| 具有异常放热现象的Fe-Nb-B-Y非晶合金燃烧机理 |
胡祥1, 葛嘉城1, 刘思楠1, 伏澍1, 吴桢舵2,3, 冯涛1, 刘冬4, 王循理2, 兰司1( ) |
1.南京理工大学 材料科学与工程学院/格莱特研究院 格莱特纳米科技研究所 南京 210094 2.香港城市大学 物理系 香港 999077 3.东莞市香港城市大学研究院 中子散射应用物理研究中心 东莞 523808 4.南京理工大学 能源与动力工程学院 南京 210094 |
|
| Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon |
HU Xiang1, GE Jiacheng1, LIU Sinan1, FU Shu1, WU Zhenduo2,3, FENG Tao1, LIU Dong4, WANG Xunli2, LAN Si1( ) |
1.Herbert Gleiter Institute of Nanoscience, School of Materials Science and Engineering/Herbert Gleiter Institute, Nanjing University of Science and Technology, Nanjing 210094, China 2.Department of Physics, City University of Hong Kong, Hong Kong 999077, China 3.Applied Physics Centre of Neutron Scattering, Dongguan University of Hong Kong Research Institute, Dongguan 523808, China 4.School of Energy and Power Engineering, Nanjing University of Science and Technology, Nanjing 210094, China |
引用本文:
胡祥, 葛嘉城, 刘思楠, 伏澍, 吴桢舵, 冯涛, 刘冬, 王循理, 兰司. 具有异常放热现象的Fe-Nb-B-Y非晶合金燃烧机理[J]. 金属学报, 2021, 57(4): 542-552.
Xiang HU,
Jiacheng GE,
Sinan LIU,
Shu FU,
Zhenduo WU,
Tao FENG,
Dong LIU,
Xunli WANG,
Si LAN.
Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. Acta Metall Sin, 2021, 57(4): 542-552.
| 1 |
Baletto F, Ferrando R. Structural properties of nanoclusters: Energetic, thermodynamic, and kinetic effects [J]. Rev. Mod. Phys., 2005, 77: 371
|
| 2 |
Sikder A K, Sikder N. A review of advanced high performance, insensitive and thermally stable energetic materials emerging for military and space applications [J]. J. Hazard. Mater., 2004, 112: 1
|
| 3 |
Li G, Zhang C Y. Review of the molecular and crystal correlations on sensitivities of energetic materials [J]. J. Hazard. Mater., 2020, 398: 122910
|
| 4 |
Yu B S, Sun Y H, Bai H Y, et al. Highly energetic and flammable metallic glasses [J]. Sci. China Phys. Mech. Astron., 2020, 63: 276112
|
| 5 |
Badgujar D M, Talawar M B, Asthana S N, et al. Advances in science and technology of modern energetic materials: An overview [J]. J. Hazard. Mater., 2008, 151: 289
|
| 6 |
Trunov M A, Schoenitz M, Dreizin E L. Ignition of aluminum powders under different experimental conditions [J]. Propell. Explos. Pyrot., 2005, 30: 36
|
| 7 |
Yagodnikov D A, Ignatov A V, Gusachenko E I. Ignition and combustion of pyrotechnic compositions based on microsized and ultra-nanosized aluminum particles in a moist medium in a two-zone gas generator [J]. Combust. Explos. Shock Waves, 2017, 53: 15
|
| 8 |
Pan J, Wang Y X, Guo Q, et al. Extreme rejuvenation and softening in a bulk metallic glass [J]. Nat. Commun., 2018, 9: 560
|
| 9 |
Dreizin E L. Phase changes in metal combustion [J]. Prog. Energy Combust. Sci., 2000, 26: 57
|
| 10 |
Ge J C, He H Y, Zhou J, et al. In-situ scattering study of a liquid-liquid phase transition in Fe-B-Nb-Y supercooled liquids and its correlation with glass-forming ability [J]. J. Alloys Compd., 2019, 787: 831
|
| 11 |
Lan S, Ren Y, Wei X Y, et al. Hidden amorphous phase and reentrant supercooled liquid in Pd-Ni-P metallic glasses [J]. Nat. Commun., 2017, 8: 14679
|
| 12 |
Tanaka H. General view of a liquid-liquid phase transition [J]. Phys. Rev., 2000, 62E: 6968
|
| 13 |
Palmer J C, Martelli F, Liu Y, et al. Metastable liquid-liquid transition in a molecular model of water [J]. Nature, 2014, 510: 385
|
| 14 |
Shimizu R, Kobayashi M, Tanaka H. Evidence of liquid-liquid transition in triphenyl phosphite from time-resolved light scattering experiments [J]. Phys. Rev. Lett., 2014, 112: 125702
|
| 15 |
Zhou Z J, Hu X, You Z, et al. Oxy-fuel combustion characteristics and kinetic parameters of lignite coal from thermo-gravimetric data [J]. Thermochim. Acta, 2013, 553: 54
|
| 16 |
Fakhraai Z, Forrest J A. Measuring the surface dynamics of glassy polymers [J]. Science, 2008, 319: 600
|
| 17 |
Kök M V, Acar C. Kinetics of crude oil combustion [J]. J. Therm. Anal. Calorim., 2006, 83: 445
|
| 18 |
Lysenko E N, Surzhikov A P, Zhuravkov S P, et al. The oxidation kinetics study of ultrafine iron powders by thermogravimetric analysis [J]. J. Therm. Anal. Calorim., 2014, 115: 1447
|
| 19 |
Qi X W, Zhou J, Yue Z X, et al. Auto-combustion synthesis of nanocrystalline LaFeO3 [J]. Mater. Chem. Phys., 2003, 78: 25
|
| 20 |
Takacs L. Self-sustaining reactions induced by ball milling: An overview [J]. Int. J. Self-Propag. High-Temp. Synth., 2009, 18: 276
|
| 21 |
Takahashi M, Koshimura M, Abuzuka T. Phase diagram of amorphous and crystallized Fe-B alloy system [J]. Jpn. J. Appl. Phys., 1981, 20: 1821
|
| 22 |
Abrosimova G E, Aronin A S. Formation of metastable phases during crystallization of amorphous iron-based alloys [J]. Crystallogr. Rep., 2020, 65: 573
|
| 23 |
Grosvenor A P, Kobe B A, Biesinger M C, et al. Investigation of multiplet splitting of Fe 2p XPS spectra and bonding in iron compounds [J]. Surf. Interface Anal., 2004, 36: 1564
|
| 24 |
Yamashita T, Hayes P. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials [J]. Appl. Surf. Sci., 2008, 254: 2441
|
| 25 |
Kim K J, Moon D W, Lee S K, et al. Formation of a highly oriented FeO thin film by phase transition of Fe3O4 and Fe nanocrystallines [J]. Thin Solid Films, 2000, 360: 118
|
| 26 |
Li Y X, Claydon J S, Ahmad E, et al. XPS and XMCD study of Fe3O4 GaAs interface [J]. IEEE Trans. Magn., 2005, 41: 2808
|
| 27 |
Rydén M, Leion H, Mattisson T, et al. Combined oxides as oxygen-carrier material for chemical-looping with oxygen uncoupling [J]. Appl. Energy, 2014, 113: 1924
|
| 28 |
Zhang C, Wu Y, Liu L. Robust hydrophobic Fe-based amorphous coating by thermal spraying [J]. Appl. Phys. Lett., 2012, 101: 121603
|
| 29 |
Filonenko N Y, Babachenko O I, Kononenko G A. Influence of overheating and cooling rate on the structures and properties of alloys of the Fe-B system [J]. Mater. Sci., 2019, 55: 440
|
| 30 |
Otero T F, Santos F. Polythiophene oxidation: Rate coefficients, activation energy and conformational energies [J]. Electrochim. Acta, 2008, 53: 3166
|
| 31 |
Zhong Z Y, Highfield J, Lin M, et al. Insights into the oxidation and decomposition of CO on Au/α-Fe2O3 and on α-Fe2O3 by coupled TG-FTIR [J]. Langmuir, 2008, 24: 8576
|
| 32 |
Cao C R, Lu Y M, Bai H Y, et al. High surface mobility and fast surface enhanced crystallization of metallic glass [J]. Appl. Phys. Lett., 2015, 107: 141606
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|