and selective laser melting [J]. J. Alloys Compd., 2020, 825: 153995
|
| 40 |
Marattukalam J J, Pacheco V, Karlsson D, et al. Development of process parameters for selective laser melting of a Zr-based bulk metallic glass [J]. Addit. Manuf., 2020, 33: 101124
|
| 41 |
Lu X Y, Nursulton M, Du Y L, et al. Structural and mechanical characteristics of Cu50Zr43Al7 bulk metallic glass fabricated by selective laser melting [J]. Materials (Basel), 2019, 12: 75
|
| 42 |
Gao X D, Liu Z L, Li J H, et al. Selective laser melting of CuZr-based metallic glass composites [J]. Mater. Lett., 2020, 259: 126724
|
| 43 |
Pauly S, Schricker C, Scudino S, et al. Processing a glass-forming Zr-based alloy by selective laser melting [J]. Mater. Des., 2017, 135: 133
|
| 44 |
Zhai L L, Lu Y Z, Wang L, et al. Quantitative evaluation of hidden hierarchical pores in laser additive manufactured bulk metallic glasses via computed tomography [J]. Mater. Lett., 2020, 265: 127376
|
| 45 |
Zhai L L, Lu Y Z, Zhao X Y, et al. High-throughput screening of laser additive manufactured metallic glass via ultrasonic wave [J]. Sci. Rep., 2019, 9: 17660
|
| 46 |
Xu H D, Lu Y Z, Liu Z H, et al. Laser 3D printing of Zr-based bulk metallic glass [J]. J. Manuf. Process., 2019, 39: 102
|
| 47 |
Lin X, Zhang Y Y, Yang G L, et al. Microstructure and compressive/tensile characteristic of large size Zr-based bulk metallic glass prepared by laser solid forming [J]. J. Mater. Sci. Technol., 2019, 35: 328
|
| 48 |
Yang G L, Lin X, Liu F C, et al. Laser solid forming Zr-based bulk metallic glass [J]. Intermetallics, 2012, 22: 110
|
| 49 |
Su S, Lu Y Z. Laser directed energy deposition of Zr-based bulk metallic glass composite with tensile strength [J]. Mater. Lett., 2019, 247: 79
|
| 50 |
Liang S X, Wang X Q, Zhang W C, et al. Selective laser melting manufactured porous Fe-based metallic glass matrix composite with remarkable catalytic activity and reusability [J]. Appl. Mater. Today, 2020, 19: 100543
|
| 51 |
Zhang P C, Ouyang D, Liu L. Enhanced mechanical properties of 3D printed Zr-based BMG composite reinforced with Ta precipitates [J]. J. Alloys Compd., 2019, 803: 476
|
| 52 |
Zhu Q J, Qu S Y, Wang X H, et al. Synthesis of Fe-based amorphous composite coatings with low purity materials by laser cladding [J]. Appl. Surf. Sci., 2007, 253: 7060
|
| 53 |
Nong X D, Zhou X L, Ren Y X. Fabrication and characterization of Fe-based metallic glasses by Selective Laser Melting [J]. Opt. Laser Technol., 2019, 109: 20
|
| 54 |
Li X P, Kang C W, Huang H, et al. The role of a low-energy-density re-scan in fabricating crack-free Al85Ni5Y6Co2Fe2 bulk metallic glass composites via selective laser melting [J]. Mater. Des., 2014, 63: 407
|
| 55 |
Xie F, Chen Q J, Gao J W. Brittle-ductile transition in laser 3D printing of Fe-based bulk metallic glass composites [J]. Metals, 2019, 9: 78
|
| 56 |
Zhang Y, Liu H S, Mo J Y, et al. Atomic-level crystallization in selective laser melting fabricated Zr-based metallic glasses [J]. Phys. Chem. Chem. Phys., 2019, 21: 12406
|
| 57 |
Zhang Y, Liu H S, Mo J Y, et al. Atomic-scale structural evolution in selective laser melting of Cu50Zr50 metallic glass [J]. Comput. Mater. Sci., 2018, 150: 62
|
| 58 |
Guo S, Wang M, Lin X, et al. Research on the crystallization behavior occurred in the process of preparing bulk metallic glass with selective laser melting [J]. Mater. Res. Express, 2019, 6: 066582
|
| 59 |
Simchi A, Pohl H. Effects of laser sintering processing parameters on the microstructure and densification of iron powder [J]. Mater. Sci. Eng., 2003, A359: 119
|
| 60 |
Zhang Y Y, Lin X, Wei L, et al. Influence of powder size on the crystallization behavior during laser solid forming Zr55Cu30Al10Ni5 bulk amorphous alloy [J]. Intermetallics, 2016, 76: 1
|
| 61 |
Zhang B, Li Y T, Bai Q. Defect formation mechanisms in selective laser melting: A review [J]. Chin. J. Mech. Eng., 2017, 30: 515
|
| 62 |
Qiu C L, Panwisawas C, Ward M, et al. On the role of melt flow into the surface structure and porosity development during selective laser melting [J]. Acta Mater., 2015, 96: 72
|
| 63 |
Ouyang D. Fabrication, structure and properties of 3D printed amorphous alloys by selective laser melting [D]. Wuhan: Huazhong University of Science and Technology, 2019
|
| 63 |
欧阳迪. 激光选区熔化3D打印非晶合金的制备、结构与性能研究 [D]. 武汉: 华中科技大学, 2019
|
| 64 |
Best J P, Ostergaard H E, Li B S, et al. Fracture and fatigue behaviour of a laser additive manufactured Zr-based bulk metallic glass [J]. Addit. Manuf., 2020, 36: 101416
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|