| 预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响 |
韩宝帅1, 魏立军1,2, 徐严谨1( ), 马晓光1, 刘雅菲1, 侯红亮1 |
1.中国航空制造技术研究院 北京 100024 2.北京航空航天大学材料科学与工程学院 北京 100083 |
|
| Effect of Pre-Deformation on Microstructure and Mechanical Properties of Ultra-High Strength Al-Zn-Mg-Cu Alloy After Ageing Treatment |
HAN Baoshuai1, WEI Lijun1,2, XU Yanjin1( ), MA Xiaoguang1, LIU Yafei1, HOU Hongliang1 |
1. AVIC Manufacturing Technology Institute, Beijing 100024, China 2. School of Materials Science and Engineering, Beihang University, Beijing 100083, China |
引用本文:
韩宝帅, 魏立军, 徐严谨, 马晓光, 刘雅菲, 侯红亮. 预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响[J]. 金属学报, 2020, 56(7): 1007-1014.
Baoshuai HAN,
Lijun WEI,
Yanjin XU,
Xiaoguang MA,
Yafei LIU,
Hongliang HOU.
Effect of Pre-Deformation on Microstructure and Mechanical Properties of Ultra-High Strength Al-Zn-Mg-Cu Alloy After Ageing Treatment[J]. Acta Metall Sin, 2020, 56(7): 1007-1014.
| [1] |
Zhang X M, Deng Y L, Zhang Y. Development of high strength aluminum alloys and processing techniques for the materials [J]. Acta Metall. Sin., 2015, 51: 257
doi: 10.11900/0412.1961.2014.00406
|
| [1] |
(张新明, 邓运来, 张 勇. 高强铝合金的发展及其材料的制备加工技术 [J]. 金属学报, 2015, 51: 257)
doi: 10.11900/0412.1961.2014.00406
|
| [2] |
Yang S J, Xing Q Y, Yu H J, et al. Al-Zn-Mg-Cu alloys with strength of 800MPa [J]. J. Mater. Eng., 2018, 46(4): 82
|
| [2] |
(杨守杰, 邢清源, 于海军等. 800MPa级Al-Zn-Mg-Cu系合金 [J]. 材料工程, 2018, 46(4): 82)
|
| [3] |
Zhang X M, Zhang T J, Tian F, et al. Effects of multi-direction forging on improving properties of 7075 aluminum alloy [J]. Rare Met. Mater. Eng., 2003, 32: 372
|
| [3] |
(张小明, 张廷杰, 田 锋等. 多向锻造对改善7075铝合金性能的作用 [J]. 稀有金属材料与工程, 2003, 32: 372)
|
| [4] |
Chen K H, Liu H W, Liu Y Z. Effect of promotively-solutionizing heat treatment on the mechanical properties and fracture behavior of Al-Zn-Mg-Cu alloys [J]. Acta Metall. Sin., 2001, 37: 29
|
| [4] |
(陈康华, 刘红卫, 刘允中. 强化固溶对Al-Zn-Mg-Cu合金力学性能和断裂行为的影响 [J]. 金属学报, 2001, 37: 29)
|
| [5] |
Hou L G, Liu M L, Wang X D, et al. Cryogenic processing high-strength 7050 aluminum alloy and controlling of the microstructures and mechanical properties [J]. Acta Metall. Sin., 2017, 53: 1075
|
| [5] |
(侯陇刚, 刘明荔, 王新东等. 高强7050铝合金超低温大变形加工与组织、性能调控 [J]. 金属学报, 2017, 53: 1075)
|
| [6] |
Han X L, Xiong B Q, Zhang Y A, et al. Effect of solution treatment on microstructures and mechanical properties of 7150 aluminum alloy [J]. Chin. J. Nonferrous Met., 2010, 20: 1095
|
| [6] |
(韩小磊, 熊柏青, 张永安等. 固溶处理对7150铝合金组织和力学性能的影响 [J]. 中国有色金属学报, 2010, 20: 1095)
|
| [7] |
Zuo J R, Hou L G, Shi J T, et al. Precipitates and the evolution of grain structures during double-step rolling of high-strength aluminum alloy and related properties [J]. Acta Metall. Sin., 2016, 52: 1105
|
| [7] |
(左锦荣, 侯陇刚, 史金涛等. 两阶段轧制变形过程中高强铝合金析出相与晶粒结构演变及其对性能的影响 [J]. 金属学报, 2016, 52: 1105)
|
| [8] |
Dursun T, Soutis C. Recent developments in advanced aircraft aluminium alloys [J]. Mater. Des., 2014, 56: 862
|
| [9] |
Jia Y D, Cao F Y, Ning Z L, et al. Influence of second phases on mechanical properties of spray-deposited Al-Zn-Mg-Cu alloy [J]. Mater. Des., 2012, 40: 536
|
| [10] |
Zhao W J, Cao F Y, Gu X L, et al. Isothermal deformation of spray formed Al-Zn-Mg-Cu alloy [J]. Mech. Mater., 2013, 56: 95
|
| [11] |
Wang F, Xiong B Q, Zhang Y A, et al. Microstructure and mechanical properties of spray-deposited Al-Zn-Mg-Cu alloy processed through hot rolling and heat treatment [J]. Mater. Sci. Eng., 2009, A518: 144
|
| [12] |
Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141
|
| [13] |
Sharma M M. Microstructural and mechanical characterization of various modified 7XXX series spray formed alloys [J]. Mater. Charact., 2008, 59: 91
|
| [14] |
Werenskiold J C, Deschamps A, Bréchet Y. Characterization and modeling of precipitation kinetics in an Al-Zn-Mg alloy [J]. Mater. Sci. Eng., 2000, A293: 267
|
| [15] |
Huang Y J, Chen Z G, Zheng Z Q. A conventional thermo-mechanical process of Al-Cu-Mg alloy for increasing ductility while maintaining high strength [J]. Scr. Mater., 2011, 64: 382
|
| [16] |
Han N M, Zhang X M, Liu S D, et al. Effect of prestretching on fracture toughness of 7050 aluminum alloy [J]. Chin. J. Nonferrous Met., 2010, 20: 2088
|
| [16] |
(韩念梅, 张新明, 刘胜胆等. 预拉伸对7050铝合金断裂韧性的影响 [J]. 中国有色金属学报, 2010, 20: 2088)
|
| [17] |
Liu S D, Li Q, Ye L Y, et al. Effects of pre-stretching on mechanical properties and localized corrosion of 7085 aluminum alloy [J]. J. Cent. South Univ. (Sci. Technol.), 2018, 49: 2152
|
| [17] |
(刘胜胆, 李 群, 叶凌英等. 预拉伸对7085铝合金力学及局部腐蚀性能的影响 [J]. 中南大学学报(自然科学版), 2018, 49: 2152)
|
| [18] |
Wang D, Ma Z Y. Effect of pre-strain on microstructure and stress corrosion cracking of over-aged 7050 aluminum alloy [J]. J. Alloys Compd., 2009, 469: 445
|
| [19] |
Zhao J J, Xu X J, Chen Y, et al. Microstructures and properties of ultra-high-strength Al-Zn-Mg-Cu-Zr-Sr alloy with pre-deformation [J]. Chin. J. Rare Met., 2016, 40: 1193
|
| [19] |
(赵建吉, 许晓静, 陈 洋等. 预变形对超高强铝合金Al-Zn-Mg-Cu-Zr-Sr组织与性能的影响 [J]. 稀有金属, 2016, 40: 1193)
|
| [20] |
Youssef K M, Scattergood R O, Murty K L, et al. Nanocrystalline Al-Mg alloy with ultrahigh strength and good ductility [J]. Scr. Mater., 2006, 54: 251
|
| [21] |
Zhao Y H, Liao X Z, Jin Z, et al. Microstructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evolutions during annealing [J]. Acta Mater., 2004, 52: 4589
|
| [22] |
Li X W, Cai Q Z, Zhao B Y, et al. Precipitation behaviors and properties of solution-aging Al-Zn-Mg-Cu alloy refined with TiN nanoparticles [J]. J. Alloys Compd., 2018, 746: 462
|
| [23] |
Dumont M, Lefebvre W, Doisneau-Cottignies B, et al. Characterisation of the composition and volume fraction of η′ and η precipitates in an Al-Zn-Mg alloy by a combination of atom probe, small-angle X-ray scattering and transmission electron microscopy [J]. Acta Mater., 2005, 53: 2881
|
| [24] |
Chen J Z, Zhen L, Yang S J, et al. Investigation of precipitation behavior and related hardening in AA 7055 aluminum alloy [J]. Mater. Sci. Eng., 2009, A500: 34
|
| [25] |
Li H C, Cao F Y, Guo S, et al. Effects of Mg and Cu on microstructures and properties of spray-deposited Al-Zn-Mg-Cu alloys [J]. J. Alloys Compd., 2017, 719: 89
|
| [26] |
Wang F, Xiong B Q, Zhang Y A, et al. Effect of two-step aging treatment on microstructure and mechanical properties of spray-deposited Al-10.8Zn-2.8Mg-1.9Cu alloy [J]. Chin. J. Nonferrous Met., 2007, 17: 1058
|
| [26] |
(王 峰, 熊柏青, 张永安等. 双级时效处理对喷射沉积Al-Zn-Mg-Cu合金微观组织和力学性能的影响 [J]. 中国有色金属学报, 2007, 17: 1058)
|
| [27] |
Li H C, Cao F Y, Guo S, et al. Microstructures and properties evolution of spray-deposited Al-Zn-Mg-Cu-Zr alloys with scandium addition [J]. J. Alloys Compd., 2017, 691: 482
|
| [28] |
Wang D, Ni D R, Ma Z Y. Effect of pre-strain and two-step aging on microstructure and stress corrosion cracking of 7050 alloy [J]. Mater. Sci. Eng., 2008, A494: 360
|
| [29] |
Deschamps A, De Geuser F, Horita Z, et al. Precipitation kinetics in a severely plastically deformed 7075 aluminium alloy [J]. Acta Mater., 2014, 66: 105
|
| [30] |
Wang S S, Jiang J T, Fan G H, et al. Accelerated precipitation and growth of phases in an Al-Zn-Mg-Cu alloy processed by surface abrasion [J]. Acta Mater., 2017, 131: 233
|
| [31] |
Lee Y S, Koh D H, Kim H W, et al. Improved bake-hardening response of Al-Zn-Mg-Cu alloy through pre-aging treatment [J]. Scr. Mater., 2018, 147: 45
|
| [32] |
Chen J Z, Lv L X, Zhen L, et al. Quantitative characterization on the precipitation of AA 7055 aluminum alloy by SAXS [J]. Acta Metall. Sin., 2017, 53: 897
|
| [32] |
(陈军洲, 吕良星, 甄 良等. AA7055铝合金时效析出过程的小角度X射线散射定量表征 [J]. 金属学报, 2017, 53: 897)
|
| [33] |
Feng D, Zhang X M, Chen H M, et al. Effect of non-isothermal retrogression and re-ageing on microstructure and properties of Al-8Zn-2Mg-2Cu alloy thick plate [J]. Acta Metall. Sin., 2018, 54: 100
doi: 10.11900/0412.1961.2017.00203
|
| [33] |
(冯 迪, 张新明, 陈洪美等. 非等温回归再时效对Al-8Zn-2Mg-2Cu合金厚板组织及性能的影响 [J]. 金属学报, 2018, 54: 100)
doi: 10.11900/0412.1961.2017.00203
|
| [34] |
Han N M, Zhang X M, Liu S D, et al. Effects of pre-stretching and ageing on the strength and fracture toughness of aluminum alloy 7050 [J]. Mater. Sci. Eng., 2011, A528: 3714
|
| [35] |
Shercliff H R, Ashby M F. A process model for age hardening of aluminium alloys—I. The model [J]. Acta Metall. Mater., 1990, 38: 1789
|
| [36] |
Park J K, Ardell A J. Microchemical analysis of precipitate free zones in 7075-A1 in the T6, T7 and RRA tempers [J]. Acta Metall. Mater., 1991, 39: 591
doi: 10.1016/0956-7151(91)90127-M
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|