| 原位反应浸渗法制备(B4C+Ti)混杂增强Mg及AZ91D复合材料及其阻尼性能 |
姚彦桃1( ), 陈礼清2, 王文广1 |
1 辽宁石油化工大学机械工程学院 抚顺 113001 2 东北大学轧制技术及连轧自动化国家重点实验室 沈阳 110819 |
|
| Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique |
Yantao YAO1( ), Liqing CHEN2, Wenguang WANG1 |
1 School of Mechanical Engineering, Liaoning Shihua University, Fushun 113001, China 2 Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China |
引用本文:
姚彦桃, 陈礼清, 王文广. 原位反应浸渗法制备(B4C+Ti)混杂增强Mg及AZ91D复合材料及其阻尼性能[J]. 金属学报, 2019, 55(1): 141-148.
Yantao YAO,
Liqing CHEN,
Wenguang WANG.
Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique[J]. Acta Metall Sin, 2019, 55(1): 141-148.
| [1] | Carvalho O, Miranda G, Buciumeanu M, et al.High temperature damping behavior and dynamic Young's modulus of AlSi-CNT-SiCp hybrid composite[J]. Compos. Struct., 2016, 141: 155 | | [2] | Jiang H J, Liu C Y, Zhang B, et al.Simultaneously improving mechanical properties and damping capacity of Al-Mg-Si alloy through friction stir processing[J]. Mater. Charact., 2017, 131: 425 | | [3] | Li Q Y, Li J, He G.Compressive properties and damping capacities of magnesium reinforced with continuous steel wire[J]. Mater. Sci. Eng., 2017, A680: 92 | | [4] | Deng K K, Li J C, Nie K B, et al.High temperature damping behavior of as-deformed Mg matrix influenced by micron and submicron SiCp[J]. Mater. Sci. Eng., 2015, A624: 62 | | [5] | Wu Y W, Wu K, Deng K K, et al.Damping capacities and microstructures of magnesium matrix composites reinforced by graphite particles[J]. Mater. Des., 2010, 31: 4862 | | [6] | Wang C J, Deng K K, Liang W.High temperature damping behavior controlled by submicron SiCp in bimodal size particle reinforced magnesium matrix composite[J]. Mater. Sci. Eng., 2016, A668: 55 | | [7] | Habibi M K, Hamouda A M S, Gupta M. Enhancing tensile and compressive strength of magnesium using ball milled Al+CNT reinforcement[J]. Compos. Sci. Technol., 2012, 72: 290 | | [8] | Kevorkijan V, ?kapin S D.Mg/B4C composites with a high volume fraction of fine ceramic reinforcement[J]. Mater. Manuf. Processes, 2009, 24: 1337 | | [9] | Yao J P, Li W, Zhang L, et al.RETRACTED ARTICLE: Wear mechanism for in situ TiC particle reinforced AZ91 magnesium matrix composites[J]. Tribol. Lett., 2010, 38: 253 | | [10] | Yao Y T, Chen L Q.Processing of B4C particulate-reinforced magnesium-matrix composites by metal-assisted melt infiltration technique[J]. J. Mater. Sci. Technol., 2014, 30: 661 | | [11] | Chen L Q, Yao Y T.Processing, microstructures, and mechanical properties of magnesium matrix composites: A review[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 762 | | [12] | Sahoo B N, Panigrahi S K.Synthesis, characterization and mechanical properties of in-situ (TiC-TiB2) reinforced magnesium matrix composite[J]. Mater. Des., 2016, 109: 300 | | [13] | Chen L Q, Dong Q, Zhao M J, et al.Synthesis of TiC/Mg composites with interpenetrating networks by in situ reactive infiltration process[J]. Mater. Sci. Eng., 2005, A408: 125 | | [14] | Schaller R.Metal matrix composites, a smart choice for high damping materials[J]. J. Alloys Compd., 2003, 335: 131 | | [15] | Zhang X Q, Wang H W, Liao L H, et al.In situ synthesis method and damping characterization of magnesium matrix composites[J]. Compos. Sci. Technol., 2007, 67: 720 | | [16] | Wu Y W, Wu K, Nie K B, et al.Damping capacities and tensile properties in Grp/AZ91 and SiCp/Grp/AZ91 magnesium matrix composites[J]. Mater. Sci. Eng., 2010, A527: 7873 | | [17] | Anasori B, Barsoum M W.Energy damping in magnesium alloy composites reinforced with TiC or Ti2AlC particles[J]. Mater. Sci. Eng., 2016, A653: 53 | | [18] | Zhang X Q, Liao L H, Ma N H, et al.Mechanical properties and damping capacity of magnesium matrix composites[J]. Composites, 2006, 37A: 2011 | | [19] | Huang W Z, Luo H J, Mu Y L, et al.Low-frequency damping behavior of closed-cell Mg alloy foams reinforced with SiC particles[J]. Int. J. Min. Metall. Mater., 2017, 24: 701 | | [20] | Gu J H, Zhang X N, Qiu Y F, et al.Damping behaviors of magnesium matrix composites reinforced with Cu-coated and uncoated SiC particulates[J]. Compos. Sci. Technol., 2005, 65: 1736 | | [21] | Wang H Y, Jiang Q C, Zhao Y Q, et al.Fabrication of TiB2 and TiB2-TiC particulates reinforced magnesium matrix composites[J]. Mater. Sci. Eng., 2004, A372: 109 | | [22] | Shen P, Zou B L, Jin S B, et al. Reaction mechanism in self-propagating high temperature synthesis of TiC-TiB2/Al composites from an Al-Ti-B4C system [J]. Mater. Sci. Eng., 2007, A454-455: 300 | | [23] | Prasad D S, Shoba C.Experimental evaluation onto the damping behavior of Al/SiC/RHA hybrid composites[J]. J. Mater. Res. Technol., 2016, 5: 123 | | [24] | Cao W, Zhang C F, Fan T X, et al.In situ synthesis and damping capacities of TiC reinforced magnesium matrix composites[J]. Mater. Sci. Eng., 2008, A496: 242 | | [25] | Liu Y C, Li J F, Yang G C, et al.High damping functional materials prepared by spray deposition[J]. J. Mater. Process Technol., 2000, 106: 94 |
|
|