| 一种Fe-Cr-Ni-Mo高强高韧合金钢焊接接头的组织和力学性能 |
胡小锋( ), 姜海昌, 赵明久, 闫德胜, 陆善平, 戎利建 |
| 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室 沈阳 110016 |
|
| Microstructure and Mechanical Properties of Welded Joint of a Fe-Cr-Ni-Mo Steel with High-Strength and High-Toughness |
Xiaofeng HU( ), Haichang JIANG, Mingjiu ZHAO, Desheng YAN, Shanping LU, Lijian RONG |
| Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
胡小锋, 姜海昌, 赵明久, 闫德胜, 陆善平, 戎利建. 一种Fe-Cr-Ni-Mo高强高韧合金钢焊接接头的组织和力学性能[J]. 金属学报, 2018, 54(1): 1-10.
Xiaofeng HU,
Haichang JIANG,
Mingjiu ZHAO,
Desheng YAN,
Shanping LU,
Lijian RONG.
Microstructure and Mechanical Properties of Welded Joint of a Fe-Cr-Ni-Mo Steel with High-Strength and High-Toughness[J]. Acta Metall Sin, 2018, 54(1): 1-10.
| [1] | Lee K H, Park S G, Kim M C, et al.Characterization of transition behavior in SA508 Gr.4N Ni-Cr-Mo low alloy steels with microstructural alteration by Ni and Cr contents[J]. Mater. Sci. Eng., 2011, A529: 156 | | [2] | Mulholland M D, Seidman D N.Nanoscale co-precipitation and mechanical properties of a high-strength low-carbon steel[J]. Acta Mater., 2011, 59: 1881 | | [3] | Wang L J, Cai Q W, Yu W, et al.Microstructure and mechanical properties of 1500 MPa grade ultra-high strength low alloy steel[J]. Acta Metall. Sin., 2010, 46: 687)(王立军,蔡庆伍,余伟等. 1500 MPa级低合金超高强钢的微观组织与力学性能[J].金属学报, 2010, 46: 687) | | [4] | Tian Y Q, Zhang H J, Chen L S, et al.Effect of alloy elements partitioning behavior on retained austenite and mechanical property in low carbon high strength steel[J]. Acta Metall. Sin.,2014, 50: 531)(田亚强,张宏军,陈连生等. 低碳高强钢合金元素配分行为对残余奥氏体和力学性能的影响[J].金属学报, 2014, 50: 531) | | [5] | Han S Y, Shin S Y, Seo C H, et al.Effects of Mo, Cr, and V additions on tensile and charpy impact properties of API X80 pipeline steels[J]. Metall. Mater. Trans., 2009, 40A: 1851 | | [6] | He X L, Yang X Q, Zhang G D, et al.Quenching microstructure and properties of 300M ultra-high strength steel electron beam welded joints[J]. Mater. Des., 2012, 40: 386 | | [7] | Malakondaiah G, Srinivas M, Rao P R.Ultrahigh-strength low-alloy steels with enhanced fracture toughness[J]. Prog. Mater. Sci., 1997, 42: 209 | | [8] | Tomita Y, Okawa T.Effect of modified heat-treatment on mechanical properties of 300M steel[J]. Mater. Sci. Technol., 1995, 11: 245 | | [9] | Lee W S, Su T T.Mechanical properties and microstructural features of AISI 4340 high-strength alloy steel under quenched and tempered conditions[J]. J. Mater. Process. Technol., 1999, 87: 198 | | [10] | Youngblood J L, Raghavan M.Correlation of microstructure with mechanical properties of 300M steel[J]. Metall. Trans., 1977, 8A: 1439 | | [11] | Ritchie R O, Francis B, Server W L.Evaluation of toughness in AISI 4340 alloy steel austenitized at low and high temperatures[J]. Metall. Trans., 1976, 7A: 831 | | [12] | Chang T L, Tsay L W, Chen C.Influence of gaseous hydrogen on the notched tensile strength of D6ac steel[J]. Mater. Sci. Eng., 2001, A316: 153 | | [13] | Caballero F G,Bhadeshia H K D H,Mawella K J A,et al. Design of novel high strength bainitic steels: Part 1[J]. Mater. Sci. Technol., 2001, 17: 512 | | [14] | Caballero F G,Bhadeshia H K D H,Mawella K J A,et al.Design of novel high strength bainitic steels: Part 2[J]. Mater. Sci. Technol., 2001, 17: 517 | | [15] | Li Y J.Welding of High Strength Steel [M]. Beijing: Metallurgical Industry Press, 2010: 89.(李亚江.高强钢的焊接[M].北京: 冶金工业出版社,2010: 89. | | [16] | Wen T, Hu X F, Song Y Y, et al.Effect of tempering temperature on carbide and mechanical properties in a Fe-Cr-Ni-Mo high-strength steel[J]. Acta Metall. Sin., 2014, 50: 447)(温涛,胡小锋,宋元元等. 回火温度对一种Fe-Cr-Ni-Mo高强钢碳化物及其力学性能的影响[J].金属学报, 2014, 50: 447) | | [17] | Wen T, Hu X F, Yan D S, et al.Effect of V contents on microstructure and mechanical properties in a Fe-Cr-Ni-Mo high-strength steel[J]. Mater. Sci. Forum, 2014, 788: 304 | | [18] | Wen T, Hu X F, Song Y Y, et al.Carbides and mechanical properties in a Fe-Cr-Ni-Mo high-strength steel with different V contents[J]. Mater. Sci. Eng., 2013, A588: 201 | | [19] | Zhang M, Wang Q, Li J H, et al.Microstructure numerical simulation of weld pool in rapid solidification[J]. Trans. China Weld. Inst.,, 2013, 34(7): 1)(张敏,汪强,李继红等. 焊接熔池快速凝固过程的微观组织演化数值模拟[J].焊接学报, 2013, 34(7): 1) | | [20] | Keehan E, Karlsson L, Andrén H O, et al. New developments with C-Mn-Ni high-strength steel weld metals, Part A-Microstructure[J]. Weld. J., 2006,85: 200-s | | [21] | Janovec J, Vyrostková A, Svoboda M, et al.Evolution of secondary phases in Cr-V low-alloy steels during aging[J]. Metall. Mater. Trans., 2004, 35A: 751 | | [22] | Shi Y W, Han Z X.Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800 MPa grade high strength low alloy steel[J]. J. Mater. Process. Technol., 2008, 207: 30 | | [23] | Alé R M, Rebello J M A,Charlier J.A metallographic technique for detecting martensite-austenite constituents in the weld heat-affected zone of a micro-alloyed steel[J]. Mater. Charact., 1996, 37: 89 | | [24] | Li X D, Shang C J, Han C C, et al.Influence of necklace-type M-A constituent on impact toughness and fracture mechanism in the heat affected zone of X100 pipeline steel[J]. Acta Metall. Sin., 2016, 52: 1025)(李学达,尚成嘉,韩昌柴等.X100管线钢焊接热影响区中链状M-A组元对冲击韧性和断裂机制的影响[J].金属学报, 2016, 52: 1025) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|